Nerush S.V., Ermolaev A.S., Rogalev A.M., Vasilenko S.A. Research of retailoring process of the rotor blade feather end of the first stage of high-pressure turbine (HPT) from ZS32-VI alloy by laser metal deposition with ZS32-VI metal alloy powder dispersed by atomization // Proceedings of VIAM. 2016. No. 8 (44). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-8-4-4.

Research of retailoring process of the rotor blade feather end of the first stage of high-pressure turbine (HPT) from ZS32-VI alloy by laser metal deposition with ZS32-VI metal alloy powder dispersed by atomization

Nerush S.V., Ermolaev A.S., Rogalev A.M., Vasilenko S.A.
Abstract

The ZS32-VI metal alloy powder for laser metal deposition dispersed by gas atomi-zation at HERMIGA 10/100 VI is researched. It is shown that the granules have a regular spherical shape with a small number of defective granules. The deposition quality of the rotor blade feather end of the high-pressure turbine first stage is performed. Laser metal deposition, performed with ZS32-VI metal alloy powder with granulometric composition 40–80 µm after degassing annealing and heating, provides with high quality deposited material (defects such as microcrack or lack of penetration are not revealed), and geometry retailoring in full. The work is executed within implementation of the complex scientific direction 10.4. «Technologies of bi-and polymetallic naturally reinforced metal materials by method of direct laser synthesis from metal powders» («The strategic directions of development of materials and technologies of their processing for the period till 2030») [1].

Keywords
gas atomization, metal powder, laser metal deposition, granulometric composition, surface morphology, rotor blade.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Prioritetnye napravleniya razvitiya tehnologij proizvodstva zharoprochnyh materialov dlya aviacionnogo dvigatelestroeniya [The priority directions of development of production technologies of heat resisting materials for aviation engine building] // Problemy chernoj metallurgii i materialovedeniya. 2013. №3. S. 47–54.
  3. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  4. Shmotin Yu.N., Starkov R.Yu., Danilov D.V., Ospennikova O.G., Lomberg B.S. Novye materialy dlya perspektivnogo dvigatelya OAO «NPO „Saturn”» [New materials for the perspective engine of JSC «NPO „Saturn”»] // Aviacionnye materialy i tehnologii. 2012. №2. S. 6–8.
  5. Razuvaev E.V. Proizvodstvo polufabrikatov iz sovremennyh i perspektivnyh zharoprochnyh splavov [Production of semi-finished products from modern and perspective hot strength alloys] // Aviacionnye materialy i tehnologii. M.: VIAM, 2002. Vyp.: Tehnologii proizvodstva aviacionnyh materialov. S. 35–39.
  6. Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharo-prochnye nikelevye splavy dlya detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] //Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
  7. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 01. Available at: http://www.viam-works.ru (accessed: July 10, 2015).
  8. Nerush S.V., Evgenov A.G., Ermolaev A.S., Rogalev A.M. Issledovanie melkodispersnogo metallicheskogo poroshka zharoprochnogo splava na nikelevoj osnove dlya lazernoj LMD-naplavki [Research of finely divided metal powder of hot strength alloy on nickel basis for laser LMD welding] // Voprosy materialovedeniya. 2013. №4 (76). S. 98–107.
  9. Nerush S.V., Evgenov A.G. Issledovanie melkodispersnogo metallicheskogo poroshka zharoprochnogo splava marki EP648-VI primenitelno k lazernoj LMD-naplavke, a takzhe ocenka kachestva naplavki poroshkovogo materiala na nikelevoj osnove na rabochie lopatki TVD [Research of fine-dispersed metal powder of the heat resisting alloy of the EP648-VI brand for laser metal deposition (LMD) and also the assessment quality of welding of powder material on the nickel basis on working blades THP] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №3. St. 01. Available at: http://www.viam-works.ru (accessed: July 10, 2015). DOI: 10.18577/2014-0-3-1-1.
  10. Evgenov A.G., Rogalev A.M., Nerush S.V., Mazalov I.S. Issledovanie svojstv splava EP648, poluchennogo metodom selektivnogo lazernogo splavleniya metallicheskih poroshkov [A study of properties of EP648 alloy manufactured by the selective laser sintering of metal powders] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 02. Available at: http://www.viam-works.ru (accessed: July 10, 2015). DOI: 10.18577/2307-6046-2015-0-2-2-2.
  11. Evgenov A.G., Nerush S.V., Vasilenko S.A. Poluchenie i oprobovanie melkodispersnogo metallicheskogo poroshka vysokohromistogo splava na nikelevoj osnove primenitelno k lazernoj LMD-naplavke [The obtaining and testing of the fine-dispersed metal powder of the high-chromium alloy on nickel-base for laser metal deposition] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №5. St. 04. Available at: http://www.viam-works.ru (accessed: July 10, 2015). DOI: 10.18577/2307-6046-2014-0-5-4-4.
  12. Ospennikova O.G., Evgenov A.G., Nerush S.V., Afanasev-Hodykin A.N. Issledovanie melkodispersnyh poroshkov pripoev na nikelevoj osnove primenitelno k polucheniyu vysokotehnologichnogo polufabrikata v vide samokleyushhijsya lenty na organicheskom svyazuyushhem [Research of finely divided powders of solders on nickel basis with reference to receiving hi-tech semi-finished product in look self-glued tapes on the organic binding ] // Vestnik UGATU. 2012. №5 (50). S. 137–144.
  13. Kablov E.N., Evgenov A.G., Rylnikov V.S., Afanas'ev-Hodykin A.N. Issledovanie melkodispersnyh poroshkov pripoev dlya diffuzionnoj vakuumnoj pajki, poluchennyh metodom avtomizacii rasplava [Research of finely divided powders of solders for the diffusion vacuum soldering, received by avtomizatsiya method rasplava] // Vestnik MGTU im. N.E. Baumana. 2011, Spec. vyp.: Perspektivnye konstrukcionnye materialy i tehnologii. S. 79–87.
  14. Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Goryunov A.V. Sovremennye tehnologii polucheniya prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokoleniya [Modern technologies of receiving the bar stock preparations from foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
  15. Goryunov A.V., Rigin V.E. Sovremennaya tehnologiya polucheniya litejnyh zharoprochnyh nikelevyh splavov [The modern technology of cast nickel base superalloys production] // Aviacionnye materialy i tehnologii. 2014. №2. S. 3–7.