Sorokin A.E., Beider E.Ya., Perfilova D.N. Effect of climatic factors on properties of carbon fiber reinforced plastic based on polyphenylenesulfide resin // Proceedings of VIAM. 2015. No. 1. Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-1-10-10.

Effect of climatic factors on properties of carbon fiber reinforced plastic based on polyphenylenesulfide resin

Sorokin A.E., Beider E.Ya., Perfilova D.N.
Abstract

Properties of carbon fiber reinforced plastic based on thermoplastic matrix were studied. An influence of different environments and temperatures on properties of carbon plastic polyphenylenesulfide resin was studied.It has been shown that CFRP has a high moisture and water resistance at normal and elevated temperatures. Influence of different lay-ups of carbon plies on the behavior of CFRP during aging in moisture environment and water has been revealed. It was established that the studied material is characterized by a high level of maintenance of strength characteristics after an effect of water, moisture, thermo-moisture aging, thermal aging and treatment by thermal cycles from -60 to +160°C. It has been shown during research that CFRP has a high level of maintenance of the properties and it is competitive with foreign and domestic analogues. It may be used in wide temperature range from -60 to +160°C.

Reference list
  1. Sirotkin O.S., Andrjunina M.A., Bejder Je.Ja. Novye konstrukcionnye i funkcional'nye PKM na osnove termoplastov i tehnologii ih formovanija [New structural and functional PTP-based thermoplastics and their molding technology] //Aviacionnaja promyshlennost'. 2012. №4. S. 43–47.
  2. Bejder Je.Ja., Petrova G.N., Izotova T.F., Barbot'ko S.L. Stekloplastiki na termoplastichnoj matrice [GRP thermoplastic matrix] //Trudy VIAM. 2013. №7. St. 03 (viam-works.ru).
  3. Petrova G.N., Bejder Je.Ja., Izotova T.F., Malyshenok S.V. Kompozicionnye termoplastichnye materialy – sposoby poluchenija i pererabotki [Composite thermoplastic materials – methods of obtaining and processing] //Vse materialy. Jenciklopedicheskij spravochnik. 2013. №10. S. 10–17.
  4. Bejder Je.Ja., Malyshenok S.V., Petrova G.N. Kompozicionnye termoplastichnye materialy – svojstva i sposoby pererabotki [The composite thermoplastic materials – properties and processing methods] //Plasticheskie massy. 2013. №7. S. 56–60.
  5. Bejder Je.Ja., Petrova G.N., Izotova T.F., Gureeva E.V. Kompozicionnye termoplastichnye materialy i penopoliimidy [Composite and thermoplastic materials penopoliimidy] //Trudy VIAM. 2013. №11. St. 01 (viam-works.ru).
  6. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  7. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and processing technologies for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  8. Gunjaev G.M., Chursova L.V., Komarova O.A., Gunjaeva A.G. Konstrukcionnye ugleplastiki, modificirovannye nanochasticami [Structural carbon composites modified nanoparticles] //Aviacionnye materialy i tehnologii. 2012. №S. S. 277–286.
  9. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  10. Guljaev I.N., Vlasenko F.S., Zelenina I.V., Raskutin A.E. Napravlenija razvitija termostojkih ugleplastikov na osnove poliimidnyh i geterociklicheskih polimerov [Direction of the heat-resistant carbon-fiber-based polyimide and heterocyclic polymers] //Trudy VIAM. 2014. №1. St. 04 (viam-works.ru).
  11. Mihajlin Ju.A. Konstrukcionnye polimernye kompozicionnye materialy [Structural polymer composite materials]. SPb.: NOT. 2008. 820 s.
  12. Kerber M.L., Vinogradov V.M. Polimernye kompozicionnye materialy: struktura, svojstva, tehnologija [Polymer composite materials: structure, properties, technology]. SPb.: Professija. 2009. 560 s.
