Lukin V.I., Ovsepyan S.V., Koval’chuk V.G., Samorukov M.L. The peculiarities of rotational friction welding of superalloy VG175 // Proceedings of VIAM. 2017. No. 12 (60). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2017-0-12-1-1.

The peculiarities of rotational friction welding of superalloy VG175

Lukin V.I., Ovsepyan S.V., Koval’chuk V.G., Samorukov M.L.
Abstract

The research of technological schemes (the sequence of welding and heat treatment operations) influence on the mechanical properties and the structure is carried out. The influence of technological heatings with a 300 hours duration and 650°C temperature on the weld’s structure and mechanical properties is studied. Friction welding parameters and optimal sequence of welding and heat treatment that allow getting the most high mechanical properties are determined.

Keywords
friction welding, welding regime parameters, static bend, short-term durability, long-term durability, impact strength, structure.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlya vysokoteplonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for the high-heatloaded details of gas turbine engines] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP4. S. 13–19.
  3. Kablov E.N., Ospennikova O.G., Lomberg B.S. Strategicheskie napravleniya razvitiya konstrukcionnyh materialov i tehnologij ih pererabotki dlya aviacionnyh dvigatelej nastoyashhego i budushhego [The strategic directions of development of constructional materials and technologies of their processing for aircraft engines of the present and the future] // Avtomaticheskaya svarka. 2013. №10. S. 23–32.
  4. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Letnikov M.N., Mazalov I.S. Primenenie novyh deformiruemyh nikelevyh splavov dlja perspektivnyh gazoturbinnyh dvigatelej [The application of new wrought nickel alloys for advanced gas turbine engines] // Aviacionnye materialy i tehnologii. 2017. №S. S. 116–129. DOI: 10.18577/2071-9140-2017-0-S-116-129.
  5. Razuvaev E.I., Moiseev N.V., Kapitanenko D.V., Bubnov M.V. Sovremennye tehnologii obrabotki metallov davleniem [Modern technologies of plastic working of metals] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 03. Available at: http://www.viam-works.ru (accessed: September 15, 2017). DOI: 10.18577/2307-6046-2015-0-2-3-3.
  6. Belyaev M.S., Terentjev V.F., Gorbovets M.A., Bakradze M.M., Antonova O.S. [Low cycle fatigue of Ni-based superalloy VZh175 at preset strain] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 01. Available at: http://www.viam-works.ru (accessed: September 15, 2017). DOI: 10.18577/2307-6046-2015-0-9-1-1
  7. Kablov E.N., Lukin V.I., Ospennikova O.G. Svarka i pajka v aviakosmicheskoj promyshlennosti [Welding and the soldering in the aerospace industry] // Tr. vseros. nauch.-praktich. konf. «Svarka i bezopasnost». Yakutsk: IFTPS SO RAN, 2012. S. 21–30.
  8. Eliseev Yu.S., Maslenkov S.B., Gejkin V.A., Poklad V.A. Tehnologiya sozdaniya nerazemnyh soedinenij pri proizvodstve gazoturbinnyh dvigatelej [Technology of creation of permanent connections by production of gas turbine engines]. M.: Nauka i tehnologii, 2001. 544 s.
  9. Sorokin L.I. Obrazovanie goryachih treshhin pri svarke zharoprochnyh nikelevyh splavov [Formation of hot cracks when welding heat resisting nickel alloys] // Svarochnoe proizvodstvo. 2005. №7. S. 29–33.
  10. Sorokin L.I. Svarivaemost zharoprochnyh nikelevyh splavov (obzor). Ch. 2 [Bondability of heat resisting nickel alloys (overview). P. 2] // Svarochnoe proizvodstvo. 2004. №9. S. 3–7.
  11. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlya aviacionnogo dvigatelestroeniya [Creation of modern heat resisting materials and technologies of their production for aviation engine building] // Krylya Rodiny. 2012. №3–4. S. 34–38.
  12. Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharo-prochnye nikelevye splavy dlya detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] // Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
  13. Vill V.I. Svarka metallov v tverdoj faze [Welding of metals in solid phase]. M.: Mashinostroenie, 1970. 176 s.
  14. Svarka treniem: spravochnik [Friction bonding: directory]. L.: Mashinostroenie, 1987. 235 s.
  15. Lukin V.I., Kovalchuk V.G., Samorukov M.L. i dr. Osobennosti tehnologii svarki treniem soedinenij iz splavov VKNA-25 i EP975 [Features of welding technology friction of connections from alloys VKNA-25 and ЭП975] // Svarochnoe proizvodstvo. 2010. №5. S. 28–33.
  16. Lomberg B.S., Bakradze M.M., Chabina E.B., Filonova E.V. Vzaimosvyaz struktury i svojstv vysokozharoprochnyh nikelevyh splavov dlya diskov gazoturbinnyh dvigatelej [Interrelation of structure and properties of high-heat resisting nickel alloys for disks of gas turbine engines ] // Aviacionnye materialy i tehnologii. 2011. №2. S. 25–30.
  17. Zhegina I.P., Kotelnikova L.V., Grigorenko V.B., Zimina Z.N. Osobennosti razrusheniya deformiruemyh nikelevyh splavov i stalej [Features of destruction of deformable nickel alloys and steel] // Aviacionnye materialy i tehnologii. 2012. №S. S. 455–465.
  18. Stepanov A.V. Metody rentgenovskogo nerazrushayushhego kontrolya v proizvodstve aviacionnyh dvigatelej [Methods of x-ray non-destructive testing in production of aircraft engines] // Aviacionnye materialy i tehnologii. 2010. №3. S. 28–32.