Platonov A.A., Dushin M.I. Carbon composites VKU-25 based on unidirectional prepregs // Proceedings of VIAM. 2015. No. 11. Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-11-6-6.

Carbon composites VKU-25 based on unidirectional prepregs

Platonov A.A., Dushin M.I.
Abstract

The results of works on development of high-strength polymer composite material of new generation on the basis of a carbon UD fiber and hotmelt resin fulfilled at VIAM are represented in article. Comparative elastic and strength characteristics of the cured composite are submitted. The received results show that the developed carbon composite VKU-25 is not inferior import analogs on is elastic and strength properties .

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of FSUE «VIAM» SSC of RF on realization of «Strategic directions of development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Hrulkov A.V., Dushin M.I., Popov Ju.O., Kogan D.I. Issledovaniya i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovaniya PKM [Researches and development autoclave and out-of-autoclave technologies of formation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  3. Grashhenkov D.V., Chursova L.V. StrategiYa razvitiYa kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  4. Grishina O.I., Kochetov V.N., Shavnev A.A., Serpova V.M. Aspecty primeneniya vysokoprochnyh i vysokomodulnyh voloknistyh metallicheskih kompozitsionnyh materialov aviatsionnogo naznacheniya (obzor) [Aspects of application of high-strength and high-modulus fiber metal composite materials for aeronautical purpose (review)] //Trudy VIAM. 2014. №10. St. 05 (viam-works.ru).
  5. Timoshkov P.N., Hrulkov A.V. Sovremennye tehnologii pererabotki polimernyh kompozitsionnyh materialov, poluchaemyh metodom propitki rasplavnym svyazuyushchim [Modern technologies of hotmelt polymer composite materials processing] //Trudy VIAM. 2014. №8. St.04 (viam-works.ru).
  6. Dement’eva L.A., Serezhenkov A.A., Lukina N.F., Kutsevich K.E. Svoistva i naznachenie kompozitsionnyh maerialov na osnove kleevyh prepregov [Properties and appointment of composite materials based on adhesive prepregs]// Trudy VIAM. 2014. №8. St. 06 (viam-works.ru).
  7. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svyazujushhie dlya perspektivnyh metodov izgotovleniya PKM novogo pokoleniya [Melt binding for perspective methods of production of PCM of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  8. Dushin M. I., Hrulkov A.V., Raskutin A.E. K voprosu udaleniya izlishkov svyazuyushchego pri avtpklavnim formovanii izdeliy iz polimernyh kompozitsionnyh materialov [To question of removal of excesses binding at avtoklavny formation of products from polymeric composite materials]// Trudy VIAM. 2013. №1. St. 03 (viam-works.ru).
  9. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for the aircraft equipment] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  10. Sposob poluchenija izdeliya iz kompozicionnogo materiala [A way of receiving a product from composite material]: pat. 2448808 Ros. Federaciya; opubl. 05.10.2010.
  11. Postnov V.I., Petuhov V.I., Kazakov I.A., Abramov P.A., Postnov A.V., Senatorova O.G., Zhelezina G.F. Izgotovlenie iz MPKM konstruktivnyh elementov planera samoleta i osobennosti ih formoobrazovaniya [Production from MPKM of constructive elements of a glider of the plane and feature of their shaping] //Aviacionnye materialy i tehnologii. 2009. №3. S. 10–19.
  12. Dushin M.I., Hrulkov A.V., Muhametov R.R. Vybor tehnologicheskih parametrov avtoklavnogo formovaniya detalej iz polimernyh kompozicionnyh materialov [A choice of technological parameters of autoclave formation of details from polymeric composite materials] //Aviacionnye materialy i tehnologii. 2011. №3. S. 20–26.
  13. Raskutin A.E. Konstrukcionnye ugleplastiki na osnove novyh svyazuyushhih rasplavnogo tipa i tkanej PORCHER [Constructional coal plastics on the basis of new binding melt type and PORCHER fabrics] //Novosti materialovedeniya. Nauka i tehnika. 2013. №5. St. 01 (materialsnews.ru).
  14. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – a basis of innovative modernization of Russia ] //Metally Evrazii. 2012. №3. S. 10–15.
  15. Kablov E.N. Materialy i tehnologii VIAM v konstruktsiyah perspectivnih dvigatelei razrabotki OAO «Aviadvigatel» [Materials and VIAM technologies in designs of perspective engines of development of JSC «Aviadvigatel»] //IB «Permskie aviatsionnye dvigateli». 2014. №31. S. 43–47.