Forostovich T.L., Narsky A.R., Bityutskaya O.N. Application of dielectric heating in the removal of model compositions from shell molds in the production of cast blades for gas turbine engines.. Part 1 // Proceedings of VIAM. 2026. No. 8 (162). С. 41-50. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-8-41-50.
Application of dielectric heating in the removal of model compositions from shell molds in the production of cast blades for gas turbine engines.
Part 1
Abstract
Removal of model masses from ceramic shell molds is one of the complex technological operations in the manufacture of gas turbine engine parts by the method of investment casting. This review considers the possibilities of using dielectric (microwave) heating as a promising method for removing model compositions. In the first part, the article considers the features of the behavior of a material that does not conduct electric current and is placed in an electromagnetic field. Also the requirements for the designs of dielectric heating units are given, and the main areas of their use are listed.
Keywords
gas turbine engine, blades, superalloys, shell molds, precision casting, model compositions, electromagnetic radiation, microwaves
Reference list
- Investment Casting. Eds. Ya. I. Shklennik, V. A. Ozerov. 3rd ed. Moscow: Mashinostroenie, 1984, 408 p.
- Repyakh S. I. Technological Fundamentals of Investment Casting. Dnepropetrovsk: Lira, 2006, 1056 p.
- History of Aviation Materials Science. VIAM – 80 Years: Years and People. Ed. E. N. Kablov. Moscow: VIAM, 2012, 520 p.
- Kablov E.N. Cast Blades of Gas Turbine Engines. Alloys, Technologies, Coatings. 2nd ed. Moscow: Nauka, 2006, 632 p.
- Demonis I. M. At full speed. Nauka i zhizn, 2007, no. 6, pp. 40-44.
- Kovalenko T.S. «Burned» type defect on cast billets of heat-resistant nickel alloys (type ZhS32). Aviation materials and technologies, 2023, no. 4 (73), pp. 14-22. Available at: http://www.journal.viam.ru (accessed: March 18, 2026). DOI: 10.18577/2713-0193-2023-0-4- 14-22.
- Echlin A.B., Bondarenko Yu.A., Kolodyazhny M.Yu., Surova V.A. Review of perspective high-temperature superalloys based on refractory non-metallic materials for production of gas turbine engines. Aviation materials and technologies, 2023, no. 3 (72), pp. 30-41. Available at: http://www.journal.viam.ru (accessed: March 18, 2026). DOI: 10.18577/2713-0193-2023- 0-3-30-41.
- Kablov E.N., Svetlov I.L., Demonis I.M., Folomeikin Yu.I. Single-crystal blades with transpiration cooling for high-temperature gas turbine engines. Aviationnye materialy i tekhnologii, 2003, no. 1, pp. 24-33.
- Cast heat-resistant alloys. The effect of S.T. Kishkin: scientific and technical collection. Ed. E.N. Kablov. Moscow: Nauka, 2006, 272 p.
- Kablov E.N. S.T. Kishkin and his contribution to the development of science and materials science. Proceedings of the Int. sc. and tech. conf. «Scientific ideas of S.T. Kishkin and modern materials science». Moscow: VIAM, 2006, pp. 5-11.
- Forostovich T.L., Narsky A.R., Bityutskaya O.N. Removal of model compositions from shell molds in the production of cast gas turbine engine blades. Trudy VIAM, 2026, no. 2 (156), pp. 134-151. Available at: http://www.viam-works.ru (accessed: March 18, 2026). DOI: 10.18577/2307-6046-2026-0-2-3-12.
- Kablov E.N., Echlin A.B., Bondarenko Yu.A. History of development of directional crystallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), pp. 3-12. Available at: http://www.viam-works.ru (accessed: March 18, 2026). DOI: 10.18577/2307-6046-2020-0-3-3-12.
- Leushina L.I., Leushin I.O., Koshelev O.S. Improving the Efficiency of Hot Water Melting of Paraffin-Stearin Precision Casting Patterns. Chernye metally, 2019, no. 10, pp. 38-42.
