E. V. Dvirnaya, E. A. Veshkin, G. V. Kornienko, O. V. Startsev Determination of durability based on the kinetic concept of strength in the development and manufacture of polymer composite materials // Proceedings of VIAM. 2026. No. 9 (163). С. 86-98. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-9-86-98.

Determination of durability based on the kinetic concept of strength in the development and manufacture of polymer composite materials

E. V. Dvirnaya1, E. A. Veshkin1, G. V. Kornienko1, O. V. Startsev1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

Durability variations were determined for VKU-39/VTkU-2.200 carbon fiber composites manufactured under different pressures and resin contents, as well as KMKS fiberglass in six filler and binder variations. Based on interlaminar shear test results at various loading rates, a thermal activation analysis was performed, which allowed to assess changes in durability and thermodynamic strength parameter depending on the material composition and manufacturing technology.

Keywords
carbon fiber reinforced polymer, glass fiber reinforced polymer, kinetic theory of strength, Zhurkov's equation, durability, thermal activation analysis, curing parameters
Reference list
  1. Chaffey B., Marchante-Rodriguez V., Brighton J., Grasso M. Degradation mechanisms effect on the mechanical properties of pultruded CFRPS: a review. Discover Polymers, 2025, vol. 2, no. 1, pp. 17. DOI: 10.1007/s44347-025-00029-1.
  2. Soloviev V.V., Rychkova A.D., Neretina A.S. Justification of the choice of material and technology for the manufacture of polymer composite materials. Kosmicheskie apparaty i tekhnologii, 2025, vol. 9, no. 2, pp. 79–86. DOI: 10.26732/j.st.2025.2.03.
  3. Barreira-Pinto R., Carneiro R., Miranda M., Guedes R.M. Polymer-matrix composites: characterising the impact of environmental factors on their lifetime. Materials, 2023, vol. 16, no. 11, p. 3913. DOI: 10.3390/ma16113913.
  4. Aleksandrov D.V., Malikov S.B. Prospects for the use of composite materials in aircraft manufacturing. Idei i novatsii, 2020, vol. 8, no. 3–4, pp. 160–163. DOI: 10.48023/2411-7943_2020_8_3_4_160.
  5. Janeikaitė J., Misiūnaitė I., Gribniak V. Fiber-Reinforced Polymer Laminates in Aviation and Structural Engineering: A Synthetic Comparison of Performance Requirements, Design Principles, and Defect Assessment Procedures. Materials, 2025, vol. 18, no. 21, p. 4938. DOI: 10.3390/ma18214938.
  6. Herbold E.B., Nesterenko V.F., Benson D.J. et al. Particle size effect on strength, failure, and shock behavior in polytetrafluoroethylene-Al-W granular composite materials. Journal of Applied Physics, 2008, vol. 104, no. 10. DOI: 104/10/103903/912097.
  7. Schlothauer A., Pappas G.A., Ermanni P. Thin-ply thermoplastic composites: from weak to robust transverse performance through microstructural and morphological tuning. Composites Part B: Engineering, 2023, vol. 261, p. 110764. DOI: 10.1016/j.compositesb.2023.110764.
  8. Adil S., Lazoglu I. A review on additive manufacturing of carbon fiber-reinforced polymers: Current methods, materials, mechanical properties, applications and challenges. Journal of Applied Polymer Science, 2023, vol. 140, no. 7, p. e53476. DOI: 10.1002/app.53476.
  9. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. Influence of technological parameters on characteristics of polymer composite materials in automated layup of prepregs (review). Trudy VIAM, 2021, no. 6 (100), pp. 46-55. Available at: http://www.viam-works.ru (accessed: February 03, 2026). DOI: 10.18577/2307-6046-2021-0-6-46-55.
  10. Mattlet A., Sicot O., Van Schoors L., Aivazzadeh S. Influence of processing and matrix parameters on the manufacturing of unidirectional flax/polypropylene composites. SN Applied Sciences, 2023, vol. 5, no. 12, p. 314. DOI: 10.1007/s42452-023-05457-x.
