Abstract

Properties of fiberglass laminates on a base of polyimide binder and various fillers were studied. It was shown, that a combined material with carbon fabric in external layers has high mechanical strength, heat resistance, anti-friction properties and high durability

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Tkachuk A.I., Grebneva T.A., Chursova L.V., Panina N.N. Termoplastichnye svjazujushhie. Nastojashhee i budushhee [Thermoplastic binders. Present and Future] //Trudy VIAM. 2013. №11. St. 07 (viam-works.ru).
  3. Kablov E.N., Starcev O.V., Deev I.S., Nikishin E.F. Svojstva polimernyh kompozicionnyh materialov posle vozdejstvija otkrytogo kosmosa na okolozemnyh orbitah [Properties of polymer composites after exposure to outer space orbiting the Earth] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №11. S. 2–16.
  4. Kablov E.N. Himija v aviacionnom materialovedenii [Chemicals in aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  5. Kablov E.N. Materialy dlja izdelija «Buran» – innovacionnye reshenija formirovanija shestogo tehnologicheskogo uklada [Materials for the product "Buran" - innovative solutions forming the sixth technological order] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  6. Davydova I.F., Kavun N.S. Stekloplastiki – mnogofunkcional'nye kompozicionnye materialy [GRP - multifunctional composite materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 253–260.
  7. Davydova I.F., Kablov E.N., Kavun N.S. Termostojkie negorjuchie poliimidnye steklotekstolity dlja izdelij aviacionnoj i raketnoj tehniki [Heat-resistant polyimide incombustible Fiberglass products for the aviation and rocketry] //Vse materialy. Jenciklopedicheskij spravochnik. 2009. №7. S. 2–11.
  8. Davydova I.F. Kavun N.S. Termostojkie germetichnye steklotekstolity [Heat-resistant sealed Fiberglass] //Vse materialy. Jenciklopedicheskij spravochnik. 2011. №11. S. 18–20.
  9. Davidova I.F., Kavun N.S. Glass plastics to auiation and roket Engineering. Springer. 2012 (clause in the electronic).
  10. Davydova I.F., Kavun N.S., Shvecov E.P. Bazal'toplastiki dlja raboty pri povyshennyh tem-peraturah [Basalt for use at elevated temperatures] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №11. S. 18–24.
  11. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PKM [New polymeric binders for the promising methods for the manufacture of structural fibrous RMB] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  12. Davydova I.F., Kavun N.S. Stekloplastiki v konstrukcijah aviacionnoj i raketnoj tehniki [GRP in the construction of aviation and rocketry] //Steklo i keramika. 2012. №4. S. 36–42.
  13. Davydova I.F., Kavun N.S. Ognestojkie stekloplastiki v konstrukcijah motogondol dvigatelej samoletov [Fire-resistant fiberglass in the construction of aircraft engine nacelles] //Vse materialy. Jenciklopedicheskij spravochnik. 2011. №7. S. 16–20.
  14. Davydova I.F., Kavun N.S., Shvecov E.P. Vysokotermostojkie karbonosoderzhashhie steklotekstolity [High temperature resistant Fiberglass carbon-containing] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №9. S. 18–24.
  15. Kondratenko A.N., Golubkova T.A. Polimernye kompozicionnye materialy v izdelijah zarubezhnoj raketno-kosmicheskoj tehniki (obzor) [Polymer composite materials in the products of foreign missile and space technology (review)] //Konstrukcii iz kompozicionnyh materialov. 2009. №2. S. 24–34.
  16. Mihajlin Ju.A. Konstrukcionnye polimernye kompozicionnye materialy [Structural polymer composite materials]. M.: «NOT». 2008. 820 s.
  17. Zorin V.A. Opyt primenenija kompozicionnyh materialov v izdelijah aviacionnoj i raketno-kosmicheskoj tehniki [Experience in the application of composite materials in the products aviation and space technology] //Konstrukcii iz kompozicionnyh materialov. 2011. №4. S. 44–58.
  18. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Promising high-temperature ceramic composites] //Rossijskij himicheskij zhur-nal. 2010. T. LIV. №1. S. 20–24.
  19. Guljaev I.N., Vlasenko F.S., Zelenina I.V., Raskutin A.E. Napravlenija razvitija termostojkih ugleplastikov na osnove poliimidnyh i geterociklicheskih polimerov [Directions of development of heat-resistant carbon-fiber-based polyimide polymers and heterocyclic] //Trudy VIAM. 2014. №1. St. 04 (viam-works.ru).