Peculiarities of computer modeling in the development of technological processes for metal pressure processing (review)
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
Specialized software packages allow for the simulation of various plastic processing operations. Calculations are performed taking into account the properties of the deformed and tooling materials, as well as varying the process parameters of the deformation processes. This makes it possible to evaluate the manufacturability of various manufacturing schemes for deformed semi-finished products by analyzing various parameters, such as deformation, forces, temperature ranges, and others. This reduces the costs of direct experiments and the development of deformation technologies.
- Duyénova V.A., Pavlova T.V., Kashapov O.S., Chuchman O.V. Fatigue strength of forgings from VT6 alloy for parts of gas turbine engines and aircrafts. Aviation materials and technologies, 2023, no. 2 (71), pp. 23–35. Available at: http://www.journal.viam.ru (accessed: April 16, 2026). DOI: 10.18577/2713-0193-2023-0-2-23-35.
- Latushkin I.A., Yashin V.V., Suzdaltsev E.A., Aryshensky E.V. Mathematical model for calculating contact stresses during hot rolling of aluminum alloy strips on a five-ring continuous rolling mill. Aviation materials and technologies, 2025, no. 4 (81), pp. 15–22. Available at: http://www.journal.viam.ru (accessed: April 16, 2026). DOI: 10.18577/2713-0193-2025-0-4-15-22.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Storozhev M.V., Popov A.E. Theory of metal forming. Moscow: Mashinostroenie, 1977, 432 p.
- Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. High-temperature heat resisting nickel alloys for details of gas turbine engines. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 52–57.
- Afanasev-Hodykin A.N., Lukin V.I., Rylnikov V.S. High-tech semi-finished high-temperature solders (tape and paste on an organic binder). Trudy VIAM, 2013, no. 9, pp. 8–11. Available at: http://www.viam-works.ru (accessed: April 16, 2026).
- Aviation materials: a reference book in 9 vols. Ed. A. T. Tumanov. Moscow: ONTI, 1989, vol. 3: Heat-resistant steels and alloys, 566 p.
- Kablov E.N., Ospennikova O.G., Lomberg B.S. Complex innovative technology of isothermal punching on air in mode of superplasticity of disks from superhot strength alloys. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 129–141.
- Kablov E.N. Marketing of materials science, aircraft manufacturing and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5–6, pp. 40–44.
- Ospennikova O.G., Bubnov M.V., Kapitanenko D.V. Computer modeling of metal working processes by pressure. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 141–147.
- Tsepin M.A., Begnarsky V.V., Lisunets N.L., Sinitsyn M.V., Erokhov M.A. Use of specialized programs in the development of technological processes for metal forming. Tsvetnye metally, 2007, no. 5, pp. 98–101.
- Vlasov A.V., Stebunov S.A., Evsyukov S.A., Biba N.V., Shitikov A.A. Finite element modeling of technological processes of forging and die stamping. Moscow: Publ. house of Bauman MSTU, 2019, 384 p.
- Shpagin A.S., Bazhenov A.R., Antipov K.V., Oglodkova Yu.S. Study of rheological properties of aluminium-lithium alloy 1441 for computer modeling of metal forming processes. Aviation materials and technologies, 2025, no. 3 (80), pp. 37–46. Available at: http://www.journal.viam.ru (accessed: April 16, 2026). DOI: 10.18577/2713-0193-2025-0-3-37-46.
- Stebunov S.A., Biba N.V. Qform – a program created for technologists. Kuznechno-shtampovochno proizvodstvo, 2004, no. 9, pp. 38–43.
- Olimzhonov Zh.O., Sherbutaev N.I., Tataru A.S. Comparative analysis of the results of modeling the rolling process of hot-rolled sheet metal in the QForm VX environment with the technical characteristics of the rolling mill of JSC Uzmetkombinat. Litye i metallurgiya, 2024, no. 1, pp. 55–59.
- Al-Khuzai A.S.O., Shirokov V.V., Vydrin A.V. Determination of the range of change in the parameters of the stress-strain state of metal during continuous rolling of pipes. Vestnik YUUrGU. Ser.: Metallurgiya, 2019, vol. 19, no. 1, pp. 74–79.
- Radionova L.V., Faizov S.R., Gromov D.V., Erdakov I.N. Computer Modeling of Temperature Regimes during Semi-Continuous Direct Pressing of Low-Metal Materials. Vestnik YUUrGU. Ser.: Metallurgiya, 2020, vol. 20, no. 4, pp. 30–38.
- Tepin N.V., Dyakonova L.Yu., Tepina N.N. Computer Modeling of Stamping Technology for the Gear Part. Vestnik Priamurskogo gosudarstvennogo universiteta im. Sholom-Aleykhema, 2023, no. 1 (50), pp. 55–64.
- Tseplyaev I.K. Study of the cold stamping process under various friction conditions. Izvestiya TulGU. Tekhnicheskiye nauki, 2023, no. 4, pp. 354–356.
- Shpagin A.S., Kapitanenko D.V., Moiseev N.V., Bazhenov A.R. Development of the technology for manufacturing ring blanks made of EP648-VI alloy by isothermal air forging using low-power hydraulic presses. Aviation materials and technologies, 2024, no. 4 (77), pp. 17–26. Available at: http://www.journal.viam.ru (accessed: April 16, 2026). DOI: 10.18577/2713-0193-2024-0-4-17-26.
- Shpagin A.S., Bazhenov A.R., Antipov K.V., Oglodkova Yu.S. Construction of a rheological model of deformable aluminum alloy 1163 for computer simulation of metal pressure processes. Trudy VIAM, 2024, no. 10 (140), pp. 24–33. Available at: http://www.viam-works.ru (accessed: April 16, 2026). DOI: 10.18577/2307-6046-2024-0-10-24-33.