Medvedev I.M., Nikitin Ya.Yu., Puzanov A.I., Laptev A.B. Hot corrosion testing methods for high-temperature alloys (review) // Proceedings of VIAM. 2018. No. 11 (71). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-11-93-100.

Hot corrosion testing methods for high-temperature alloys (review)

Medvedev I.M., Nikitin Ya.Yu., Puzanov A.I., Laptev A.B.
Abstract

Hot corrosion testing of superalloys can be conducted using burner rig, deposit recoat method or electrochemical testing. Periodical deposition of salts, followed by heating in furnace is the most common way to evaluate resistance of superalloy to hot corrosion. 75% Na2SO4+25% NaCl is the most common corrosive solution for this type of testing. Test temperatures range from 650 to 950°C. The main criteria for assessment of alloys resistance to hot corrosion is gravimetry, which is used to measure weight loss and corrosion depth. Many researchers have also investigated the influence of hot corrosion on mechanical properties of high temperature alloys.

Keywords
superalloys, destruction, service conditions, durability, corrosive environment.
Reference list
  1. Sidhu T.S., Agrawal R.D., Prakash S. Hot corrosion of some superalloys and role of high-velocity oxy-fuel spray coatings ‒ a rewiew // Surface and coating technology. 2005. Vol. 198. Is. 1–3. P. 441–446.
  2. Kosmin A.A., Budinovskiy S.A., Matveyev P.V., Smirnov A.A. Issledovaniye zharoprochnogo splava ZhS36 s razlichnymi tipami ionno-plazmennykh zashchitnykh pokrytiy na stoykost k sulfidno-oksidnoy korrozii v oblasti temperatur 850–900°C [Research of sulfide-oxide corrosion resistance of ZhS36 nickel superalloy with different types of ion-plasma coatings in temperature range 850–900°С] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №12. St. 05. Available at: http://www.viam-works.ru (accessed: August 24, 2018). DOI: 10.18577/2307-6046-2015-0-12-5-5.
  3. Bazyleva O.A., Arginbayeva E.G., Lutskaya S.A. Metody povysheniya korrozionnoy stoykosti zharoprochnykh nikelevykh splavov (obzor) [Ways of increasing corrosion resistance of superalloys (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №4. St. 01. URL: http://www.viam-works.ru (data obrashcheniya: 24.08.2018). DOI: 10.18577/2307-6046-2018-0-4-3-8.
  4. Kosmin A.A., Budinovskiy S.A., Muboyadzhyan S.A. Zharo- i korrozionnostoykoye pokrytiye dlya rabochikh lopatok turbiny iz perspektivnogo zharoprochnogo splava VZhL21 [Heat and corrosion resistant coating for working turbine blades from promising high-temperature alloy VZhL21] // Aviacionnyye materialy i tekhnologii. 2017. №1 (46). S. 17–24. DOI: 10.18577/2071-9140-2017-0-1-17-24.
  5. Kablov E.N., Muboyadzhyan S.A., Budinovskiy S.A., Pomelov Ya.A. Ionno-plazmennyye zashchitnyye pokrytiya dlya lopatok gazoturbinnykh dvigateley [Ion-plasma protective coatings for blades of gas turbine engines] // Konversiya v mashinostroyenii. 1999. №2. S. 42–47.
  6. Inozemtsev A.A., Nikhamkin M.A., Sandratskiy V.L. Osnovy konstruirovaniya aviatsionnykh dvigateley i energeticheskikh ustanovok [Basics of designing aircraft engines and power plants]. M.: Mashinostroyeniye, 2008. T. 2: Kompressory. Kamery sgoraniya. Forsazhnyye kamery. Turbiny. Vykhodnyye ustroystva. 367 s.
  7. Bratukhin A.G., Reshetnikov Yu.E., Inozemtsev A.A. i dr. Osnovy tekhnologii sozdaniya gazoturbinnykh dvigateley dlya magistral'nykh samoletov [Fundamentals of technology for creating gas turbine engines for long-haul aircraft]. M.: Aviatekhinform, 1999. 553 s.
  8. Kablov E.N., Ospennikova O.G., Lomberg B.S. Strategicheskiye napravleniya razvitiya konstruktsionnykh materialov i tekhnologiy ikh pererabotki dlya aviatsionnykh dvigateley nastoyashchego i budushchego [Strategic directions of development of structural materials and technologies for their processing for aviation engines of the present and the future] // Avtomaticheskaya svarka. 2013. №10. S. 23–32.
  9. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  10. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  11. Nicholls J.R., Saunders S.R.J. Comparison of hot-salt corrosion behaviour of superalloys in high and low velocity burner rigs // High Temperature Technology. 1989. Vol. 7. Is. 4. P. 193–201. DOI: 10.1080/02619180.1989.11753437.
  12. Mahobia G.S., Paulose N., Mannan S.L. et al. Effect of hot corrosion on low cycle fatigue behavior of superalloy IN718 // International Journal of Fatigue. 2014. Vol. 59. P. 272–281. DOI: 10.1016/j.ijfatigue.2013.08.009.
  13. Mannava V., Rao A.S., Paulose N. et al. Hot corrosion studies on Ni-base superalloy at 650°C under marine-like environment conditions using three salt mixture (Na2SO4+NaCl+NaVO3) // Corrosion Science. 2016. Vol. 105. P. 109–119. DOI: 10.1016/j.corsci.2016.01.008.
