Artyomov N.S., Kapustianskaia M.A., Kovalenko A.V., Sidelnikov N.K., Kurnosov A.O. Research of the influence of curing temperature conditions on the physical and mechanical properties of two-component cold curing spheroplastic VPZ-7M // Proceedings of VIAM. 2024. No. 7 (137). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-7-45-55.

Research of the influence of curing temperature conditions on the physical and mechanical properties of two-component cold curing spheroplastic VPZ-7M

Artyomov N.S., Kapustianskaia M.A., Kovalenko A.V., Sidelnikov N.K., Kurnosov A.O.
Abstract

In this study, an analysis of the influence of curing temperature conditions on the physical and mechanical properties of two-component spheroplastics VPZ-7M is carried out. Based on previously studied curing modes of resins included in spheroplastics, the most suitable curing modes were selected. A model of the curing reaction of a polymer filler is considered based on experimental data obtained by differential scanning calorimetry. The microstructure of the samples of spheroplastic was studied. The obtained results allow making a choice of the curing conditions to achieve the required material characteristics.

Keywords
spheroplastic, polymer filler, microstructure, polymer composite material, curing, epoxy binder
Reference list
  1. Zastrogina O.B., Sinyakov S.D., Serkova E.А. Materials based on phenolformaldehyde oligomers of resol and novolac tipes (review). Part 2. Trudy VIAM, 2021, no. 11 (105), paper no. 06. Available at: http://www.viam-works.ru (accessed: March 01, 2024). DOI: 10.18577/2307-6046-2021-0-11-55-65.
  2. Kablov E.N. Main results and directions of development of materials for advanced aircraft. 75 years. Aviation materials. Moscow: VIAM, 2007, pp. 20–26.
  3. Postnov V.I., Veshkin E.A., Makrushin K.V., Sudin Yu.I. Technological features of manufacturing polymer composite materials of main rotor blades for a light helicopter. Aviation materials and technologies, 2023, no. 1 (70), paper no. 06. Available at: http://www.journal.viam.ru (accessed: March 01, 2024). DOI: 10.18577/2713-0193-2023-0-1-30-50.
  4. Mikhailin Yu.A. Heat-resistant polymers and polymer materials. St. Petersburg: Profession, 2006, 624 p.
  5. Malysheva G.V., Marakhovskiy P.S., Barinov D.Ya., Nikolaev E.V. Optimization of the curing modes of fiber-glass based on epoxy binder. Aviation materials and technologies, 2023, no. 2 (71), paper no. 08. Available at: http://www.journal.viam.ru (accessed: March 01, 2024). DOI: 10.18577/2713-0193-2023-0-2-94-103.
  6. Trostyanskaya E.B., Golovkin G.S., Dmitrenko V.P. Promising PCMs and advanced technologies for the production of aircraft structural elements from them. Aviatsionnaya promyshlennost, 1987, no. 2, pp. 37–42.
  7. Kablov E.N. Materials for aerospace technology. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, pp. 7–27.
  8. Bulanov I.M., Vorobey V.V. Technology of rocket and aerospace structures made of composite materials. Moscow: MSTU im. N.E. Bauman, 1998, 516 p.
  9. Kapustyanskaya M.A., Gurevich Ya.M., Mishurov K.S. Polymer filler for accelerated molding technology. Plasticheskiye massy, 2023, no. 11–12, pp. 50–53. DOI: 10.35164/0554-2901-2023-11-12-50-53.
  10. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: March 01, 2024). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  11. Kurnosov A.O., Raskutin A.E., Mukhametov R.R., Melnikov D.A. Polymer composite materials based on thermosetting polyimide binders for aerospace engineering. Review. Voprosy materialovedeniya, 2016, no. 4 (88), pp. 50‒62.
  12. Chursova L.V., Panina N.N., Grebeneva T.A., Kutergina I.Yu. Epoxy resins, hardeners, modifiers and binders based on them. St. Petersburg: Profession, 2020, 576 p.
  13. Veshkin E.A., Satdinov R.A., Barannikov A.A. Modern materials for the aircraft cabin. Trudy VIAM, 2021, no. 9 (103), paper no. 04. Available at: http://www.viam-works.ru (accessed: March 01, 2024). DOI: 10.18577/2307-6046-2021-0-9-33-42.
  14. Kovalenko A.V., Sidelnikov N.K., Sokolov I.I., Tundaykin K.O. Spheroplastic with adjustable viscosity for filling sections of honeycomb structures. Trudy VIAM, 2019, no. 11 (83), paper no. 04. Available at: http://www.viam-works.ru (accessed: March 01, 2024). DOI: 10.18577/2307-6046-2019-0-11-37-43.
  15. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  16. Aristova Е.Yu., Denisova V.А., Drozhzhin V.S. et al. Composite materials using hollow microspheres. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 52–57. DOI: 10.18577/2071-9140-2018-0-1-52-57.
  17. Kutsevich K.E., Tyumeneva T.Yu., Petrova A.P. Influence of fillers on properties of adhesive prepregs and PCM on their basis. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 51–55. DOI: 10.18577/2071-9140-2017-0-4-51-55.
  18. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  19. Polyamide hardeners CHIMEX Limited LTD. Available at: http://chimexltd.com/catalog/otverditeli-uskoriteli-otverzhdeniya/poliamidnye-otverditeli/ (accessed: March 01, 2024).
  20. Osipchik V.S., Olikhova Yu.V., Nguyen L.H., Lushcheykin G.A., Aristov V.M. Determination of the glass transition temperature of an epoxy-siloxane composition by thermal analysis methods. Plasticheskiye massy, 2017, no. 7–8, pp. 34‒37.