Antipov V.V., Varrik N.M., Maximov V.G., Lugovoy A.A., Babashov V.G., Shavnev A.A. Study of mechanical and thermal characteristics of a porous ceramic material based on mullite // Proceedings of VIAM. 2023. No. 6 (124). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-6-38-45.

Study of mechanical and thermal characteristics of a porous ceramic material based on mullite

Antipov V.V., Varrik N.M., Maximov V.G., Lugovoy A.A., Babashov V.G., Shavnev A.A.
Abstract

Porous ceramic materials are in demand in many industries using high-temperature furnaces and other equipment operating at elevated temperatures. In this work, a porous ceramic material was obtained from a mullite fiber, and a solid binder containing fine boron powder and crushed quartz fibers was used as a binder. Samples of porous ceramic materials were obtained and their mechanical and thermal characteristics after heat treatment at various temperatures were evaluated.

Keywords
ceramic material, mullite, refractory fibers, heat resistance, aluminum oxide
Reference list
  1. Zok F.W. Developments in oxide fiber composites. Journal of the American Ceramic Society, 2006, vol. 89, no. 11, pp. 3309–3324.
  2. Sadik C., El Amranib I.-E., Albizane A. Recent advances in silica-alumina refractory: A review. Journal of Asian Ceramic Societies, 2014, vol. 2, pp. 83–96.
  3. Parlier M., Ritti M.H. State of the art and perspectives for oxide/oxide composites. Aerospace Science and Technology, 2003, vol. 7, no. 3, pp. 211–221.
  4. Buznik V.M., Kablov E.N. Arctic materials sciences. Tomsk: Tomsk State Univ., 2018, is. 3, 44 p.
  5. Babashov V.G., Maksimov V.G., Varrik N.M., Samorodova O.N. Studying of structure and properties of samples of ceramic composite materials on the basis of mullite. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 54–63. DOI: 10.8577/2071-9140-2020-0-1-54-63.
  6. Baklouti S., Bouaziz J., Chartier T., Baumard J.-F. Binder burnout and evolution of the mechanical strength of dry-pressed ceramics containing poly (vinyl alcohol). Journal of the European Ceramic Society, 2001, vol. 21, no. 8, pp. 1087–1092.
  7. Wiśniewska M., Chibowski S., Urban T., Sternik D. Investigation of the alumina properties with adsorbed polyvinyl alcohol. Journal of Thermal Analysis and Calorimetry, 2011, vol. 103, no. 1, pp. 329–337.
  8. Process for gelling a sol in fiberformed ceramic insulation: pat. 5021369 USA; filed 01.08.88; publ. 04.06.91.
  9. Refractory fibrous ceramic insulation and process of making same: pat. 6183852 USA; filed 11.03.94; publ. 06.02.01.
  10. Thermal insulation system employing oxide ceramic matrix composite: pat. 6969546 USA; filed 20.10.03; publ. 29.11.05.
  11. Bonding of Thermal Tile Insulation: pat. 6494979 USA; filed 29.09.00; publ. 17.12.02.
  12. Buchilin N.V., Lyulyukina G.Yu., Varrik N.M. Influence of the mode of roasting on structure and property of high-porous ceramic mullite materials. Trudy VIAM, 2017, no. 5 (53), paper no. 04. Available at: http://www.viam-works.ru (accessed: October 05, 2020). DOI: 10.18577/2307-6046-2017-0-5-4-4.
  13. Kudryavtsev P.G., Figovsky O.L. Inorganic heat-resistant binders. Nanotekhnologii v stroitelstve, 2017, vol. 9, no. 2, pp. 66–81. Available at: http://nanobuild.ru/ru_RU/journal/Nanobuild-2-2017/66-81.pdf (accessed: October 05, 2020). DOI: 10.15828/2075-8545-2017-9-2-66-81.
  14. Aviation materials: reference book in 13 vols. Ed. E.N. Kablov. Moscow: VIAM, 2011, vol. 9: Heat-shielding, heat-insulating and composite materials, high-temperature non-metallic coatings, pp. 31–37.
  15. Zuev A.V., Zarichnyak Yu.P., Barinov D.Ya., Krasnov L.L. Measurement of thermophysical properties of flexible thermal insulation. Aviation materials and technology, 2021, no. 1 (62), paper no. 11. Available at: http://www.journal.viam.ru (accessed: January 30, 2023). DOI: 10.18577/2713-0193-2021-0-1-119-126.
  16. Oreshko E.I., Erasov V.S., Krylov V.D. Construction of 3D stress-strain diagram for the analysis of mechanical behavior of the material tested at various loading rates. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 59–66. DOI: 10.18577/2071-9140-2018-0-2-59-66.
  17. Barinov D.Ya., Shorstov S.Yu., Razmahov M.G., Gulyaev A.I. Examination of thermophysical characteristics of a heat-protective material based on fiberglass during destruction. Aviation materials and technologies, 2021, no. 4 (65), paper no. 10. Available at: http://www.journal.viam.ru (accessed: January 30, 2023). DOI: 10.18577/2713-0193-2021-0-4-91-97.