Merkulova Yu.I., Serdcelyubova A.S., Zheleznyak V.G. Lacquer coating system based on cold dry polyurethane enamel for protecting nose spinners of planes // Proceedings of VIAM. 2021. No. 8 (102). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-8-59-66.

Lacquer coating system based on cold dry polyurethane enamel for protecting nose spinners of planes

Merkulova Yu.I., Serdcelyubova A.S., Zheleznyak V.G.
Abstract

Recently in the aviation industry there has been an increasing demand for the development of functional paints and varnishes, in particular, for the production of coatings intended to protect aviation equipment from abrasion and erosion damaged. Coatings of this type are especially relevant for polymer products. This work is devoted to the development of a new polyurethane enamel for the protection of antenna radomes. The comparative data of fluoroplastic, polyurethane imported enamel, enamels based on chlorosulfonated polyethylene and fluorinated rubber, intended for protection of abrasive damage.

Keywords
paint materials, functional coatings, erosion resistant, polymer materials, coating system, polyurethane enamel.
Reference list
  1. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  2. Zhelezina G.F., Solovyeva N.A., Makrushin K.V., Rysin L.S. Polymer composite materials for manufacturing engine air particle separation of advanced helicopter engine. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 58–63. DOI: 10.18577/2071-9140-2018-0-1-58-63.
  3. Gunyayeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
  4. Nefedov N.I., Semenova L.V., Kuznecova V.A., Vereninova N.P. Paint coatings for protection of metallic and polymer composite materials against aging, corrosion and biodeterioration. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 393–404. DOI: 10.18577/2071-9140-2017-0-S-393-404.
  5. Kablov E.N. Materials for aerospace technology. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, pp. 7–27.
  6. Kablov E.N. The main directions of development of materials for aerospace technology of the XXI century. Perspektivnye materialy, 2000, no. 3, pp. 27–36.
  7. Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products. Trudy VIAM, 2019, no. 5 (77), paper no. 07. Available at: http://www.viam-works.ru. (accessed: July 7, 2021). DOI: 10.18577/2307-6046-2019-0-5-62-67.
  8. Kondrashov E.K., Vladimirsky V.N., Beider E.Ya. Erosion-resistant paints and varnishes. Moscow: Chemistry, 1989, 136 p.
  9. Kuznetsova V.A., Vladimirsky V.N., Kondrashov E.K. Prediction of erosion resistance of paint and varnish coatings taking into account dynamic parameters. Paints and varnishes and coatings. Aviation materials and technologies. Moscow: VIAM, 2003, pp. 50–53.
  10. Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A. The main directions of improving the operational, technological and environmental characteristics of paint and varnish coatings for aviation technology. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 96–102.
  11. Kondrashov E.K., Naidenov N.D. Erosion resistant paint coverings of aviation purpose. Part 1. Erosion resistant paint coatings based on epoxy and polyurethane films forming (review). Trudy VIAM, 2020, no. 2 (86), paper no. 09. Available at: http://www.viam-works.ru (accessed: February 20, 2020). DOI: 10.18577/2307-6046-2020-0-2-81-90. (accessed: July 7, 2021).
  12. Kondrashov E.K. Paints and varnishes and coatings based on them in mechanical engineering. Moscow: Paint-Media, 2021, 256 p.
  13. Pavlov A.V., Merkulova Yu.I., Zelenskaya A.D., Zheleznyak V.G. Wear resistance of paint and varnish coatings (literature review). Lakokrasochnye materialy i ikh primenenie, 2018, no. 1–2, pp. 40–43.
  14. Yakovlev A.D. Chemistry and technology of paints and varnishes: textbook for universities. Leningrad: Chemistry, 1989, 84 p.
  15. Zubarev P.A. Protective wear-resistant coatings based on modified polyurethanes: thesis, Cand. Sc. (Tech.). Penza: PGUAS, 2014, 156 p.
  16. Zubarev P.A., Lakhno A.V. Wear-resistant polyurethane coatings. Molodoy ucheny, 2014, no. 20, pp. 143–146.
  17. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  18. Semenova L.V., Kondrashov E.K. Modified bromine epoxy Aviacionnye materialy i tehnologii, 2010, no. 1, pp. 29–32.