Shoshev F.L., Bogachev I.A., Sukhov D.I. The features of processing an aluminum matrix composite material by selective laser melting // Proceedings of VIAM. 2023. No. 11 (129). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-11-66-76.
The features of processing an aluminum matrix composite material by selective laser melting
Abstract
The structure of aluminum matrix composite powder reinforced by silicon carbide particles and then spheroidized is investigated. The structure of selective laser melting material made of this powder is investigated as well. The main principles of forming of such structure are determined. In addiction an effect of gasostatic and heat treatment on selective laser melting material structure is considered.
Keywords
aluminum matrix composite, selective laser melting, plasma treatment, spheroidizing, additive manufacturing, structure
Reference list
- Kanth U.R., Rao P.S., Krishna M.G. Mechanical behaviour of fly ash/SiC particles reinforced Al–Zn alloy-based metal matrix composites fabricated by stir casting method. Journal of Materials Research and Technology, 2019, vol. 8, no. 1, pp. 737–744. DOI: 10.1016/J.JMRT.2018.06.003.
- Kablov E.N., Evgenov A.G., Petrushin N.V., Shurtakov S.V., Zaitsev D.V. To the question of the mechanism of the formation of the thin structure of the track in the process of selective laser rafting. Metallovedenie i termicheskaya obrabotka metallov, 2023, no. 2 (812), pp. 44–55. DOI: 10.30906/Mitom.2023.2.44-55.
- Aslanian G.G., Sukhov D.I., Mazalov P.B., Sulyanova E.A. Fractographic study of Co–Cr–Ni–W–Ta alloy samples obtained by selective laser melting. Trudy VIAM, 2019, no. 4 (76), paper no. 01. Available at: http://www.viam-works.ru (accessed: August 16, 2023). DOI: 10.18577/2307-6046-2019-0-4-3-10.
- Ospennikova O.G., Naprienko S.A., Medvedev P.N., Zaitsev D.V., Rogalev A.M. Features of the formation of the structural-phase state of the EP648 alloy during selective lase manufacture. Trudy VIAM, 2021, no. 8 (102), paper no. 01. Available at: http://www.viam-works.ru (accessed: August 16, 2023). DOI: 10.18577/2307-6046-2021-0-8-3-11.
- Nerush S.V., Kaplanskii Yu.Yu., Dynin N.V., Benarieb I., Savichev I.D. Development of laser powder bed fusion parameters, structure and mechanical properties of a high-strength aluminum alloy Al–Ce–Cu. Trudy VIAM, 2023, no. 1 (119), paper no. 05. Available at: http://www.viam-works.ru (accessed: August 16, 2023). DOI: 10.18557/2307-6046-2023-0-1-50-68.
- Sukhov D.I., Kaplansky Yu.Yu., Rogalev A.M., Kurkin S.E. The features of processing Cr-rich nickel based alloy by selective laser melting. Trudy VIAM, 2023, no. 1 (119), paper no. 02. Available at: http://www.viam-works.ru (accessed: August 16, 2023). DOI: 10.18557/2307-6046-2023-0-1-15-27.
- Stoyakina E.A., Kurbatkina E.I., Simonov V.N., Kosolapov D.V., Gololobov A.V. Mechanical properties of aluminium-matrix composite materials reinforсed with SiC particles, depending on the matrix alloy (review). Trudy VIAM, 2018, no. 2, paper no. 08. Available at: http://www.viam-works.ru (accessed: August 16, 2023). DOI: 10.18577 / 2307-6046-2018-0-2-8-8.
- Nyafkin A.N., Shavnev A.A., Kurbatkina E.I., Kosolapov D.V. Studying the effect of silicon carbide particle size on the linear thermal expansion coefficient of the composite material based on aluminum alloy. Trudy VIAM, 2020, no. 2 (86), paper no. 05. Available at: http://www.viam-works.ru (accessed: August 16, 2023). DOI: 10.18577/2307-6046-2020-0-2-41-49.
- Martin J.H., Yahata B.D., Hundley J.M. et al. 3D printing of high-strength aluminium alloys. Nature, 2017, vol. 549, pp. 365−369. DOI: 10.1038/nature23894.
- Spigarelli S., Paoletti C. A new model for the description of creep behaviour of aluminium-based composites reinforced with nanosized particles. Composites Part A: Applied Science and Manufacturing, 2018, vol. 112, pp. 346−355. DOI: 10.1016/j.compositesa.2018.06.021.
- Loh L.E., Chua C.K., Yeong W.Y. et al. Numerical investigation and an effective modelling on the selective laser melting (SLM) process with aluminium alloy 6061. International Journal of Heat and Mass Transfer, 2015, vol. 80, pp. 288−300. DOI: 10.1016/j.ijheatmasstransfer.2014.09.014.
- Chang F., Gu D., Dai D., Yuan P. Selective laser melting of in-situ Al4SiC4+SiC hybrid reinforced Al matrix composites: Influence of starting SiC particle size. Surface and Coatings Technology, 2015, vol. 272, pp. 15−24. DOI: 10.1016/j.surfcoat.2015.04.029.
- Dai D., Gu D., Xia M. et al. Melt spreading behavior, microstructure evolution and wear resistance of selective laser melting additive manufactured AlN/AlSi10Mg nanocomposite. Surface and Coatings Technology, 2018, vol. 349, pp. 279−288. DOI: 10.1016/j.surfcoat.2018.05.072.
- Light Metal Alloys Application. Еd. Mandredi W.А. Croatia: InTech, 2014, 252 p. DOI: 10.5772/57069.
- Canali R. Study, development and characterization of aluminum based materials by additive manufacturing: PhD thesis. Turin: Politecnico di Torino, 2015, 116 p. DOI: 10.6092/polito/porto/2598770.
- Zhitnyuk S.V., Medvedev P.N. Investigation of microstructure and phase composition of the metallic composite material Al–Si–Mg system modified by silicon carbide particles by mechanical alloying. Part 1. Trudy VIAM, 2023, no. 1 (119), paper no. 08. Available at: http://www.viam-works.ru (accessed: August 16, 2023). DOI: 10.18577/2307-6046-2023-0-1-97-106.
- Zhitnyuk S.V., Medvedev P.N. Investigation of microstructure and phase composition of the metallic composite material Al–Si–Mg system modified by silicon carbide particles by mechanical alloying. Part 2. Trudy VIAM, 2023, no. 1 (119), paper no. 09. Available at: http://www.viam-works.ru (accessed: August 16, 2023). DOI: 10.18577/2307-6046-2023-0-1-107-118.