Vlasov I.I., Sevalnev G.S., Lyakhov A.A., Nefedkin D.Yu. Study of the structure and mechanical properties of Ni–Co–Cr entropy alloy in the cast state // Proceedings of VIAM. 2024. No. 12. Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-12-18-30.

Study of the structure and mechanical properties of Ni–Co–Cr entropy alloy in the cast state

Vlasov I.I., Sevalnev G.S., Lyakhov A.A., Nefedkin D.Yu.
Abstract

In the article were studied the microstructure, phase composition, and the change in mechanical properties depending on the test temperature of the high-entropy alloy in the NiCoCrWNbAlTiReC system after vacuum induction melting. According to the results of the studies and tests, it was established that the alloy structure consists of a FCC solid solution with excess phases, with the implementation of the mechanism of strain hardening at the test temperature of 20 °C and structural-phase transformations in the temperature range of 900–1100 °C.

Keywords
entropy alloys, alloying, structure, phase composition, hardness, mechanical properties
Reference list
  1. Sevalnev G.S., Korobova E.N., Dvoreckov R.M., Doroshenko A.V., Muzafarova S.-V.R., Samoilova I.I. Influence of the degree of martensitic structure dispersion and size of carbide phase on the frictional interaction under conditions of dry sliding friction of high-carbon complex alloy steel. Trudy VIAM, 2022, no. 6 (112), paper no. 03. Available at: http://www.viam-works.ru (accessed: July 25, 2024). DOI: 10.18577/2307-6046-2022-0-6-15-26.
  2. Sevalnev G.S. Beryllium-containing steels – perspective material with a high level of physical and mechanical properties. Aviation materials and technologies, 2023, no. 3 (72), paper no. 02. Available at: http://www.journal.viam.ru (accessed: July 25, 2024). DOI: 10.18577/2713-0193-2023-0-3-15-29.
  3. Kaplanskii Yu.Yu., Mazalov P.B. World trends in the development of refractory high-entropy alloys for heat-loaded units of aerospace technics (review). Aviation materials and technologies, 2022, no. 2 (67), paper no. 03. Available at: http://www.journal.viam.ru (accessed: July 25, 2024). DOI: 10.18577/2713-0193-2022-0-2-30-42.
  4. Kablov E.N., Sidorov V.V., Min P.G., Vadeev V.E., Kramer V.V. Research and development of technological parameters for vacuum melting of corrosion-resistant heat-resistant nickel alloys. Metallurg, 2021, no. 2, pp. 62–67.
  5. Yeh J.-W., Chen Y.-L., Lin S.-J., Chen S.-K. High-entropy alloys – a new era of exploitation. Materials Science Forum, 2007, vol. 560, pp. 1–9. DOI: 10.4028/www.scientifi c.net/MSF.560.1.
  6. Cantor B., Chang I.T.H., Knight P., Vincent A.J.B. Microstructural development in equiatomic multicomponent alloys. Materials Science and Engineering: A, 2004, vol. 375–377, pp. 213–218. DOI: 10.1016/j.msea.2003.10.257.
  7. Cantor B. Multicomponent and high entropy alloys. Entropy, 2014, vol. 16, no. 9, pp. 4749–4768.
  8. Yeh J.-W., Chen S.-K., Lin S.-J. et al. Nanostructured highentropy alloys with multiple principal elements: novel alloy design concepts and outcomes. Advanced Engineering Materials, 2004, vol. 6, pp. 299–303. DOI: 10.1002/adem.200300567.
  9. Yeh J.W. Recent progress in high-entropy alloys. Annales de Chimie-Science des Materiaux, 2006, vol. 31, pp. 633–648. DOI: 10.3166/acsm.31.633-648.
  10. Yeh J.-W., Chen S.-K., Gan J.-Y. et al. Formation of simple crystal structures in Cu‒Co‒Ni‒Cr‒Al‒Fe‒Ti‒V alloys with multiprincipal metallic elements. Metallurgical and Materials Transactions: A, 2004, vol. 35, pp. 2533–2536. DOI: 10.1007/s11661-006-0234-4.
  11. Singh S., Wanderka N., Glatzel U., Banhart J. Decomposition in multi-component AlCoCrCuFeNi highentropy alloy. Acta Materialia, 2011, vol. 59, pp. 182–190. DOI: 10.1016/j.actamat.2010.09.023.
  12. Trofimenko N.N., Efimochkin I.Yu., Bolshakova A.N. Problems of creation and prospects for the use of heat-resistant high-entropy alloys. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 3–8. DOI: 10.18577/2071-9140-2018-0-2-3-8.
  13. Trofimenko N.N., Efimochkin I.Yu., Osin I.V., Dvoretskov R.M. The research of the possibility of high entropy alloy VNbMoTaW production by mixing elementary powders with further hybrid spark plasma sintering. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 12–20. DOI: 10.18577/2071-9140-2019-0-2-12-20.
  14. George E.P., Raabe D., Ritchie R.O. High-entropy alloys. Nature Reviews Materials, 2019, vol. 4, pp. 515–534. DOI: 10.1038/s41578-019-0121-4.
  15. Zhang Y., Zhou Y.J., Lin J.P. et al. Solid-solution phase formation rules for multi-component alloys. Advanced Engineering Materials, 2018, vol. 10 (6), pp. 534–538. DOI: 10.1002/adem.200700240.
  16. Smith T. GRX-810: NASA High Temperature Alloy Development for Additive Manufacturing. Lawrence Livermore National Lab Seminar, 2022. Available at: https://ntrs.nasa.gov/citations/20220013032 (accessed: July 25, 2024).
  17. Smith T. High Temperature Alloy Development for AM–GRX-810. Bridging the Gap Webinar: Emerging Additive Manufacturing Materials. 2023. Available at: ntrs.nasa.gov/citations/20230010486 (accessed: July 25, 2024).
  18. NASA’s New Material Built to Withstand Extreme Conditions. Available at: https://www.nasa.gov/aeronautics/nasas-new-material-built-to-withstand-extreme-conditions/ (accessed: July 25, 2024).
  19. The Materials Project. Available at: next-gen.materialsproject.org (accessed: July 25, 2024).
  20. Johnson G.R., Cook W.N. A constitutive model and data for metals subjected to large strains. High rates and high temperatures. Proceedings of the 7th Intern. symp. on ballistics (Hague, Netherlands, Apr. 19–21, 1983). Hague: Roy. Inst. of Engrs in the Netherlands, 1983, pp. 541–547.
  21. Johnson G.R., Cook W.H. Fracture characteristics of three metals subjected to various strains, strain rates, temperatures, and pressures. Engineering fracture mechanism, 1985, vol. 21, no. 1, pp. 31–48.
  22. Lukin E.I., Ashmarin A.A., Bannykh I.O. et al. Study of the influence of the reduction value during cold rolling on the phase composition, texture and residual stresses in 20Kh15AN3MD2 steel. Metally, 2023, no. 6, pp. 26–34. DOI: 10.31857/S0869573323060046.
  23. Sevalnev G.S., Gromov V.I., Dulnev K.V., Sevalneva T.G. Contact endurance of nitrogenous austenitic-martensitic steels with different hardening mechanism. Aviation materials and technologies, 2024, no. 2 (75), paper no. 01. Available at: http://www.journal.viam.ru (accessed: July 25, 2024). DOI: 10.18577/2713-0193-2024-0-2-3-14.