  13. Nozdrina L.V., Korotkova V.I., Bejder Je.Ja. Primenenie kompozicionnyh materialov s termoplastichnoj matricej [The use of composite materials with a thermoplastic matrix] //Konstrukcii iz kompozicionnyh materialov. 1991. №1. S. 18–24.
  14. Ustinov V.A., Bejder Je.Ja. Primenenie kompozicionnyh materialov s termoplastichnoj matricej [The use of composite materials with a thermoplastic matrix] //Konstrukcii iz kompozicionnyh materialov. 1991. №1. S. 25–32.
  15. Petrova G.N., Beider E.Ya. Construction materials based on reinforced thermoplastics //Russian Journal of General Chemistry. 2011. T. 81. №5. P. 1001–1007.
  16. Kirillov V.N., Starcev O.V., Efimov V.A. Klimaticheskaja stojkost' i povrezhdaemost' polimernyh kompozicionnyh materialov, problemy i puti reshenija [Weather resistance and defectiveness of polymer composite materials, problems and solutions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  17. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. II. Relaksacija ishodnoj strukturnoj neravnovesnosti i gradient svojstv po tolshhine [Climatic aging of composite materials aviation applications. II. Relaxation of the original structural and non-equilibrium properties of gradient across the thickness] //Deformacija i razrushenie materialov. 2012. №6. S. 17–19.
  18. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. I. Mehanizmy starenija [Climatic aging of composite materials aviation applications. I. Mechanisms of aging] //Deformacija i razrushenie materialov. 2010. №11. S. 19–27.
  19. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. III. Znachimye faktory starenija [Climatic aging of composite materials aviation applications. III. Significant factors of aging] //Deformacija i razrushenie materialov. 2011. №1. S. 34–40.
  20. Kablov E.N., Starcev O.V., Deev I.S., Nikishin E.F. Svojstva polimernyh kompozici-onnyh materialov posle vozdejstvija otkrytogo kosmosa na okolozemnyh orbitah [Properties of polymer composite materials after exposure to the open space in Earth orbits] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №10. S. 2–9.
  21. Сhen-chi M.M., Chang-lun L., Min-jong C., Wyan-hwa T. Effect of physical aging on the thoughness of carbon fiber-reinforsed poly(ether ether ketone) and poly(phenylene sulfide) composite //Polymer composite. 1992. V. 13. №6. P. 441–447.
  22. Сhen-chi M.M., Chang-lun L., Min-jong C., Wyan-hwa T. Hydrothermal behaivor of carbon fiber-reinforsed poly(ether ether ketone) and poly(phenylene sulfide) composite //Polymer composite. 1992. V. 13. №6. P. 448–453.
  23. Batista N.L., Faria M.C.M., Jha K., Olivera P.C., Bothelho E.C. Influence of water immersion and ultraviolet weathering on mechanical properties of polyphenylene sulfide-carbon fiber composites //Journal of thermoplastic composite materials. 2013. №1. P. 1–17.
  24. Choqueuse D., Davies P., Mareas F., Baireur R. Aging of Composites in water: comparison of five materials in term of absorption kinetics and revolution of mechanical properties //Polymeric composites. 1997. V. 2. P. 73–96.
  25. Ishak Z.A., Berry J.P. Hygrothermal aging studies of short carbon fiber reinforced nylon 6.6 //Journal of applied polymer science. 1994. V. 51. №13. Р. 2144–2155.
  26. Amore A.D., Cocchini K., Pompo A., Apicella A., Nicolais L. The effect of physical aging on long-term properties of poly ether-ketone (PEEK) and PEEK based composites //Journal of applied polymer science. 1990. V. 39. P. 1163–1174.
  27. Dao D., Hodgkin J., Krstina J., Mardel J., Tian W. Accelerated aging versus realistic aging aerospace composites. II Chemistry of thermal aging //Journal of applied polymer science. 2006. V. 102. P. 3221–3232.