Kosarina E.I., Grimova A.P., Osiyanenko N.V., Smirnov A.V. Modes of X-ray exposure for parts, made using additive technologies // Proceedings of VIAM. 2024. No. 12. Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-12-85-95.

Modes of X-ray exposure for parts, made using additive technologies

Kosarina E.I., Grimova A.P., Osiyanenko N.V., Smirnov A.V.
Abstract

The values of linear radiation attenuation coefficients for metal powders for additive technologies and their foundry analogues depending on the anode voltage on the X-ray tube are calculated. Alloys based on iron, nickel, titanium, aluminum and pure metals were considered, and the coefficients were calculated for three values of anode voltage. It has been theoretically established and experimentally confirmed that the GOST 20426‒82 regulations can be used for parts produced by additive technologies.

Keywords
additive technologies, metal powders, casting alloys, radiation energy, linear radiation attenuation coefficient, radiation image contrast, control sensitivity
Reference list
  1. Sirotkin O.S. Current state and development prospects of additive technologies. Aviatsionnaya promyshlennost, 2015, no. 2, pp. 22–25.
  2. Kablov E.N., Evgenov A.G., Bakradze M.M., Nerush S.V., Krupnina O.A. New generation materials and digital additive technologies for the production of resource parts of FSUE VIAM. Part 1. Materials and synthesis technologies. Elektrometallurgiya, 2022, no. 1, pp. 2–12.
  3. Shishkovsky I.V. Fundamentals of high-resolution additive technologies. St. Petersburg: Piter, 2015, 348 p.
  4. Zelenko M.A., Popovich A.A., Mutylina I.M. Additive technologies in mechanical engineering. St. Petersburg: SPbPU, 2013, 222 p.
  5. Seifi M., Gorelik M., Waller J. et al. Progress towards metal additive manufacturing standardization to support qualification and certification. JOM, 2017, no. 69 (3), pp. 439–455.
  6. Waller J.M., Parker B.H., Hodges K.L. et al. Non-Destructive Testing Methods for Products by Additive Manufacturing. Journal of the Korean Society for Nondestructive testing, 2016, vol. 36, is. 4, pp. 308–314.
  7. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  8. Nerush S.V., Kaplanskii Yu.Yu., Dynin N.V., Benarieb I., Savichev I.D. Development of laser powder bed fusion parameters, structure and mechanical properties of a high-strength aluminum alloy Al–Ce–Cu. Trudy VIAM, 2023, no. 1 (119), paper no. 05. Available at: http://www.viam-works.ru (accessed: May 12, 2024). DOI: 10.18577/2307-6046-2023-0-1-50-68.
  9. Sukhov D.I., Kaplansky Yu.Yu., Rogalev A.M., Kurkin S.E. The features of processing Cr-rich nickel based alloy by selective laser melting. Trudy VIAM, 2023, no. 1 (119), paper no. 02. Available at: http://www.viam-works.ru (accessed: May 13, 2024). DOI: 10.18557/2307-6046-2023-0-1-15-27.
  10. Evgenov A.G., Shurtakov S.V., Chumanov I.R. New wear-resistant cobalt-base alloy: features of the structure of the metal obtained by the direct laser growth method. Part 2. Aviation materials and technologies, 2022, no. 3 (68), paper no. 04. Available at: http://www.journal.viam.ru (accessed: May 13, 2024). DOI: 10.18577/2713-0193-2022-0-3-37-49.
  11. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 2. Aviation materials and technologies, 2023, no. 2 (71), paper no. 01. Available at: http://www.journal.viam.ru (accessed: May 13, 2024). DOI: 10.18577/2713-0193-2023-0-2-3-22.
  12. Shablov S.V., Kosarina E.I., Mikhailova N.A., Demidov A. A. Physical foundations and practice of radiation non-destructive testing. Moscow: Spektr, 2023, 168 p.
  13. State Standard 20426–82. Non-destructive testing. Radiation flaw detection methods. Scope. Moscow: Publ. House of Standards, 1982, 23 p.
  14. Demidov A.A., Stepanov A.V., Turbin Ye.M., Krupnina O.A. The х-ray testing modes providing with radiation imaging with predetermined contrast. Aviacionnye materialy i tehnologii, 2016, no. 4 (45), pp. 80–85. DOI: 10.18577/2071-9140-2016-0-4-80-85.
  15. Stepanov A.V., Kosarina E.I. Requirements for radiographic non-destructive testing in Russian and foreign standards. Kommentarii k standartam, TU, sertifikatam, 2013, no. 9, pp. 2–7.
  16. Gtate Standard ISO 17636:1–2017. Non-destructive testing of welded joints. Radiographic testing. Part 1. Methods of X-ray and gamma-ray testing using film. Moscow: Standartinform, 2022, 36 p.