  11. Ivanov N.V., Gurevich Ya.M., Khaskov M.A., Akmeev A.R. Mode studying curing binding VSE-34 and its influences on mechanical properties. Aviacionnyye materialy i tehnologii, 2017, no. 2, pp. 50-55. DOI: 10.18577/2071-9140-2017-0-2-50-55.
  12. Okolie O., Latto J., Faisal N. et al. Manufacturing defects in thermoplastic composite pipes and their effect on the in-situ performance of thermoplastic composite pipes in oil and gas applications. Applied composite materials, 2023, vol. 30, no. 1, pp. 231-306. DOI: 10.1007/s10443-022-10066-9.
  13. Malysheva G.V., Guzeva T.A., Grashchenkov D.V., Raskutin A.E. The influence of heating technology on the duration of the curing process of polymer composite materials. Trudy VIAM, 2018, no. 8 (68), pp. 23-27. Available at: http://www.viam-works.ru (accessed: February 03, 2026). DOI: 10.18577/2307-6046-2018-0-8-23-27.
  14. Diaz-Rodriguez J.G., Pertuz-Comas A.D., Bohorquez-Becerra O.R. Impact strength for 3D-printed PA6 polymer composites under temperature changes. Journal of Manufacturing and Materials Processing, 2023, vol. 7, no. 5, p. 178. DOI: 10.3390/jmmp7050178.
  15. Liang J., Liu L., Qin Z. et al. Experimental study of curing temperature effect on mechanical performance of carbon fiber composites with application to filament winding pressure vessel design. Polymers, 2023, vol. 15, no. 4, p. 982. DOI: 10.3390/polym15040982.
  16. Singh J.I.P., Singh S., Dhawan V. Influence of fiber volume fraction and curing temperature on mechanical properties of jute/PLA green composites. Polymers and polymer composites, 2020, vol. 28, no. 4, pp. 273-284. DOI: 10.1177/0967391119872875.
  17. Parente J.M., Simoes R., Silva A.P., Reis P.N. Impact of the curing temperature on the manufacturing process of multi-nanoparticle-reinforced epoxy matrix composites. Materials, 2024, vol. 17, no. 8, p. 1930. DOI: 10.3390/ma17081930.
  18. Singh J.I.P., Singh S., Dhawan V. Effect of curing temperature on mechanical properties of natural fiber reinforced polymer composites. Journal of natural fibers, 2018, vol. 15, no. 5, pp. 687-696. DOI: 10.1080/15440478.2017.1354744.
  19. El-Hawary M.M., Abdel-Fattah H. Temperature effect on the mechanical behavior of resin concrete. Construction and Building Materials, 2000, vol. 14, no. 6-7, pp. 317-323. DOI: 10.1016/S0950-0618(00)00032-5.
  20. Stroe L.A., Crunteanu D.E., Botan M. et al. Thermo-Mechanical Behavior of Carbon Fiber Composites Processed at Elevated Temperatures. Polymers, 2026, vol. 18, no. 3, p. 401. DOI: 10.3390/polym18030401.
  21. Meng S.S., Zhang B.M. Effects of curing temperature on glass fiber/urethane composite’s mechanical and thermal properties. Materials Science Forum, 2015, vol. 813, pp. 194-201. DOI: 10.4028/www.scientific.net/MSF.813.194.
  22. Handwerker M., Wellnitz J., Marzbani H., Tetzlaff U. Pressure and heat treatment of continuous fiber reinforced thermoplastics produced by fused filament fabrication. Progress in Additive Manufacturing, 2023, vol. 8, no. 2, pp. 99-116. DOI: 10.1007/s40964-022-00315-5.
  23. Rajak D.K., Wagh P.H., Linul E. Manufacturing technologies of carbon/glass fiber-reinforced polymer composites and their properties: A review. Polymers, 2021, vol. 13, no. 21, p. 3721. DOI: 10.3390/polym13213721.
