Gorbovets M.A., Golinets S.A, Sukhov D.I., Monin S.A. Research of characteristics of durability of the alloy of Co–Cr–Ni–W–Ta system, obtained by SLM // Proceedings of VIAM. 2022. No. 2 (108). Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-2-111-121.

Research of characteristics of durability of the alloy of Co–Cr–Ni–W–Ta system, obtained by SLM

Gorbovets M.A., Golinets S.A, Sukhov D.I., Monin S.A.
Abstract

Additive manufacturing is increasingly used in the aviation industry. Its main feature is the manufacture of parts of complex external and internal geometric shapes without increasing the cost of their production. To calculate the resource of nodes and reliable operation of new equipment, it is necessary to have a set of calculated values of characteristics of structural strength, including the characteristics of tensile, creep rupture and high-cycle fatigue (HCF). The study of characteristics of tensile, creep rupture and HCF of the Co–Cr–Ni–W–Ta alloy obtained by the method of selective laser melting (SLM) is presented in this paper.

Keywords
cobalt alloy, selective laser melting, metal powder composition, mechanical properties, testing temperature, strength characteristics
Reference list
  1. Kablov E.N. Additive technologies - the dominant of the national technological initiative. Intellekt i tekhnologii, 2015, no. 2 (11), pp. 52–55.
  2. Kablov E.N. Present and future of additive technologies. Metally Evrazii, 2017, no. 1, pp. 2–6.
  3. Graf B., Gook S.E., Gumenyuk A.V., Retmayer M. Combined laser additive technologies for the production of turbine blades of complex geometric shape. Globalnaya yadernaya bezopasnost, 2016, no. 3 (20), pp. 34–42.
  4. Bytsenko O.A., Chabina E.B., Filonova E.V., Rogalev A.M. Interrelation of structural defects in heat-resistant nickel alloy obtained by selective laser alloying, strategy and scanning parameters. Nauka i obrazovanie, 2016, no. 3, pp. 121–132.
  5. Min P.G., Vadeev V.E., Rogalev A.M., Knyazev A.E. Study of the chemical composition, structure and mechanical properties of the EP648 alloy at various stages of additive manufacturing. Materialovedenie, 2018, no. 12, pp. 17–22.
  6. Kablov E.N. VIAM materials and technologies for Aviadvigatel. Permskiye aviatsionnye dvigateli, 2014, no. 31, pp. 43–47.
  7. Di W., Yongqiang Ya., Xubin S., Yonghua Ch. Study on energy input and its influences on single-track, multi-track, and multi-layer in SLM. The International Journal of Advanced Manufacturing Technology, 2012, vol. 58, is. 9, pp. 1189–1199.
  8. Strano G., Hao L., Everson R.M., Evans K.E. Surface roughness analysis, modeling and prediction in selective laser melting. Journal of Materials Processing Technology, 2013, vol. 213, no. 4, pp. 589–597.
  9. Smurov I.Yu., Movchan I.A., Yadroitsev I.A. et al. Additive manufacturing using a laser. Vestnik MGTU «Stankin», 2011, vol. 2, no. 4, pp. 144–146.
  10. Deng D., Peng R.L., Brodin H., Moverare J. Microstructure and mechanical properties of Inconel 718 produced by selective laser melting: sample orientation dependence and effects of post heat treatments. Materials Science & Engineering A, 2018, vol. 713, pp. 294–306. DOI: 10.1016/j.msea.2017.12.043.
  11. Zhou L., Mehta A., McWilliams B. et al. Microstructure, precipitations and mechanical properties of powder bed fused Inconel 718 before and after heat treatment. Journal of Materials Science and Technology, 2019, vol. 35, is. 6, pp. 1153–1164. DOI: 10.1016/j.jmst.2018.12.006.
  12. Tucho M., Cullivier P., Sjolyst-Kverneland A., Hansen V. Microstructure and hardness studies of Inconel 718 manufactured by selective laser melting before and after solution heat treatment. Materials Science & Engineering A, 2017, vol. 689, pp. 220–232. DOI: 10.1016/j.msea.2017.02.062.
