Karachevtsev F.N., Dvoretskov R.M., Zagvozdkina T.N. Microwave probe preparation of nickel alloys for determination of alloying elements using ICP-AES method // Proceedings of VIAM. 2014. No. 11. Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2014-0-11-11-11.

Microwave probe preparation of nickel alloys for determination of alloying elements using ICP-AES method

Karachevtsev F.N., Dvoretskov R.M., Zagvozdkina T.N.
Abstract

A large amount of alloying elements such as Al, Ti, Cr, Co, Zr, Nb, Mo, Ru, Ta, W, Re may be in a composition of heat-resistant nickel alloys simultaneously. However, till the last time there were no techniques for simultaneous determination of them (without an application of similar by composition standard samples).To determine the alloying elements in nickel alloys a method of atomic emission spectroscopy with inductively coupled plasma has been proposed (ICP-AES). The technique of microwave sample preparation of nickel alloys was worked out for samples of different composition includ-ing ruthenium containing ones. Compositions of dissolution mixtures and parameters of microwave digestion were chosen. Measurement techniques of mass fraction of Al, Ti, Cr, Co, Nb, Mo, Ru, Ta, W, Re in nickel alloys by atomic emission spectrometry with inductively coupled plasma were de-veloped and verified. Limits of relative measurement error for elements mass content from 0,1 to 20% don't exceed 4

Reference list
  1. Kablov E.N., Bondarenko Ju.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [The development process of directional solidification of gas turbine engine blades with a single-crystal superalloys and composite structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  2. Shmotin Ju.N., Starkov R.Ju., Danilov D.V. i dr. Novye materialy dlja perspektivnogo dvigatelja OAO «NPO „Saturn”» [New materials for advanced engine JSC «NPO „Saturn”»] //Aviacionnye materialy i tehnologii. 2012. №2. S. 6–8.
  3. Kablov E.N., Sidorov V.V., Kablov D.E. i dr. Sovremennye tehnologii poluchenija prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokolenija [Modern technologies for bar stock of casting superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
  4. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Casting nickel superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–52.
  5. Lomberg B.S., Bakradze M.M., Chabina E.B., Filonova E.V. Vzaimosvjaz' struktury i svojstv vysokozharoprochnyh nikelevyh splavov dlja diskov gazoturbinnyh dvigatelej [Relationship between structure and properties of nickel-base superalloys for gas turbine engine disks] //Aviacionnye materialy i tehnologii. 2011. №2. S. 25–30.
  6. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Litejnye zharoprochnye nikelevye splavy dlja perspektivnyh aviacionnyh GTD [Casting nickel superalloys for advanced gas turbine engines] //Tehnologija legkih splavov. 2007. №2. S. 6–16.
  7. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharoprochnye nikelevye splavy dlja detalej gazoturbinnyh dvigatelej [High-temperature heat-resistant nickel alloys for turbine engines parts] //Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
  8. Kablov E.N., Petrushin N.V., Bronfin M.B., Alekseev A.A. Osobennosti monokristallicheskih zharoprochnyh nikelevyh splavov, legirovannyh reniem [Features single-crystal high-temperature nickel alloys, alloyed with rhenium] //Metally. 2006.
  9. №5. S. 47–57.
  10. Pupyshev A.A., Danilova D.A. Ispol'zovanie atomno-jemissionnoj spektrometrii s induktivno-svjazannoj plazmoj dlja analiza materialov i produktov chernoj metallurgii [Using atomic emission spectrometry with inductively coupled plasma analysis of materials and products of ferrous metallurgy] //Analitika i kontrol'. 2007.
  11. T. 11. №2–3. S. 131–181.
  12. Pelevina N.G. Primenenie plazmennoj atomno-jemissionnoj spektrometrii dlja kontrolja kachestva svinca marochnogo [The application of plasma atomic emission spectrometry for quality control lead vintage] //Zavodskaja laboratorija. Diagnostika materialov. 2007. T. 73. №12. S. 12–16.
  13. Dvoreckov R.M., Karachevcev F.N., Zagvozdkina T.N., Mehanik E.A. Opredelenie himicheskogo sostava vysokolegirovannyh nikelevyh splavov aviacionnogo naznachenija metodom AJeS-ISP v sochetanii s mikrovolnovoj probopodgotovkoj [Determination of chem-ical composition of high-nickel alloys for aircraft industry by AES-ICP in combination with microwave sample preparation] //Zavodskaja laboratorija. Diagnostika materialov. 2013. T. 79. №9. S. 6–9.
  14. Tormysheva E.A., Smirnova E.V., Ermolaeva T.N. Mikrovolnovaja probopodgotovka naplavochnyh materialov dlja analiza metodom atomno-jemissionnoj spektroskopii s induktivno-svjazannoj plazmoj [Microwave sample preparation surfacing materials for analysis by atomic emission spectroscopy with inductively coupled plasma] //Zavodskaja laboratorija. Diagnostika materialov. 2010. T. 76. №10. S. 10–13.
  15. GOST 6012–98. Nikel'. Metody himiko-atomno-jemissionnogo spektral'nogo analiza [Nickel. Methods of chemical and atomic emission spectral analysis].
  16. AM 0557665-72-323–2008. MKHA naplavochnyh materialov i splavov na nikelevoj osnove. Opredelenie massovyh dolej hroma i zheleza atomno-jemissionnym metodom s induktivno-svjazannoj plazmoj pri vhodnom kontrole [MKHA surfacing materials and nickel-based alloys. Determination of mass fraction of chromium and iron atomic emission method with inductively coupled plasma with an input control].
  17. ASTM E2594–09. Standard Test Method for Analysis of Nickel Alloys by Inductively Coupled Plasma Atomic Emission Spectrometry (Performance-Based Method).
  18. Kablov E.N. Fiziko-himicheskie i tehnologicheskie osobennosti sozdanija zharoprochnyh splavov, soderzhashhih renij [Physico-chemical and technological features of a high-temperature alloys containing rhenium] //Vestnik MGU. Ser. 2. Himija. 2005.
  19. T. 46. №3. S. 154–155.
  20. Todoli J.L., Gras L., Hernandis V., Mora J. Elemental matrix effects in ICP-AES //Journal of Analytical Atomic Spectrometry. 2002. №17. P. 142–169.
  21. GOST R ISO 14284–2009. Stal' i chugun. Otbor i podgotovka obrazcov dlja opredelenija himicheskogo sostava [Steel and iron. Selection and preparation of samples for determination of chemical composition.].
  22. Lidin R.A., Molochko V.A., Andreeva L.L. Himicheskie svojstva neorganicheskih veshhestv [Chemical properties of inorganic substances]. M.: Himija. 2000. 480 s.
  23. Avtokratova T.D. Analiticheskaja himija rutenija [Analytical chemistry of ruthenium]. M.: Izd-vo AN SSSR. 1962. 135 s.
  24. Ginzburg S.I., Ezerskaja N.A., Prokof'eva I.V. i dr. Analiticheskaja himija platinovyh metallov [Analytical chemistry of platinum metals]. Monografija.
  25. M.: Nauka. 1972. 616 s.