Kuznetsov B.Yu., Vlasov I.I., Grinevich D.V., Sorokin O.Ju. Modeling the destruction of a metal-ceramic composite material with a multilayer structure by the finite element method // Proceedings of VIAM. 2023. No. 11 (129). Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-11-99-110.

Modeling the destruction of a metal-ceramic composite material with a multilayer structure by the finite element method

Kuznetsov B.Yu., Vlasov I.I., Grinevich D.V., Sorokin O.Ju.
Abstract

The purpose of this work is to determine the effect of the transitional diffusion zone at the interfacial boundary of the layers of the ceramic composite material of the Mo–Si–B system on the nature of destruction and physical and mechanical properties. Qualitative models have been created that make it possible to predict the most critical fracture zones of a composite material, and the effect of microstructure on the fracture mechanisms has been studied. Field tests of a ceramic-metal composite material with a multilayer structure were carried out, as a result of which a high convergence with the calculated models was established.

Keywords
composite material, multilayer structure, crack resistance, mechanical properties, finite element method, elasticity model, plasticity model
Reference list
  1. Nozhnitsky Y.A., Fedina Y.A., Rekin A.D. et al. Development and investigation of ceramic parts for gas-turbine engines. International Gas Turbine and aeroengine congress and exhibition. Orlando, 1997, pp. 1–8.
  2. Carollo V., Reinoso J., Paggi M. Modeling complex crack paths in ceramic laminates: A novel variational framework combining the phase field method of fracture and the cohesive zone model. Journal of the European Ceramic Society, 2018, vol. 38, no. 7, pp. 4565–4567.
  3. Korzhov V.P., Kijko V.M. Structure of layered Mo–Si–B and Nb–Si–B composites. 9th Int. Conf. «Phase transformation and crystal strength». Chernogolovka, 2016, p. 155.
  4. Jain M.K., Subrahmanyam J., Ray S. Development of Mo and Ta foil reinforced (MoSi2 + 20 vol% SiCp) matrix laminated composites. Advanced Materials Research, 2012, vol. 585, pp. 306–310.
  5. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Wang H., Wang C. Preparation and mechanical properties of laminated zirconium diboride/molybdenum composites sintered by spark plasma sintering. Frontiers Material Science in China. 2009, vol. 3, pp. 273–280.
  7. Cheng L., Sun M., Ye F. Structure design, fabrication, properties of laminated ceramics: A review // International Journal of Lightweight Materials and Manufacture, 2018, vol. 1, pp. 126–141.
  8. Garshin A.P., Nilov A.S., Galinskaya O.O., Krasnov V.I. Prospects for development and ways to improve aircraft braking systems on the base ceramic matrix composite materials (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 09. Available at: http://www.journal.viam.ru (accessed: June 13, 2023). DOI: 10.18577/2713-0193-2023-0-2-104-121.
  9. Kablov E.N., Antipov V.V., Girsh R.I. Constructed layered materials based on sheets of aluminum-lithium alloys and fiberglass in the structures of new generation aircraft. Vestnik mashinostroyeniya, 2020, no. 12, pp. 46–52.
  10. Sevalnev G.S., Dulnev K.V., Bannykh I.O., Krasulya A.A., Tsikh S.G., Lukin E.I. Investigation of the structure and properties of diffusion layers after boriding high nitrogen steels. Aviation materials and technologies, 2023, no. 1 (70), paper no. 02. Available at: http://www.journal.viam.ru (accessed: April 27, 2023). DOI: 10.18577/2307-6046-2023-0-1-17-29.
  11. Shuwei Z., Rabczuk T., Zhuang X. Phase field modeling of quasi-static and dynamic crack propagation: COMSOL implementation and case studies. Advances in Engineering Software, 2018, no. 122, pp. 31–49.
  12. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  13. Voronov V.A., Chainikova A.S., Lebedeva Yu.E., Zhitnyuk S.V. Production, physico-mechanical and tribotechnical properties of hot-pressed carbon-ceramic composite material on the basis of silicon carbide. Aviation materials and technologies, 2022, no. 2 (67), paper no. 07. Available at: http://www.journal.viam.ru (accessed: April 14, 2023). DOI: 10.18577/2713-0193-2022-0-2-74-84.
  14. Kiiko V., Prokhorov D., Stroganova T. Investigation of heat resistance and structure of layered refractory composites reinforced by chemical compound with silicon, carbon, and boron. Scientific proceedings XIV International congress «Machines. Technologies. Materials», 2017, vol. VII, pp. 544–547.
  15. Goncharov B.E., Sipatov A.M., Cherkashneva N.N., Pleskan A.Yu., Samokhvalov N.Yu., Vaganova M.L., Sorokin O.Yu., Solntsev St.S., Evdokimov S.A. Studies of thermal shock resistance of an anti-oxidation coating for a multi-layered ceramic composite. Aviation materials and technologies, 2021, no. 4 (65), paper no. 06. Available at: http://www.journal.viam.ru (accessed: April 23, 2023). DOI: 10.18577/2713-0193-2021-0-51-58.
  16. Kiyko V.M., Korzhov V.P. Structure of layered composites Mo–Si–B and Nb–Si–B. Izvestiya RAN, ser.: Physical, 2017, vol. 81, no. 11, pp. 1513–1521.
  17. Biamino S., Antonini A., Pavese M. MoSi2 laminate processed by tape casting: Microstructure and mechanical properties’ investigation. Intermetallics, 2008, vol. 16, pp. 758–768.
  18. Korzhov V.P., Kiyko V.M. Phase structure of multilayer Nb/(Si–B) and Mo/(Si–B) composites after heat treatment under pressure. VI All-Rus. Conference on Nanomaterials. Moscow, 2016, pp. 386–387.