Popov D.A., Ogorodov D.V., Trapeznikov A.V. Alternative sources of boron-containing raw materials for the Al–B ligatures production (review) // Proceedings of VIAM. 2015. No. 10. Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-10-7-7.

Alternative sources of boron-containing raw materials for the Al–B ligatures production (review)

Popov D.A., Ogorodov D.V., Trapeznikov A.V.
Abstract

This article describes and analyzes raw materials and production methods of aluminum-boron ligatures such as: direct alloying aluminum with pure boron or borides; aluminothermic reduction of boron compounds, oxygen-containing and oxygen-free; receiving ladle clean boride followed by dissolving them in aluminum (SHS, electroplated carbothermic reduction, etc.).

Reference list
  1. Belov N.A. Jekonomnolegirovannye zharoprochnye aljuminievye splavy: principy optimizacii fazovogo sostava [Ekonomnolegirovannye heat resisting aluminum alloys: principles of optimization of phase structure] //Aviacionnye materialy i tehnologii. 2011. №2. S. 6–11.
  2. Kablov E.N. Osnovnye itogi i napravlenija razvitija materialov dlja perspektivnoj aviacionnoj tehniki [The main results and the directions of development of materials for perspective aviation engineering] /V kn. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauch.-tehnich. sb. M.: VIAM. 2007. S. 20–26.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  4. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Aljuminievye deformi-ruemye splavy [Aluminum deformable alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  5. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Ju. Perspektivy primenenija magnievyh i litejnyh aljuminievyh splavov [Perspectives of application of magnesium and cast aluminum alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
  6. Kablov E.N. Kontrol' kachestva materialov – garantija bezopasnosti jekspluatacii aviacionnoj tehniki [Quality control of materials – security accreditation of operation of aviation engineering] /V sb. Aviacionnye materialy i tehnologii. M.: VIAM. 2001. №1. S. 3–8.
  7. Napalkov V.I., Mahov S.V. Legirovanie i modificirovanie aljuminija i magnija [Alloying and aluminum and magnesium modifying]. M.: MISiS. 2002. 376 s.
  8. Sposob prigotovlenija ligatury aljuminij–tugoplavkij metal [Way of preparation of ligature aluminum-refractory metal]: pat. 2232827 Ros. Fe-deracija; opubl. 03.02.2003.
  9. Mironov V.M., Byshkvarko G.S., Kitari G.G. Proizvodstvo ligatur dlja aljuminievyh i magnievyh splavov [Production of ligatures for aluminum and magnesium alloys]. Tula: Glavnaja redakcija cvetnoj metallurgii. 1963. 84 s.
  10. Ligatura [Ligature]: pat. 2026935 Ros. Federacija; opubl. 06.04.1995.
  11. Jacenko S.P., Skachkov V.M., Varchenja P.A. Poluchenie ligatur na osnove aljuminija metodom vysokotemperaturnyh obmennyh reakcij v rasplavah solej [Receiving ligatures on the basis of aluminum method of high-temperature exchange reactions in rasplavakh salts] //Rasplavy. 2010. №2. S. 89–94.
  12. Jacenko S.P., Ovsjannikov B.V., Ardashev M.A. Cementacionnoe poluchenie «master-splava» iz ftoridno-hloridnyh rasplavov [Tsementatsionnoye receiving «master-alloy» from fluoride hloridnykh rasplavov] //Rasplavy. 2006. №5. S. 29–36.
  13. Ljakishev N.P., Pliner Ju.L., Ignatenko G.F. Aljuminotermija [Aluminothermy]. M.: Metallurgija. 1978. 424 s.
  14. Belov N.A., Alabin A.N. Sravnitel'nyj analiz legirujushhih dobavok primenitel'no k izgotovleniju termostojkih provodov na osnove aljuminija [The comparative analysis of alloying additives with reference to manufacturing of heat-resistant wires on the basis of aluminum] //MiTOM. 2011. №9. S. 54–58.
  15. Sposob izgotovlenija ligatur na osnove aljuminija [Way of manufacturing of ligatures on the basis of aluminum]: pat. 2190682 Ros. Federacija; opubl. 17.05.2001.
  16. Osincev O. Diagrammy sostojanija dvojnyh i trojnyh sistem. Fazovye ravnovesija v splavah [Charts of condition of double and threefold systems. Phase balance in alloys]. M.: Mashinostroenie. 2009. 352 s.
  17. Napalkov V.I., Cherepok G.V., Mahov S.V. Nepreryvnoe lit'e aljuminievyh splavov [Continuous casting of aluminum alloys]. M.: Intermet Inzhinirng. 2005. 512 s.
  18. Truhov A.P., Maljarov A.I. Litejnye splavy i plavka [Cast alloys and melting]. M.: Akademija. 2004. 377 s.