Effect of loading frequency and cycle shape on the parameters of the fatigue crack growth kinetic diagram of VT8-1 titanium alloy
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
The influence of loading frequency, dwell time at the maximum load, and block loading on fatigue crack growth kinetics in VT8-1 titanium alloy room temperature is examined. Diagrams were obtained, showing the dependence of crack growth rate da/dN on the stress intensity factor (ΔK) for a sinusoidal cycle (5–50 Hz), a trapezoidal cycle with dwell time (30–300 s), and block loading (quantity of cycles in a block 240–480). It was shown that in the stable crack growth region, an increase in the time component of the cycle and in the block duration leads to a decrease in the crack growth rate. The level of statistical scatter was determined from repeated tests.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Nochovnaya N.A., Gribkov Yu.A., Shiryaev A.A. Development of high-strength titanium pseudo-β-alloy and technologies for obtaining semi-finished products from it. Voprosy Materialovedeniya, 2016, no. 3 (87), pp. 23–31.
- Kablov E.N., Kashapov O.S., Medvedev P.N., Pavlova T.V. Study of a α + β-titanium alloy based on a system of Ti-Al-Sn-Zr-Si-β-stabilizing alloying elements. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 30–37. DOI: 10.18577/2071-9140-2020-0-1-30-37.
- Nochovnaya N.A., Shiryaev A.A. Features of the structural and phase composition, mechanical properties of metastable β-titanium alloy VT47 alloyed with silicon. Aviation materials and technologies, 2023, no. 1 (70), pp. 51–60. Available at: http://www.journal.viam.ru (accessed: March 15, 2026). DOI: 10.18577/2713-0193-2023-0-1-51-60.
- Erasov V.S., Oreshko E.I. Tests for fatigue of metal materials (review). Part 2. Analysis of the Basquin-Manson-Coffin equation. Methods of testing and processing of results. Aviation materials and technology, 2021, no. 1 (62), pp. 80–94. Available at: http://www.journal.viam.ru (accessed: March 15, 2026). DOI: 10.18577/2713-0193-2021-0-1-80-94.
- Gorbovets M.A., Hodinev I.A., Karashaev M.M., Ryzhkov P.V. Low cycle dwell fatigue testing of heat resistant metallic materials (review). Trudy VIAM, 2022, no. 5 (111), pp. 123–137. Available at: http://www.viam-works.ru (accessed: February 26, 2026). DOI: 10.18577/2307-6046-2022-0-5-123-137.
- Hodinev I.A., Baranova E.V. Fatigue life of a heat-resistant titanium alloy at various loading frequencies. Trudy VIAM, 2024, no. 9 (139), pp. 71–82. Available at: http://www.viam-works.ru (accessed: February 26, 2026). DOI: 10.18577/2307-6046-2024-0-9-71-82.
- Stubbington C.A., Pearson S. Effect of dwell on the growth of fatigue cracks in Ti–6Al–4V alloy bar. Engineering Fracture Mechanics, 1978, vol. 10, is. 4, pp. 723–756.
- Gorbovets M.A. Cyclic crack resistance of heat-resistant nickel alloys for aircraft engines and power plants: thesis, Cand. Sc. (Tech.) Moscow, 2016, 107 p.
- Chesnutt J.C., Paton N.E. Hold time effects on fatigue crack propagation in Ti–6Al and Ti–6Al–4V. Metallurgical Transactions A, 1977, vol. 8, is. 7, pp. 1025–1037.
- Xu Y., Joseph S., Karamched P. et al. Predicting dwell fatigue life in titanium alloys using modelling and experiment. Nature Communications, 2020, vol. 11, art. 5868. DOI: 10.1038/s41467-020-19470-w.
- Su C.-Y., Zhou C.-Y., Lu L. et al. Effect of Temperature and Dwell Time on Fatigue Crack Growth Behavior of CP–Ti. Metals, 2018, vol. 8, no. 12, art. 1031. DOI: 10.3390/met8121031.
- Pilchak A., Fox K., Payton E. et al. Cold Dwell Fatigue of Titanium Alloys: History, Current State, and Aviation Industry Perspective: tech. rep. DOT/FAA/TC-23/40. Washington, 2024. Available at: https://rosap.ntl.bts.gov/view/dot/77938 (accessed: February 26, 2026). DOI: 10.21949/rfzv-6285.
- Hurley P.J., Whittaker M.T., Webster P., Evans W.J. A methodology for predicting creep/fatigue crack growth rates in Ti 6246. International Journal of Fatigue, 2007, vol. 29, is. 9, pp. 1702–1710. DOI: 10.1016/j.ijfatigue.2007.01.014.