Astashkin A.I., Zaysev D.V., Selivanov A.A., Tkachenko E.A. The influence of homogenization annealing on the structural phase evolution and technological plasticity of aluminum alloy 1163 ingots // Proceedings of VIAM. 2024. No. 7 (137). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-7-12-23.

The influence of homogenization annealing on the structural phase evolution and technological plasticity of aluminum alloy 1163 ingots

Astashkin A.I., Zaysev D.V., Selivanov A.A., Tkachenko E.A.
Abstract

Homogenization annealing of wrought aluminum alloys ingots is crucial for further processes such as hot and cold deformation due to the increasing uniformity of structure and technological plasticity. The paper presents the effects of homogenization parameters under various modes on microstructure evolution and technological plasticity of 1163 alloy (Al–Cu–Mg) ingots in the temperature range of 350–470 °C. The microstructure evolution in 1163 alloy was studied by optical microscopy, transmission electron microscopy and energy-dispersive X-ray spectroscopy.

Keywords
aluminum alloy 1163, Al‒Cu‒Mg system, homogenization annealing, microstructure, phase composition of ingots, technological plasticity
Reference list
  1. Kablov E.N. Modern materials are the basis of innovative modernization of Russia. Metally Evrazii, 2012, no. 3, pp. 10–15.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N., Nechaikina T.A., Somov A.V., Ivanov A.L., Murzabaeva O.Yu. The influence of heat treatment on the structure and properties of pressed semi-finished products from the promising super-strong aluminum alloy V-1977. Metallovedenie i termicheskaya obrabotka metallov, 2023, no. 1 (811), pp. 28–33.
  4. Nefedova Yu.N., Shlyapnikova T.A., Ivanov A.L., Sedelnikov V.V. Methods for reducing residual stresses during hardening of high-strength aluminum alloys. Trudy VIAM, 2023, no. 7 (125), paper no. 03. Available at: http://www.viam-works.ru (accessed: March 28, 2024). DOI: 10.18577/2307-6046-2023-0-7-23-33.
  5. Ovsyannikov B.V., Zamyatin V.M., Razinkin A.V., Mushnikov V.S. The influence of casting speed on the crystallization process and the structure of a large flat ingot of alloy 1163. Tekhnologiya legkikh splavov, 2020, no. 1, pp. 169–173.
  6. Tsukrov S.L., Isyakaev K.T. On the results of hardening sheets of alloy 1163 on a continuous heat treatment line. Tekhnologiya legkikh splavov, 2020, no. 1, pp. 35–38.
  7. Novikov I.I. Theory of heat treatment of metals. Moscow: Metallurgiya, 1978, 392 p.
  8. Belov N.A. Phase composition of industrial and advanced aluminum alloys. Moscow: MISIS, 2010, 511 p.
  9. Fridlyander I.N. Metallurgy of aluminum alloys. Moscow: Nauka, 1985, 238 p.
  10. Oglodkov M.S., Shchetinina N.D., Rudchenko A.S., Panteleev M.D. Directions of the development of promising aluminum-lithium alloys for aero-space engineering (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 19–29. DOI: 10.18577/2071-9140-2020-0-1-19-29.
  11. Kolobnev N.I., Ber L.B., Tsukanov S.L. Heat treatment of deformable aluminum alloys. Moscow: APRAL, 2020, 552 p.
  12. Zamyatin V.M., Grachev S.V., Grinenko M.A. et al. Rational alloying and modification of aluminum alloys based on the Al‒Cu‒Mg‒Mn and Al‒Zn‒Mg‒Cu systems. Neft i gaz, 2011, no. 3, pp. 106–112.
  13. Tkachenko E.A., Latushkina L.V. The influence of homogenization modes on the structure and properties of ingots and pressed-stamped semi-finished products from alloy 1933. Tekhnologiya legkikh splavov, 2003, no. 4, pp. 34–38.
  14. Astashkin A.I., Babanov V.V., Selivanov A.A., Tkachenko E.A. Structure and properties of massive forgings with a reduced level of residual stresses made of aluminum alloy 1933sb of balanced composition. Trudy VIAM, 2021, no. 7 (101), paper no. 02. Available at: http://www.viam-works.ru (accessed: December 18, 2023). DOI: 10.18577/2307-6046-2021-0-7-13-21.
  15. Vakhromov R.O., Tkachenko E.A., Lukina E.A., Selivanov A.A. Influence of homogenization annealing on structure and properties of ingots from 1933 alloy of Al–Zn–Mg–Cu system. Trudy VIAM, 2015, no. 11, paper no. 01. Available at: http://www.viam-works.ru (accessed: January 28, 2024). DOI: 10.18577/2307-6046-2015-0-11-1-1.
  16. Fridlyander I.N. Aluminum wrought structural alloys. Moscow: Metallurgiya, 1979, 208 p.
  17. Xiao Y.L., Qing L.P., Xi F. et al. Microstructural evolution of Al–Cu–Mg–Ag alloy during homogenization. Journal of Alloys and Compounds, 2009, vol. 484, pp. 790–794.
  18. Huang T., Qin Y., Chao D. et al. Study on homogenization process of large size Al‒Cu‒Mg‒Mn alloy ingot. Materials reports, 2020, vol. 24, is. Z1, pp. 325–327.
  19. Lin H., Zhu K., Liu Q. et al. Microstructural characterization of the as-cast and homogenized Al‒Cu‒Mg‒Ag alloy. Materials, 2023, vol. 16, is. 1, pp. 433–441.
  20. Liu Q., Li X., Li Z. et al. Effect of Cu content on microstructures of as-cast and homogenized Al‒Cu‒Mg‒Ag alloys. Key engineering materials, 2022, vol. 921, pp. 59–64.
  21. Jian Wang, Yalin Lu, Dongshuai Zhou et al. Influence of homogenization on microstructural response and mechanical property of Al‒Cu‒Mn alloy. Materials (Basel), 2018, vol. 11, is. 6, pp. 914–921.
  22. Antipov V.V., Tkachenko E.A., Zajtsev D.V., Selivanov A.A., Ovsyannikov B.V. Тhe influence of homogenizing annealing regimes on the structural phase state and mechanical properties of aluminum-lithium alloy 1441 ingots. Trudy VIAM, 2019, no. 3 (75), paper no. 05. Available at: http://www.viam-works.ru (accessed: December 18, 2023). DOI: 10.18577/2307-6046-2019-0-3-44-52.
  23. Oglodkov M.S., Romanenko V.A., Benarieb I., Rudchenko A.S., Grigoryev M.V. Study of industrial semi-finished products from advanced aluminum-lithium alloys for aircraft products. Aviation materials and technologies, 2023, no. 3 (72), paper no. 05. Available at: http://www.journal.viam.ru (accessed: December 18, 2023). DOI: 10.18577/2713-0193-2023-0-3-62-77.
  24. Liu X.Y., Pan Q.L., Fan X. et al. Microstructural evolution of Al‒Cu‒Mg‒Ag alloy during homogenization. Journal Alloys Compounds, 2009, vol. 484, pp. 790–794.
  25. Li H.Z., Ou Y.J., Liao H.J. et al. Microstructural evolution of high purity Al‒Cu‒Mg alloy during homogenization. Materials Science Forum, 2014, vol. 788, pp. 208‒214.