  14. Zhao S., Xie X., Smith G.D., Patel S.J. Research and Improvement on structure stability and corrosion resistance of nickel-base superalloy INCONEL alloy 740 // Materials and Design. 2006. Vol. 27. P. 1120–1127. DOI: 10.1016/j.matdes.2005.03.015.
  15. Lortrakul P., Trice R.W., Trumble K.P., Dayananda M.A. Investigation of the mechanisms of Type-II hot corrosion of superalloy CMSX-4 // Corrosion Science. 2014. Vol. 80. P. 408–415. DOI: 10.1016/j.corsci.2013.11.048.
  16. Sumner J., Encinas-Oropesa A., Simms N.J., Nicholls J.R. Type II hot corrosion: Kinetics studies of CMSX-4 // Oxidation of Metals. 2013. Vol. 80. Is. 5–6. P. 553–563. DOI: 10.1007/s11085-013-9395-x.
  17. Sumner J., Encinas-Oropesa A., Simms N.J., Nicholls J.R. Type II hot corrosion: Behavior of CMSX-4 and IN738LC as a function of corrosion environment // Materials and Corrosion. 2014. Vol. 65. P. 188–196. DOI: 10.1002/maco.201307425.
  18. Nicholls J.R., Simms N.J., Encinas-Oropesa A. Modelling hot corrosion in industrial gas turbines // Materials at High Temperatures. 2007. Vol. 24. Is. 3. P. 149–162. DOI: 10.3184/096034007X263587.
  19. Aung N.N., Liu X. Effect of temperature on coal ash hot corrosion resistance of Inconel 740 superalloy // Corrosion Science. 2014. Vol. 82. P. 227–238. DOI: 10.1016/j.corsci.2014.01.020.
  20. Sahu J.K., Ravi Kumar B., Das S.K. et al. Isothermal high temperature low cycle fatigue behavior of Nimonic-263: Influence of type I and type II hot corrosion // Materials Science and Engineering A. 2015. Vol. 622. P. 131–138. DOI: 10.1016/j.msea.2014.11.016.
  21. Sahu J.K., Gupta R.K., Swaminathan J. et al. Influence of hot corrosion on low cycle fatigue behavior of nickel base superalloy SU 263 // International Journal of Fatigue. 2013. Vol. 51. P. 68–73. DOI: 10.1016/j.ijfatigue.2013.02.006.
  22. El-Awadi G.A., Abdel-Samad S., Elshazly E.S. Hot corrosion behavior of Ni based Inconel 617 and Inconel 738 superalloys // Applied surface science. 2016. Vol. 378. P. 224–230. DOI: 10.1016/j.apsusc.2016.03.181.
  23. Sumner J., Potter A., Simms N.J., Oakey J.E. Hot corrosion resistance of gas turbine materials in combusted syngas environments // Materials at High Temperatures. 2015. Vol. 32. Is. 1–2. P. 177–187. DOI: 10.1179/0960340914Z.00000000098.
  24. Bagui S., Ray A.K., Sahu J.K. et al. Influence of saline environment on creep rupture life of Nimonic-263 for marine turbine application // Materials Science and Engineering A. 2013. Vol. 566. P. 54–60. DOI: 10.1016/j.msea.2012.12.081.
  25. Yang X., Li S., Qi H. Effect of high-temperature hot corrosion on the low cycle fatigue behavior of a directionally solidified nickel-base superalloy // International journal of fatigue. 2015. Vol. 70. P. 106–113. DOI: 10.1016/j.ijfatigue.2014.08.011.
  26. Homaeian A., Alizadeh M. Interaction of hot corrosion and creep in Alloy 617 // Engineering Failure Analysis. 2016. Vol. 66. P. 373–384. DOI: 10.1016/j.engfailanal.2016.03.012.
  27. Simms N.J., Encinas-Oropesa A., Nicholls J.R. Modelling the Development of Type I Hot Corrosion on Coated and Uncoated Single Crystal Superalloys // Materials Science Forum. 2008. Vol. 595–598. P. 689–698. DOI: 10.4028/www.scientific.net/MSF.595-598.689.
  28. Liu E., Zheng Z., Guan X. et al. Influence of Pre-oxidation on the Hot Corrosion of DZ68 Superalloy in the Mixture of Na2SO4–NaCl // Journal of Materials Science and Technology. 2010. Vol. 26. Is. 10. P. 895–899. DOI: 10.1016/S1005-0302(10)60143-0.
  29. Zhang K., Liu M.M., Liu S.L. et al. Hot corrosion behaviour of a cobalt-base super-alloy K40S with and without NiCrAlYSi coating // Corrosion Science. 2011. Vol. 53. Is. 5. P. 1990–1998. DOI: 10.1016/j.corsci.2011.02.022.
  30. Chang J.X., Wang D., Zhang G. et al. Interaction of Ta and Cr on Type-I hot corrosion resistance of single crystal Ni-base superalloys // Corrosion Science. 2017. Vol. 117. P. 35–42. DOI: 10.1016/j.corsci.2017.01.011.
  31. Dever J.A., Nathal M.V., DiCarlo J.A. Research on High-Temperature Aerospace Materials at NASA Glenn Research Center // Journal of Aerospace. 2013. Vol. 26. Is. 2. P. 500–514. DOI: 10.1061/(ASCE)AS.1943-5525.0000321.
  32. Supersplavy II: Zharoprochnyye materialy dlya aerokosmicheskikh i promyshlennykh energoustanovok v 2 kn. / pod red. Ch.T. Simsa, N.S. Stoloffa, U.K. Khagelya; per. s angl. [Superalloys II: Heat-resistant materials for aerospace and industrial power plants in 2 books / ed. by C.T. Sims, N.S. Stoloff, W.K. Hagel; tans. from Eng.]. M.: Metallurgiya, 1995. Kn. 1. 384 s.