Antipov V.V., Krivushina A.A., Startsev V.O., Kogan A.M. Study of the paint coatings properties after impact of micromycetes in a moderate and moderate warm climate // Proceedings of VIAM. 2023. No. 6 (124). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-6-130-141.

Study of the paint coatings properties after impact of micromycetes in a moderate and moderate warm climate

Antipov V.V., Krivushina A.A., Startsev V.O., Kogan A.M.
Abstract

The properties of paint coatings under the influence of standard test cultures and microscopic fungi isolated under natural conditions of a temperate (Moscow) and moderately warm climate (Gelendzhik) were studied. Changes in the decorative properties of coatings VE-69 and EP-140 after exposure to individual strains of micromycetes were revealed. It is shown that the color change of VE-69 and EP-140 coatings with red pigment is higher than for coatings of similar enamels with gray pigment. The study of adhesive properties did not reveal any changes on all samples, both after standard tests with test cultures according to GOST 9.049–91, and after long-term (45 and 90 days) exposure to monocultures of micromycetes isolated in temperate and moderately warm climates.

Keywords
biodeterioration, paint coatings, degrading microorganisms, microbiological resistance, microbiological damage, micromycetes, polymeric materials, enamels
Reference list
  1. Startsev O.V., Molokov M.V., Erofeev V.T. Investigation of the impact of mold fungi on wood and its protective epoxy coatings by dynamic mechanical spectroscopy. Vse materialy. Entsiklopedicheskiy spravochnik, 2016, no. 4, pp. 34–42.
  2. Polyakova A.V., Krivushina A.A., Goryashnik Yu.S., Buharev G.MMicrobiological resistance tests under nature conditions in variety of climatiс zones. Trudy VIAM, 2016, no. 4, paper no. 11. Available at: http://www.viam-works.ru (accessed: December 22, 2022). DOI: 10.18577/2307-6046-2016-0-4-11-11.
  3. Startsev V.O., Molokov M.V., Startsev O.V., Nizina T.A., Nizin D.R. Influence of the aliphatic thinner ETAL-1 on the climatic resistance of epoxy polymers based on ED-20 resin. Vse materialy. Entsiklopedicheskiy spravochnik, 2016, no. 12, pp. 26–36.
  4. Kablov E.N., Startsev V.O. Influence of internal stresses on the aging of polymer composite materials. Review. Mekhanika kompozitnykh materialov, 2021, vol. 57, no. 5, pp. 805–822.
  5. Kablov E.N., Startsev O.V., Medvedev I.M. Corrosive aggressiveness of the coastal atmosphere. 2. New approaches to assessing the corrosiveness of coastal atmospheres. Korroziya: materialy, zashchita, 2016, no. 1, pp. 1–15.
  6. Startsev O.V., Medvedev I.M., Kurs M.G. Hardness as the indicator of corrosion of aluminum alloys in sea conditions. Aviacionnye materialy i tehnologii, 2012, no. 3, pp. 16–19.
  7. Batraev I.S., Rybin D.K., Ivanyuk K.V., Ulianitsky V.Yu., Shtertser A.A. Wear resistant detonation coatings based on tungsten carbide for aviation products. Aviation materials and technologies, 2022, no. 1 (66), paper no. 08. Available at: http://www.journal.viam.ru (ассеssed: December 22, 2022). DOI:10.18577/2713-0193-2022-0-1-92-109.
  8. Merkulova Yu.I., Kuznetsova V.A., Kodachenko E.N., Zheleznyak V.G. Study of the influence of the primer layer’s chemical nature on the properties of the coating system based on fluoropolyurethane enamel. Aviation materials and technologies, 2022, no. 1 (66), paper no. 09. Available at: http://www.journal.viam.ru (ассеssed: December 22, 2022). DOI: 10.18577/2713-0193-2022-0-1-110-119.
  9. Zheleznyak V.G., Serdcelyubova A.S., Merkulova Yu.I., Skivko P.V. Paint coating system based on polyurethane enamel for protecting heated frontal surfaces of aviation products. Aviation materials and technologies, 2022, no. 1 (66), paper no. 10. Available at: http://www.journal.viam.ru (ассеssed: December 22, 2022). DOI: 10.18577/2713-0193-2022-0-1-120-128.
  10. Merkulova Yu.I., Kurshev E.V., Vdovin A.I., Andreeva N.P. Microstructural and electrochemical studies of paint coatings under natural climate tests of tropical climate of North America. Aviation materials and technologies, 2022, no. 2 (67), paper no. 11. Available at: http://www.journal.viam.ru (accessed: December 22, 2022). DOI: 10.18577/2713-0193-2022-0-2-120-130.
  11. Rojas T.I., Aira M.J., Batista A. et al. Fungal biodeterioration in historic buildings of Havana (Cuba). Grana, 2012, vol. 51, is. 1, pp. 44–51.
  12. Popikhina E.A., Trepova E.S. Mikodestruktory building materials. Report Fourth Congress of Russian Mycologists "Modern Mycology in Russia". Moscow: National Academy of Mycology, 2017, vol. 6, pp. 424–426.
  13. Ogarkova G.R., Bukovskaya N.E., Samusenok L.V., Ogarkov B.N. Biodamage of porous building materials by associations of specific microorganisms. Report Third Congress of Russian Mycologists "Modern Mycology in Russia". Moscow: National Academy of Mycology, 2012, vol. 3, pp. 224–225.
  14. Balyuta A.A., Vazhinskaya I.S. The resistance of modern building materials to mold damage. Report Third Congress of Russian Mycologists "Modern Mycology in Russia". Moscow: National Academy of Mycology, 2012, vol. 3, pp. 210.
  15. Kataev A.D., Kurakov A.V. Microbial colonization and destruction of biodegradable synthetic materials based on polyhydroxybutyrate and polyhydroxyvalerate in soils. Report Third Congress of Russian Mycologists "Modern Mycology in Russia". Moscow: National Academy of Mycology. 2012, vol. 3, pp. 218–219.
  16. Goncharova I.A., Sabadakha E.N., Trigubovich A.M., Chernaya N.V. Mycological analysis of industrial materials contaminated with microscopic fungi. Proceedings of BSTU. Ser.: 2, 2020, no. 2, pp. 163–168.
  17. Smolyanitskaya O.L. Micromycetes as potential agents of biodamage of cultural values and a strategy for protection against them in the State Hermitage Museum: thesis, Cand Sc. (Biol.). SPb., 2007, 26 p.
  18. Sevastyanov D.V., Sutubalov I.V., Daskovskij M.I., Shein E.A. Polymer biocomposites based on biodegradable binders reinforced by natural fibers (review). Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 42–50. DOI: 10.18577/2071-9140-2017-0-4-42-50.
  19. Goryaeva A.G., Velikova T.D., Dobrusina S.A. Mycobiota of air and polymer-coated paper composites in the Russian National Library. Mikologiya i fitopatologiya, 2010, no. 44 (1), pp. 10–18.
  20. Lugauskas A.Yu., Mikulskene A.I., Shlyauzhene D.Yu. Catalog of micromycetes – biodestructors of polymeric materials. Moscow: Nauka, 1987, pp. 258–259.