- Method for Microwave Heat Treatment of Ceramic Casting Molds: pat. 2312733 Rus. Federation; appl. 03.03.05; publ. 20.12.07.
- Garanin V.F., Ozerov V.A., Murkina A.S., Kurenkova O.A. Melting of Patterns from Shell Molds. Liteynoe proizvodstvo, 1997, no. 2, pp. 16-19.
- Uglev N.P., Poilov V.Z., Merzlyakov K.S. et al. On the removal of pattern masses from ceramic shells during investment casting. Liteynoe proizvodstvo, 2015, no. 3, pp. 17-20.
- Sapchenko I.G., Evstigneev A.I., Kostina T.V. Features of removing patterns from shell molds in investment casting machines. Liteynoe proizvodstvo, 1999, no. 2, pp. 35-36.
- Forostovich T.L., Narsky A.R., Bityutskaya O.N. Removal of model compositions from shell molds using a boiler autoclave. Trudy VIAM, 2026, no. 4 (158), pp. 3-10. Available at: http://www.viam-works.ru (accessed: March 18, 2026). DOI: 10.18577/2307-6046-2026-0-4-3-10.
- Selivanov Yu.A. Microwave energy in the processes of investment casting shaping. Improving the quality and efficiency of investment casting: seminar materials. Moscow: MDNTP, 1989, pp. 91-97.
- Ozerov V.A., Garanin V.F., Murkina A.S. Melting of pattern compositions using microwave heating energy. Improving the quality and efficiency of investment casting: seminar materials. Moscow: MDNTP, 1986, pp. 108-110.
- Kablov E.N., Demonis I.M., Deev V.V., Bondarenko O.A., Narsky A.R. Technology of removing pattern masses from ceramic molds for investment casting. Liteynoe proizvodstvo, 2005, no. 3, pp. 12-14.
- Narsky A.R. Manufacturing of shell molds using microwave energy. Metallurgiya mashinostroeniya, 2005, no. 5, pp. 40-44.
- Zakhvatov Yu.K., Reva I.L., Podymov A.N. Removal of model masses from ceramic molds in a high-frequency current field. Aviation materials. Moscow, 1981, is. 6: Progressive processes of casting cooled blades. Eds. V.M. Stepanov, V.G. Chubarov, pp. 76-80.
- Gutko Yu.I., Voitenko V.V., Medvedchuk S.A. Experimental studies of melting wax models from plaster casting molds by microwave radiation. Science of the young – the future of Russia: Coll. art. VII All-Rus. sc.-pract. conf. Penza: MCNS «Science and education», 2024, pp. 67–70.
- Semenov A.S., Baiburin V.B. Microwave energy and its application. Features, equipment, technological processes. Saratov: Publ. house of Saratov Univ., 1999, 116 p.
- Arkhangelsky Yu.S. Dielectric heating units. Microwave units. Saratov: Saratov State Tech. Univ., 2003. 344 p.
- Knyazhevskaya G.S., Firsova M.G., Kilkeev R.Sh. High-Frequency Heating of Dielectric Materials. Ed. A.N. Shamov. 2nd ed., rev. and add. Leningrad: Mashinostroenie, 1989, 64 p.
- Modern Problems of Microwave Energy Application: Abstract of Report of the Int. Sc. and Tech. Conf. Ed. V.A. Sosunov. Saratov: Saratov State Tech. Univ., 1993, 104 p.
- Kolomeitsev V.A., Komarov V.V., Zheleznyak A.R. Microwave Systems with Uniform Volumetric Heating. Saratov: Saratov State Technical University, 2006, part 2, 232 p.
- Morozov O.G., Samigullin R.R., Nasybullin A.R. Microwave technologies in the processes of recycling and utilization of household polymer waste. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2010, vol. 12, no. 4 (3), pp. 580–582.
- Morozov S.M. Application of microwave radiation energy in the implementation and control of technological processes. Vyazma, 2012, 305 p.
The article was submitted
2026-05-12
approved and accepted for publication after reviewing
2026-05-14