  24. Janiszewski J., Komorek A., Bakula M. et al. The influence of pressure in the infusion method upon mechanical properties of polymer composites. Advances in Science and Technology. Research Journal, 2023, vol. 17, no. 6. DOI: 10.12913/22998624/173382.
  25. Coulon P., Chatelain J.F., Dubé M., Rimpault X. Effect of curing pressure on machinability of carbon fiber composite. Procedia CIRP, 2018, vol. 77, pp. 307-310. DOI: 10.1016/j.procir.2018.09.022.
  26. Ivanov M.S., Morozova V.S., Pavlukovich N.G. Influence of technological modes of manufacture on properties of consolidated plates of carbon fiber reinforced thermoplastic based on polyetheretherketone. Trudy VIAM, 2025, no. 3 (145), pp. 60–69. Available at: http://www.viam-works.ru (accessed: February 03, 2026). DOI: 10.18577/2307-6046-2025-0-3-60-69.
  27. Gong J., Saeed N., Huang X. et al. Influences of fiber volume content on the mechanical properties of 2D plain carbon-fiber woven composite materials. Polymers, 2023, vol. 16, no. 1, p. 108. DOI: 10.3390/polym16010108.
  28. Damanik W.S., Siregar M.A., Lubis S. Evaluation of the effect of variations in resin and fiber composition on tensile and compressive properties of natural material composites. Hybrid Advances, 2025, vol. 10, p. 100434. DOI: 10.1016/j.hybadVol.2025.100434.
  29. Mishkin S.I., Zhakova L.S., Klimenko O.N., Vasilchuk E.A. Research of influence of the contents resin in CFRP on their mechanical properties. Trudy VIAM, 2023, no. 2 (120), pp. 77–86. Available at: http://www.viam-works.ru (accessed: February 05, 2026). DOI: 10.18577/2307-6046-2023-0-2-77-86.
  30. Petrov M.G., Startsev O.V., Lebedev M.P., Kopyrin M.M. Analysis of destruction and prediction of durability of carbon fiber reinforced plastic under various temperature-force conditions and environmental influences. Tselostnost i resurs v ekstremalnykh usloviyakh, 2024, no. 1, pp. 36–39. DOI: 10.24412/cl-37269-2024-1-36-39.
  31. Petrov M.G. Study of durability of materials using the kinetic concept of destruction. Prikladnaya mekhanika i tekhnicheskaya fizika, 2021, vol. 62, no. 1, pp. 165–178. DOI: 10.1134/S0021894421010181.
  32. Startsev O.V., Skirta A.A., Startsev V.O., Valevin E.O., Kogan A.M. Ageing of VKU-39 carbon plastic under moderately warm and tropical climate conditions. 1. Changes of strength indicators. Polymer Science, Series D, 2025, vol. 178, pp. 382–386.
  33. Petrov M.G., Startsev O.V., Lebedev M.P. et al. Strength characteristics of carbon fiber reinforced plastic in shear and cyclic extension-compression after 7 years of climate exposure. Universal Journal of Carbon Research, 2024, vol. 2, no. 1, pp. 1–13.
  34. Startsev O.V., Dvirnaya E.V., Kornienko G.V., Petrov M.G. The effect of moisture on the strength and durability of carbon fiber reinforced plastic. Trudy VIAM, 2026, no. 4 (158), pp. 68–84. Available at: http://www.viam-works.ru (accessed: February 05, 2026). DOI: 10.18577/2307-6046-2026-0-4-68-84.
  35. Regel V.R., Slutsker A.I., Tomashevsky E.E. Kinetic nature of the strength of solids. Moscow: Nauka, 1974, 560 p.
  36. Kablov E.N., Kirillov V.N., Startsev O.V., Krotov A.S. Climatic aging of composite aviation materials: II. Relaxation of the initial structural nonequilibrium and through-thickness gradient of properties. Russian Metallurgy (Metally), 2011, vol. 2011, no. 10, pp. 1001–1007. DOI: 10.1134/S0036029511100077.