Kovalenko A.V. Study of resin properties for forming of articles by resin transfer molding // Proceedings of VIAM. 2015. No. 1. Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-1-6-6.

Study of resin properties for forming of articles by resin transfer molding

Kovalenko A.V.
Abstract

One of relatively new methods of articles manufacture from polymer composite materials is a resin transfer molding technology (RTM -technology). Basic principle of the method is an injection of molding resin into a mold cavity,the preform contains a packet of «dry» reinforcing fiber. During injection resin is spreading throughout an entire volume of the mold cavity, displacing the air located there, and impregnates fibers. Resin transfer molding involves a usage of a rigid sealed form, consisting of a matrix and punch. Study of properties of the binder for articles forming by resin transfer molding method is considered in the present article.

Keywords
RTM
Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and processing technologies for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Jepoksidnoe svjazujushhee, prepreg na ego osnove i izdelija, vypolnennye iz nego [Epoxy binder prepreg on the basis thereof and articles made therefrom]: pat. 2424259 Ros. Federacija; opubl. 22.10.2009.
  3. Christian F. Lightweight automotive design with HP-RTM //Reinforced Plastics. 2011. P. 29–31.
  4. Kablov E.N., Kondrashov S.V., Jurkov G.Ju. Perspektivy ispol'zovanija uglerodsoderzhashhih nanochastic v svjazujushhih dlja polimernyh kompozicionnyh materialov [Prospects for the use of carbonaceous nanoparticles in binders for polymer composites] //Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 24–42.
  5. Dushin M.I., Hrul'kov A.V., Muhametov R.R., Chursova L.V. Osobennosti izgotovlenija izdelij iz PKM metodom propitki pod davleniem [Especially the manufacture of PCM by pressure impregnation] //Aviacionnye materialy i tehnolo-gii. 2012. №1. C. 18–26.
  6. Chensong Dong. A modified rule of mixture for the vacuum-assisted resin transfer moulding process simulation //Composites Science and Technology. 2008. V. 68. №9. P. 2125–2133.
  7. Simacek P., Suresh G., Stanley A. Modeling Flow in Compression Resin Transfer Molding for Manufacturing of Complex Lightweight High-Performance Automotive Parts //Journal of Composite Materials. 2008. №42. P. 2523–2545.
  8. Neljub V.A., Grashhenkov D.V., Kogan D.I., Sokolov I.A. Primenenie prjamyh metodov formovanija pri proizvodstve krupnogabaritnyh detalej iz stekloplastikov [The application of direct methods of molding in the production of large parts of fiberglass] //Himicheskaja tehnologija. 2012. T. 13. №12. S. 17–23.
  9. Horobryh M.A., Kashirskij D.A. Metody izgotovlenija detalej iz kompozicionnyh materialov propitkoj pod davleniem v osnastke [Methods for manufacturing parts made of composite materials by impregnation under pressure in a snap] //Molodoj uchenyj. 2013. №5. S. 116–122.
  10. Mouton S., Teissandier D., Sebastian P., Nadeau J.P. Manufacturing requirements in design: The RTM process in aeronautics //Composites Part A: Applied Science and Manufacturing. 2010. V. 41. №1. P. 125–130.
  11. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PKM [New polymeric binders for advanced manufacturing methods of structural fiber PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  12. Muhametov R.R., Merkulova Ju.I., Chursova L.V. Termoreaktivnye polimernye svjazujushhie s prognoziruemym urovnem reologicheskih i deformativnyh svojstv [Thermosetting polymeric binders with the projected level of rheology and deformation properties] //Klei. Germetiki. Tehnologii. 2012. №5. S. 19–24.
  13. ASTM Standard D790. Standard Test Method for flexural properties of unreinforced and reinforced plastics and electrical insulating materials. ASTM International. 2003.
  14. GOST 25.601–80. Metody mehanicheskih ispytanij kompozicionnyh materialov s polimernoj matricej (kompozitov). Metod ispytanija ploskih obrazcov na rastjazhenie pri normal'noj, povyshennoj i ponizhennoj temperaturah [Methods of mechanical testing of composite materials with a polymer matrix (composites). Method of testing flat tensile specimens at normal, low and high temperatures].
  15. ASTM Standard D3039. Standard Test Method for Tensile Properties of Polymer Matrix Composite Materials. ASTM International. 2002.
  16. Deleglise M. Modeling of high speed RTM injection with highly reactive resin with on-line mixing //Applied Science and Manufacturing. 2011. V. 42(10). P. 1390–1397.
  17. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S., Sevast'yanov V.G. Glass and ceramics based high-temperature composite materials for use in aviation technology //Glass and Ceramics. 2012. P. 1–4.
  18. Postnova M.V., Postnov V.I. Opyt razvitija bezavtoklavnyh metodov formovanija PKM [Experience in the development of methods of forming RMB bezavtoklavnogo] //Trudy VIAM. 2014. №4. St. 06 (viam-works.ru).
  19. Grigor'ev M.M., Kogan D.I., Tverdaja O.N., Panina N.N. Osobennosti izgotovlenija PKM metodom RFI [Peculiarities of PCM by RFI] //Trudy VIAM. 2013. №4. St. 03 (viam-works.ru).
  20. Tkachuk A.I., Grebeneva T.A., Chursova L.V., Panina N.N. Termoplastichnye svjazujushhie. Nastojashhee i budushhee [Thermoplastic binders. Present and Future] //Trudy VIAM. 2013. №11. St. 07 (viam-works.ru).
  21. Kirillov V.N., Starcev O.V., Efimov V.A. Klimaticheskaja stojkost' i povrezhdaemost' polimernyh kompozicionnyh materialov, problemy i puti reshenija [Weather resistance and defectiveness of polymer composite materials, problems and solutions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.