Pykhtin A.A., Sorokin A.E., Larionov S.A., Lonskii S.L. Study of the influence of non-covalent modifiers on the structure and properties of polymer filaments for FDM-printing based on ABS-plastic and carbon nanoparticles // Proceedings of VIAM. 2021. No. 10 (104). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-10-36-44.

Study of the influence of non-covalent modifiers on the structure and properties of polymer filaments for FDM-printing based on ABS-plastic and carbon nanoparticles

Pykhtin A.A., Sorokin A.E., Larionov S.A., Lonskii S.L.
Abstract

The paper presents the results of a study of the effect of non-covalent modifiers on the structure and properties of polymer filaments for FDM-printing based on ABS-plastic and carbon nanoparticles. The dependences of the characteristics of nanocomposites and filaments based on them to the type of functionalization have been established. The effect of the concentration of CNTs on the hardness, water absorption, electrical resistance, and shear strength for modified polymer filament has been investigated. The optimal formulations and technological parameters of FDM-printing of templates have been determined. 

Keywords
nanotechnology, additive technologies, filament, FDM-printing, carbon nanotubes, dispersant, ABS-plastic, template.
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Semenova L.V., Petrova G.N. and other Polymer composite materials on a thermoplastic matrix. Izvestiya vysshikh uchebnykh zavedeniy. Ser,: Chemistry and Chemical Technology. 2016, vol. 59, no. 10, pp. 61.
  3. Kablov E.N., Startsev V.O., Inozemtsev A.A. The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
  4. Kraev I.D., Popkov O.V., Shuldeshov E.M., Sorokin A.E., Yurkov G.Yu. Prospects for the use of organosilicon elastomers in the development of modern polymer materials and coatings for various purposes. Trudy VIAM, 2017, no. 12 (60), paper no. 5. Available at: http://www.viam-works.ru (accessed: June 28, 2021). DOI: 10.18577/2307-6046-2017-0-12-5-5.
  5. Sorokin A.E., Platonov M.M., Larionov S.A. Selective laser sintering of polymer compositions based on polyamide 12. Trudy VIAM, 2017, no. 9, paper no. 05. Available at: http://www.viam-works.ru (accessed: June 28, 2021). DOI: 10.18577/2307-6046-2017-0-9-5-5.
  6. Kirin B.S., Lonskii S.L., Petrova G.N., So-rokin A.E. Materials for the 3D-printing on the basis of polyetheretherketones. Trudy VIAM, 2019, no. 4 (76), paper no. 03. Available at: http://viam-works.ru (accessed: June 28, 2021). DOI: 10.18577/2307-6046-2019-0-4-21-29.
  7. Kablov E.N. Trends and guidelines for innovative development in Russia: Collection of scientific information materials. 3rd ed. Moscow: VIAM, 2015, 720 p.
  8. Bikas H., Stavropoulos P., Chryssolouris G. Additive manufacturing methods and modeling approaches: a critical review. The International Journal of Advanced Manufacturing Technology, 2016, vol. 83, pp. 389–405. DOI: 10.1007/s00170-015-7576-2.
  9. Lobanov M.V., Voronov V.A., Kondrat’ev S.A., Govorov V.A., Bobrikov I.A., Balaguroc A.M., Belyaev A.A., Medvedev P.N., Lebedeva Yu.E., Sorokin A.E. Preparation of submicron CaCu3Ti4O12 dispersions and filled epoxy compositions based on them. Inorganic Materials, 2019, vol. 55, no. 8, pp. 856–863.
  10. Petrova G.N., Larionov S.A., Sorokin A.E., Sapego Yu.A. Modern ways of processing of thermoplastics. Trudy VIAM, 2017, no. 11 (59), paper no. 07. Available at: http://www.viam-works.ru (accessed: June 28, 2021). DOI: 10.18577/2307-6046-2017-0-11-7-7.
  11. Kablov E.N. Additive technologies are the dominant feature of the national technology initiative. Intellekt i tekhnologii, 2015, no. 2 (11), pp. 52–55.
  12. Kablov E.N. Present and future of additive technologies. Metally of Evrazii, 2017, no. 1, pp. 2–6.
  13. Schmid M., Kleijnen R., Vetterli M. et al. Influence of the Origin of Polyamide 12 Powder on the Laser Sintering Process and Laser Sintered Parts. Applied Sciences, 2017, vol. 7, pp. 462.
  14. Turnkey continuous fiber 3D printing solutions for producing anisoprinted composite parts. Stronger, lighter and cheaper than metal or non-optimal composites. Available at: https://anisoprint.com/solutions (accessed: June 28, 2021).