  13. Kuo Y.-L., Nagahari T., Kakehi K. The Effect of Post-Processes on the Microstructure and Creep Properties of Alloy718 Built Up by Selective Laser Melting. Materials (Basel), 2018, vol. 11(6), pp. 183–192. DOI: 10.3390/ma11060996.
  14. Sukhov D.I., Nerush S.V., Efimochkin I.Yu., Karachevchev F.N., Bogachev I.A. Production of MMC based on VZh159 alloy by selective laser melting. Aviation materials and technologies, 2021, no. 2 (63), paper no. 07. Available at: http://www.journal.viam.ru (accessed: November 2, 2021). DOI: 10.18577/2713-0193-2021-0-2-62-72.
  15. Evgenov A.G., Rogalev A.M., Karachevtsev F.N., Mazalov I.S. Influence of hot isostatic pressing and heat treatment on the properties of the EP648 alloy synthesized by the method of selective laser alloying. Tekhnologiya mashinostroeniya, 2015, no. 9, pp. 11–16.
  16. Evgenov A.G., Shurtakov S.V., Prager S.M., Malinin R.Yu. On the development of a universal calculation method for assessing the degradation of recycled metal powder materials, depending on the cyclicity of use in the selective laser melting process. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-4-3-11.
  17. Evgenov A.G., Gorbovec M.A., Prager S.M. Structure and mechanical properties of heat resistant alloys VZh159 and EP648, prepared by selective laser fusing. Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 8–15. DOI: 10.18577/2071-9140-2016-0-S1-8-15.
  18. Kablov E.N., Evgenov A.G., Ospennikova O.G., Semenov B.I., Semenov A.B., Korolev V.A. Metal-powder compositions of heat-resistant alloy EP648 produced by FGUP "VIAM" SSC of the RF in technologies of selective laser alloying, laser gas-powder surfacing and high-precision casting of polymers filled with metal powders. Izvestiya vysshikh uchebnykh zavedeniy. Mashinostroyenie, 2016, no. 9 (678), pp. 62–80.
  19. Kablov E.N., Evgenov A.G., Mazalov I.S., Shurtakov S.V., Zaitsev D.V., Prager S.M. Structure and properties of EP648 and VZh159 alloys synthesized by selective laser melting after simulation annealing. Materialovedenie, 2020, no. 6, pp. 3–10.
  20. Gorbovets M.A., Belyayev M.S., Ryzhkov P.V. Fatigue strength of heat-resistant nickel alloys produced by selec-tive laser melting. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 50–55. DOI: 10.18577/2071-9140-2018-0-3-50-55.
  21. Podyachev V.N., Demonis I.M., Baranova O.A. Laboratory of Refractory Alloys of VIAM and its first head A.S. Stroev. To the 55th anniversary of the organization. Istoriya nauki i tekhniki, 2013, no. 4, pp. 19–25.
  22. Kazantseva N.V., Ezhov I.V., Davydov D.I., Merkushev A.G. Analysis of the structure and mechanical properties of the Co–Cr–Mo alloy obtained by 3D printing. Fizika metallov i metallovedenie, 2019, vol. 120, no. 12, pp. 1271–1278.
  23. Mazalov I.S., Mazalov P.B., Suhov D.I., Sulyanova E.A. Influence of hot isostatic pressing parameters on structure and properties of cobalt-based alloys obtained by selective laser melting. Aviation materials and technologies, 2021, no. 2 (63), paper no. 01. Available at: http://www.journal.viam.ru (accessed: November 2, 2021). DOI: 10.18577/2713-0193-2021-0-2-3-14.
  24. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  25. Kablov E.N., Golubovsky E.R. Heat resistance of nickel alloys. Moscow: Mashinostroenie, 1998, 463 p.
  26. Stepnov M.N. Statistical methods for processing the results of mechanical tests. Moscow: Mashinostroenie, 1985, 232 p.
  27. Shkolnik L.M. Fatigue Test Methodology: handbook. Moscow: Metallurgiya, 1978, 304 p.