Sevalnev G.S., Vlasov I.I., Klimov V.S., Nefedkin D.Yu. Evaluation of resistance to contact-deformation impact during intensive wear of the surface of cast entropy alloys based on the Ni–Co–Cr system // Proceedings of VIAM. 2024. No. 11 (141). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2024-0-11-3-13.

Evaluation of resistance to contact-deformation impact during intensive wear of the surface of cast entropy alloys based on the Ni–Co–Cr system

Sevalnev G.S., Vlasov I.I., Klimov V.S., Nefedkin D.Yu.
Abstract

The tribological characteristics of entropy alloys based on the Ni–Co–Cr alloying system under contact-deformation impact under dry sliding friction conditions were studied. The results of the studies showed that the hardness of the equimass alloy is 10 % greater than equiatomic alloy, and the use of additional alloying increases the hardness of the equiatomic alloy by 20–45 %. The wear resistance of the alloys depends slightly on the hardness and, to a greater extent, on hardening due to the accumulation of subsurface defects.

Keywords
entropy alloys, alloying, structure, hardness, wear resistance, contact deformation
Reference list
  1. Sevalnev G.S. Beryllium-containing steels – perspective material with a high level of physical and mechanical properties. Aviation materials and technologies, 2023, no. 3 (72), paper no. 02. Available at: http://www.journal.viam.ru (accessed: July 25, 2024). DOI: 10.18577/2713-0193-2023-0-3-15-29.
  2. Kaplanskii Yu.Yu., Mazalov P.B. World trends in the development of refractory high-entropy alloys for heat-loaded units of aerospace technics (review). Aviation materials and technologies, 2022, no. 2 (67), paper no. 03. Available at: http://www.journal.viam.ru (accessed: July 25, 2024). DOI: 10.18577/2713-0193-2022-0-2-30-42.
  3. Kablov E.N., Sidorov V.V., Min P.G., Vadeev V.E., Kramer V.V. Research and development of technological parameters for vacuum melting of corrosion-resistant heat-resistant nickel alloys. Metallurg, 2021, no. 2, pp. 62–67.
  4. Trofimenko N.N., Efimochkin I.Yu., Bolshakova A.N. Problems of creation and prospects for the use of heat-resistant high-entropy alloys. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 3–8. DOI: 10.18577/2071-9140-2018-0-2-3-8.
  5. Singh S., Wanderka N., Glatzel U., Banhart J. Decomposition in multi-component AlCoCrCuFeNi highentropy alloy. Acta Materialia, 2011, vol. 59, pр. 182–190. DOI: 10.1016/j.actamat.2010.09.023.
  6. Trofimenko N.N., Efimochkin I.Yu., Osin I.V., Dvoretskov R.M. The research of the possibility of high entropy alloy VNbMoTaW production by mixing elementary powders with further hybrid spark plasma sintering. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 12–20. DOI: 10.18577/2071-9140-2019-0-2-12-20.
  7. Cantor B., Chang I.T.H., Knight P., Vincent A.J.B. Microstructural development in equiatomic multicomponent alloys. Materials Science and Engineering: A, 2004, vol. 375–377, pр. 213–218. DOI: 10.1016/j.msea.2003.10.257.
  8. Cantor B. Multicomponent and high entropy alloys. Entropy, 2014, vol. 16, no. 9, pр. 4749–4768.
  9. Yeh J.-W., Chen S.-K., Lin S.-J. et al. Nanostructured highentropy alloys with multiple principal elements: novel alloy design concepts and outcomes. Advanced Engineering Materials, 2004, vol. 6, p. 299–303. DOI: 10.1002/adem.200300567.
  10. Yeh J.W. Recent progress in high-entropy alloys. Annales de Chimie-Science des Materiaux, 2006, vol. 31, pр. 633–648. DOI: 10.3166/acsm.31.633-648.
  11. Smith T. GRX-810: NASA High Temperature Alloy Development for Additive Manufacturing. 2022. Available at: https://ntrs.nasa.gov/citations/20220013032 (accessed: July 25, 2024).
  12. Smith T. High Temperature Alloy Development for AM–GRX-810. Available at: ntrs.nasa.gov/citations/20230010486 (accessed: July 25, 2024).
  13. NASA’s New Material Built to Withstand Extreme Conditions. Available at: https://www.nasa.gov/aeronautics/nasas-new-material-built-to-withstand-extreme-conditions/ (accessed: July 25, 2024).
  14. Soleimani M., Kalhor A., Mirzadeh H. Transformation-induced plasticity (TRIP) in advanced steels: a review. Materials Science and Engineering: A, 2020, vol. 795, p. 140023.
  15. De Cooman B.C., Estrin Y., Kim S.K. Twinning-induced plasticity (TWIP) steels. Acta Materialia, 2018, vol. 142, pр. 283–362.
  16. Lukin E.I., Ashmarin A.A., Bannykh I.O. et al. Study of the influence of the reduction value during cold rolling on the phase composition, texture and residual stresses in 20Kh15AN3MD2 steel. Metals, 2023, no. 6, pp. 26–34. DOI: 10.31857/S0869573323060046.
  17. Sevalnev G.S., Gromov V.I., Dulnev K.V., Sevalneva T.G. Contact endurance of nitrogenous austenitic-martensitic steels with different hardening mechanism. Aviation materials and technologies, 2024, no. 2 (75), paper no. 01. Available at: http://www.journal.viam.ru (accessed: July 25, 2024). DOI: 10.18577/2713-0193-2024-0-2-3-14.
  18. Miracle D.B., Senkov O.N. A critical review of high entropy alloys and related concepts. Acta Materialia, 2017, vol. 122, pр. 448–511. DOI: 10.1016/j.actamat.2016.08.081.
  19. George E.P., Raabe D., Ritchie R.O. High-entropy alloys. Nature Reviews Materials, 2019, vol. 4, pр. 515–534. DOI: 10.1038/s41578-019-0121-4.
  20. Zhang Y., Zhou Y.J., Lin J.P. et al. Solid-solution phase formation rules for multi-component alloys. Advanced Engineering Materials, 2018, vol. 10 (6), pр. 534–538. DOI: 10.1002/adem.200700240.
  21. Moghaddam P.V., Hardell J., Vuorinen E., Prakash B. The role of retained austenite in dry rolling/sliding wear of nanostructured carbide-free bainitic steels. Wear, 2019, vol. 428, pр. 193–204.
  22. Harzallah R., Mouftiez A., Felder E. et al. Rolling contact fatigue of Hadfield steel X120Mn12. Wear, 2010, vol. 269. No. 9-10, pр. 647–654.
  23. Sevalnev G.S., Sevalneva T.G., Kolmakov A.G., Dulnev K.V., Krylov S.A. Study of the tribo-technical characteristics of corrosion-resistant steels with different mechanisms of volumetric hardening. Trudy VIAM, 2021, no. 10 (104), paper no. 01. Available at: http://www.viam-works.ru (accessed: July 25, 2024). DOI: 10.18577/2307-6046-2021-0-10-3-11.