  15. The backbone of aluminum-strength composite parts. Available at: https://markforged.com/materials/continuous-fibers/continuous-carbon-fiber (accessed: June 28, 2021).
  16. Liu Z., Lei Q., Xing S. et al. Mechanical characteristics of wood, ceramic, metal and carbon fiber-based PLA composites fabricated by FDM. Journal of Materials Research and Technology, 2019, vol. 8, no. 5, pp. 3741–3751. DOI: 10.1016/j.jmrt.2019.06.034.
  17. Heidari-Rarani M., Rafiee-Afarani M., Zahedi A.M. Mechanical characterization of FDM 3D printing of continuous carbon fiber reinforced PLA composites. Composites, Part B, 2019, vol. 175, pp. 1–8.
  18. Moumen A., Tarfaoui M., Lafdi K. Additive manufacturing of polymer composites: Processing and modeling approaches. Composites, Part B, 2019, vol. 171, pp. 166–182.
  19. Popescu D., Zapciu A., Amza C. et al. FDM process parameters influence over the mechanical properties of polymer specimens: A review. Polymer Testing, 2018, vol. 69, pp. 157–166.
  20. Yang L., Lia Sh., Zhou X. et al. Effects of carbon nanotube on the thermal, mechanical, and electrical properties of PLA/CNT printed parts in the FDM process. Synthetic Metals, 2019, vol. 253, pp. 122–130.
  21. Dawoud M., Taha I., Ebeid S. J. Strain sensing behaviour of 3D printed carbon black filled ABS. Journal of Manufacturing Processes, 2018, vol. 35, pp. 337–342.
  22. Mahfuza H., Adnan A., Rangari V.K. et al. Enhancement of strength and stiffness of Nylon 6 filaments through carbon nanotubes reinforcement. Applied Physics Letters, 2006, vol. 88, no. 8, pp. 083119.
  23. Luo J., Krause B., Pötschke P. Melt-mixed thermoplastic composites containing carbon nanotubes for thermoelectric applications. AIMS Materials Science, 2016, vol. 3, no. 3, pp. 1107–1116.
  24. Vijayan R., Ghazinezami A., Taklimi S.R. et al. The geometrical advantages of helical carbon nanotubes for high-performance multifunctional polymeric nanocomposites. Composites, Part B. 2019, vol. 156, pp. 28–42.
  25. Mansurova I.A., Isupova O.Y., Burkov A.A. et al. Functionalization of 1d carbon nanostructures by components of curing system and their influence on the properties of the vulcanizates. Nanotechnologies in Russia, 2016, vol. 11, pp. 603–609.
  26. Sandler J.K.W., Kirk J.E., Kinloch I.A. et al. Ultra-low electrical percolation threshold in carbon-nanotube epoxy composites. Polymer, 2003. vol. 44, no. 19, pp. 5893–5899.
  27. Lobanov M.V., Voronov V.A., Larionov S.A. et al. A new method for producing anisotropic two-matrix materials with controlled spatial distribution of fillers using 3D printing. Proceedings of the IV All-Rus. conf. "The role of fundamental research in the implementation of "Strategic directions for the development of materials and technologies for their processing for the period up to 2030". Moscow: VIAM, 2018, pp. 213–233.
  28. Wang J., Zhou H., Zhuang J., Liu Q. Influence of spatial configurations on electromagnetic interference shielding of ordered mesoporous carbon/ordered mesoporous silica/silica composites. Scientific Reports, 2013, vol. 3, pp. 3252.
  29. Sorokin A.E., Pykhtin A.A., Larionov S.A. et al. Structure and properties of CNT modified filaments based on ABS plastic. Vse materialy. Entsiklopedicheskiy spravochnik, 2020, no. 4, pp. 1–16.
  30. Paul D., Bucknell K. Polymer mixtures. Trans. from Engl. Ed. V.N. Kuleznev. St. Petersburg: Nauchnye osnovy i tekhnologii, 2009, vol. II: Functional properties. 606 p.
  31. Solovyanchik L.V., Shashkeev K.A., Soldatov M.A. A method for controlling the electrical conductive properties of a polymer composition. Vestnik Moskovskogo aviatsionnogo instituta, 2017, vol. 24, no. 4, pp. 184–194.
  32. Solovyanchik L.V., Kondrashov S.V., Shashkeev K.A., Marachovskiy P.C., Soldstov M.A. A new approach to impart to polymer composites functional properties. Trudy VIAM, 2017, no. 4 (52), paper no. 05. Available at: http://www.viam-works.ru (accessed: May 10, 2021). DOI: 10.18577/2307-6046-2017-0-4-5-5.
  33. Ayewah D., Davis D., Krishnamoorti R. et al. A surfactant dispersed SWCNT-polystyrene composite characterized for electrical and mechanical properties. Composites. Part A, 2010, vol. 41, no. 7, pp. 842–849.
  34. Kuleznev V.N. Mixtures and alloys of polymers. St. Petersburg: Nauchnye osnovy i tekhnologii, 2013, 216 p.