Gorlov D.S., Kashin D.S., Azarovskiy E.N., Druzhnova Ya.S. Technological methods of ion processing with applying condensation-diffusion coating // Proceedings of VIAM. 2023. No. 12 (130). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-12-87-97.

Technological methods of ion processing with applying condensation-diffusion coating

Gorlov D.S., Kashin D.S., Azarovskiy E.N., Druzhnova Ya.S.
Abstract

The results of gradient deposition of a condensation-diffusion coating to protect a nickel alloy from sulfide-oxide corrosion and high-temperature oxidation are presented in order to obtain the minimum size of the droplet phase at the initial moment of deposition when the bias voltage is operating in constant or pulse modes. It is established that the displacement operating modes do not significantly affect the adhesive component and the number of defects at the alloy-coating interface, and the gradient onset of deposition increases these characteristics.

Keywords
gradient deposition, condensation-diffusion coating, sulfide-oxide corrosion, high-temperature oxidation, constant displacement voltage, pulse displacement voltage, alloy-coating interface
Reference list
  1. VIAM 90 years: We are proud of the past, create the future. Ed. E.N. Kablov. Moscow: NIC «Kurchatov Institute» – VIAM, 2022, pp. 97–103.
  2. Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crystallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), paper no. 01. Available at: http://www.viam-works.ru (accessed: July 10, 2023). DOI: 10.18577/2307-6046-2020-0-3-3-12.
  3. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nickel foundry heat resisting alloys of new generation. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 36–52.
  4. Bazyleva O.A., Arginbayeva E.G., Lutskaya S.A., Dmitriev N.S. Foundry intermetallic alloy based on Ni3Al compound for turbine blades gas turbine engines. Aviation materials and technologies, 2022, no. 2 (67), paper no. 01. Available at: http://www.journal.viam.ru (accessed: July 11, 2023). DOI: 10.18577/2713-0193-2022-0-2-5-17.
  5. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577/2071-9140-2019-0-2-3-11.
  6. A method of applying a combined heat-resistant coating: pat. 2402633 Rus. Federation; appl. 31.03.09; publ. 27.10.10.
  7. A method of processing the surface of a metal product: pat. 2368701 Rus. Federation; appl. 08.11.07; publ. 27.09.09.
  8. Muboyajyan S.A., Kablov E.N., Budinovsky S.A. Vacuum-plasma technology for obtaining protective coatings from complex alloy alloys. Metallovedeniye i termicheskaya obrabotka metallov, 1995, no. 2, рр. 15–18.
  9. Budinovsky S.A., Muboyajyan S.A. The effectiveness of a two-stage ion-plasma technology for obtaining alloy diffusion aluminum coatings on heat-resistant nickel alloy. Metallovedeniye i termicheskaya obrabotka metallov, 2003, no. 5, pp. 27–32.
  10. Muboyadzhyan S.A., Budinovskij S.A. Ion-plasma technology: prospective processes, coatings, equipment. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 39–54. DOI: 10.18577/2071-9140-2017-0-S-39-54.
  11. Kablov E.N., Muboyajyan S.A., Budinovsky S.A., Egorova L.P., Lutsenko A.N., Galoyan A.G. Protective and strengthening coatings of the blades and parts of the GTD. 75 years. Aviation materials. Moscow: VIAM, 2007, pp. 27–44.
  12. Belous V.Ya., Zhirnov A.D., Lutsenko A.N., Muboyajyan S.A. Increase in corrosion resistance of steel blades of the compressor of the GTD by using ion-plasma coating. Aviacionnye materialy i tehnologii, 2006, no. 1, pp. 53–60.
  13. Matveev P.V., Budinovskij S.A. Research of the properties of protective heat-resistant coating for intermetallic nickel alloys operating at temperatures up to 1300 °C. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 22–26.
  14. Muboyajyan S.A., Budinovsky S.A. Heat-resistant high-temperature ion-plasma coatings for turbines of modern GTD. Aviacionnye materialy i tehnologii, 2003, no. 1, pp. 92–102.
  15. Aleksandrov D.A., Muboyadzhyan S.A., Zhuravleva P.L., Gorlov D.S. Investigation of the effect of surface preparation and ion-assisted deposition on the structure and properties of erosion-resistant ion-plasma coating. Trudy VIAM, 2018, no. 10 (70), paper no. 08. Available at: http://www.viam-works.ru (accessed: July 20, 2023). DOI: 10.18577/2307-6046-2018-0-10-62-73.
  16. Budinovsky S.A., Lyapin A.A., Benklyan A.S. Expensive industrial-plasma installations of MASH-50 and MAP-R for applying protective coatings to parts of transport and energy gas turbine installations. Inzhenernyy zhurnal: nauka i innovatsii, 2021, no. 10, pp. 1–13. DOI: 10.18698/2308-6033-2021-10-2120.
  17. Azarovskiy E.N., Doronin O.N., Muboyadzhyan S.A. Formation of porosity on the border «of heat-resistant alloy–heat-resistant condensation-diffusion coating». Trudy VIAM, 2019, no. 2 (74), paper no. 12. Available at: http://www.viam-works.ru (accessed: July 17, 2023). DOI: 10.18577/2307-6046-2019-0-2-113-120.