Kolokoltseva T.V., Popov J.O., Usacheva M.N., Gromova A.A. Prepregs of fiberglass and prepreg of carbon fiber on the basis of the resin VSE-67 for the use in the structures of helicopter blades // Proceedings of VIAM. 2023. No. 11 (129). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-11-47-55.

Prepregs of fiberglass and prepreg of carbon fiber on the basis of the resin VSE-67 for the use in the structures of helicopter blades

Kolokoltseva T.V., Popov J.O., Usacheva M.N., Gromova A.A.
Abstract

This article presents the main results on the development of prepregs and polymer composite materials (fiberglass and carbon fiber) based on the melting epoxy resin union and reinforcing fillers-glass-circuits of the T-64(VMP)-78, glass-winding RVMPN10-1200-14 and carbon fiber UMT49S-12K-EP. The process of developing prepregs, technologies for their manufacture on the impregnation, the choice of the main parameters of impregnation is described. The results of a study of the properties of the prepregs obtained under selected technological regimes and made from them PCM are also given.

Keywords
fiberglass, carbon fiber, prepregs, helicopter blades, resin, polymer composite materials, aviation products
Reference list
  1. Composites take off ... in some civil helicopters. Available at: https://www.compositesworld.com/articles/composites-take-off-in-some-civil-helicopters (accessed: July 22, 2023).
  2. Basharov E.A., Vagin A.Yu. Analysis of the use of composite materials in the design of helicopter airframes. Trudy MAI, 2017, no. 92, pp. 1–33.
  3. Composites-intensive helicopter makes commercial debut. CompositesWorld.com. Available at: https://www.compositesworld.com/news/composites-intensive-helicopter-makes-commercial-debut (accessed: July 22, 2023).
  4. Weber T.A., Ruff-Stahl H.-J.K. Advances in Composite Manufacturing of Helicopter Parts. International Journal of Aviation, Aeronautics and Aerospace, 2017, vol. 4, is. 1, pp. 1–33.
  5. Kablov E.N., Erofeev V.T., Zotkina M.M., Dergunova A.V., Moiseev V.V., Rimshin V.I. Plasticized epoxy composites for manufacturing of composite reinforcement. Journal of Physics: Conference Series: International Conference on Engineering Systems 2020, 2020, vol. 1687, p. 012031.
  6. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports XXI Mendeleev Congress on General and Applied Chemistry: in 6 vol. St. Petersburg, 2019, vol. 4, p. 24.
  7. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  8. Gunyaev G.M., Sorina T.G., Khoroshilova I.P., Rumyantsev A.F. Structural epoxy carbon fiber reinforced plastics. Aviatsionnaya promyshlennost, 1984, no. 12, pp. 2–16.
  9. Belinis P.G., Lukyanenko Yu.V., Rogozhnikov V.N., Tsykun R.G., Donetskiy K.I. Design research on a constructural multilayer woven preform of an integral panel fragment for aircraft. Aviation materials and technologies, 2023, no. 3 (72), paper no. 09. Available at: http://www.journal.viam.ru (accessed: August 29, 2023). DOI: 10.18577/2713-0193-2023-0-3-114-124.
  10. Antipov V.V., Somov A.V., Sidelnikov V.V., Nefedova Yu.N., Ogurtsov P.S., Soloviev V.A. Technological features of shaping fire-resistant light laminated material for helicopter engine hood manufacturing. Aviation materials and technologies, 2023, no. 3 (72), paper no. 07. Available at: http://www.journal.viam.ru (accessed: August 29, 2023). DOI: 10.18577/2713-0193-2023-0-3-90-100.
  11. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: August 29, 2023). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  12. Zavalov O.A. Design of helicopter rotors and tail rotors. Moscow: MAI, 2001, 72 p.
  13. Popov Y.O., Kolokolceva T.V., Gusev Y.A., Gromova A.A. Development of the constructive and technological solution for a sheet fibreglass for tail section skins of helicopter rotor blades. Trudy VIAM, 2016, no. 1 (37), paper no. 05. Available at: http://www.viam-works.ru (accessed: July 28, 2023). DOI: 10.18577/2307-6046-2016-0-1-42-49.
  14. Miychenko I.P. Technology of semi-finished polymer materials. St. Petersburg: NOT, 2012. 374 p.
  15. Composite Materials Handbook-17. SAE International, 2012. Vol. 1: Polymer matrix composites guidelines for characterization of structural materials, р. 96.
  16. Kolokoltseva T.V., Popov Yu.O., Usacheva M.N., Gromova A.A. Prepregs and fiberglass based on VSR-3М binder and fiberglass fabrics for use in helicopter blades. Trudy VIAM, 2018, no. 3 (109), paper no. 03. Available at: http://www.viam-works.ru (accessed: July 27, 2023). DOI: 10.18577/2307-6046-2022-0-3-27-34.