Serov M.M., Bezophen S.Ya., Patrushev A.Yu., Dvoretskov R.M., Elyutin E.S. Production of microcrystalline alloy particles of the system Co(Ni, Fe)–Ti–B–C by high-speed solidigication of the melt // Proceedings of VIAM. 2023. No. 10 (128). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2023-0-10-52-63.

Production of microcrystalline alloy particles of the system Co(Ni, Fe)–Ti–B–C by high-speed solidigication of the melt

Serov M.M., Bezophen S.Ya., Patrushev A.Yu., Dvoretskov R.M., Elyutin E.S.
Abstract

Using the method of high-speed solidification of a hanging drop of a melt, discrete of the Ме–3TiC–2B4C, where Me is a metal Co, Ni or Fe. The microstructure of the alloy was studied, and mechanical properties of discrete fibers were obtained. To assess the effect of high-speed solidification of the melt on the properties of the alloys, cast samples were made without quenching. It was shown that the cobalt – based alloy in the initial state after quenching contains a metastable phase whit a face-centered cubic lattice, the proportion of which is 58 %. In addition, cobalt-based fibers contain metastable disperse intermetallic compounds of Co2B and Co3B.

Keywords
microcrystalline, cobalt boride, cobalt carbide, instrumental materials
Reference list
  1. Zhao J., He J., Zhi Qing H., Lorenz R. Microstructure evolution in immiscible alloys during rapid directional solidification. Zeitschrift fur metallkunde, 2004, vol. 95, pp. 362–368. DOI: 10.3139/146.017967.
  2. Dvoretskaya E.V., Korolev D.V., Piskorskii V.P., Valeev R.A., Koplak O.V., Morgunov R.B. Magnetron sputtering of the iron shell and microinclusions in microwires PrDyFeCoB. Aviation materials and technologies, 2022, no. 2 (67), paper no. 08. Available at: http://www.journal.viam.ru (accessed: April 08, 2023). DOI: 10.18577/2713-0193-2022-0-2-85-96.
  3. Vershinin G.A., Panova T.V. Distribution analysis of impurity atoms in binary systems after high-speed solidification of the melt. International research journal, 2015, no. 8 (39). Available at: https://research-journal.org/archive/8-39-2015-september/ (accessed: April 08, 2023).
  4. Stasiak T., Oleszak D., Fraczkiewicz A. Effects of solidification condition on microstructure and properties of high-entropy alloys from the CoCrFeMnNi family. JOM, 2022, vol. 74, pp. 4842–482. DOI: 10.1007/s11837-022-05543-2.
  5. Korolev D.V., Valeev R.A., Morgunov R.B., Piskorsky V.P. Calculation of the temperature dependence of the magnetization of sintered materials Pr–Dy–Fe–Co–B using molecular field approximation theory. Trudy VIAM, 2023, no. 2 (120), paper no. 4. Available at: http://www.viam-works.ru (accessed: April 08, 2023). DOI: 10.18577/2307-6046-2023-0-2-42-52.
  6. Tamizifar H., Hadian A.M., Tamizifar M. The comparison between boron carbide (B4C) with other common inhibitors on physical and mechanical properties of WC/Co. International Journal of Modern Physics: Conference Series, 2012, vol. 5, pp. 102–110. DOI: 10.1142/S2010194512001900.
  7. Davies I.J., Nozue A., Nakabayashi S., Okubo T. Fracture behaviour of boride-dispresed composites fabricated by hot-pressing amorphous Ni60Mo30B10 powder. Journal of materials science, 1998, vol. 33 (19), pp. 4727–4732. DOI: 10.1023/A:1004441205253.
  8. Perez N.L., Place T.A. X-ray diffraction of a heat-treated rapidly solidified Ni35Mo35Fe9B2 alloy. Journal of materials science letters, 1990, vol. 9, pp. 940–942.
  9. Kablov E.N., Lukina E.A., Zavodov A.V., Efimochkin I.Yu. The formation of structure in ultrafine WC–Cо carbide material in the presence of inhibitory additives. Trudy VIAM, 2020, no. 4–5 (88), paper no. 10. Available at: http://www.viam-works.ru (accessed: April 08, 2023). DOI: 10.18577/2307-6046-2020-0-45-89-99.
  10. Mégret A., Vitry V., Delaunois F. The effect of boron-doped cobalt additions on mechanical properties of a recycled WC–Co powder. International Journal of Refractory Metals and Hard Materials, 2023, vol. 111, art. 106098. DOI: 10.1016/j.ijrmhm.2022.106098.
  11. Serov M.M., Betsofen S.Ya., Patrushev A.Yu., Ashmarin A.A., Gordeeva M.I. Influence of high-speed solidification of the melt on the structural characteristics of the Co–6TiC alloy. Deforma-tsiya i razrusheniye materialov, 2022, no. 11, art. 01. DOI: 10.31044/1814-4632-2022-11-2-9.
  12. Farafonov D.P., Migunov V.P., Degovec M.L., Aleshina R.Sh. Porous-fibrous metallic material for sound-absorbing structures of aircraft GTE. Trudy VIAM, 2016, no. 4 (40), paper no. 01. Available at: http://www.viam-works.ru (accessed: April 08, 2023). DOI: 10.18577/2307-6046-2016-0-4-1-1.
  13. Farafonov D.P., Serov M.M., Patrushev A.Yu., Leshchev N.E., Yaroshenko A.S. Metal fibers for new aircraft engine materials. Trudy VIAM, 2020, no. 12 (94), paper no. 03. Available at: http://www.viam-works.ru (accessed: April 08, 2023). DOI: 10.18577/2307-6046-2020-0-12-23-34.
  14. Miroshnichenko I.S., Sergeev G.A., Galushko I.M. Metastable diagrams in nickel–carbon and cobalt–carbon systems. Izvestiya vuzov. Chernaya metallurgiya, 1964, no. 1, pp. 164–166.
  15. Lyakishev N.P. State diagrams of double metallic systems: reference book in 3 vols: Moscow: Mashinostroenie, 1996, vol. 1, 992 p.
  16. Panov V.S., Chuvilin A.M., Technology and properties of sintered hard alloys and products made from them: a textbook for univ. Moscow: MISIS, 2011, 428 p.
  17. Isaev B.A., Burkhanov A.R. Study of the structure of U8A steel after electromechanical treatment. Zapiski Gornogo instituta, 2018, vol. 233, pp. 518–524. DOI: 10.31897/PMI.2018.5.518.
  18. Druchinina O.A., Vershinin D.S., Smolyakova M.Yu. Using an automatic microhardness analysis system to assess the depth of the nitrided layer on R6M5 steel. Vestnik TSU, 2010, vol. 15, is. 3, pp. 1194–1197.
  19. Guryev A.M. Improving the performance characteristics of sintered ceramic W–Co materials by simultaneous diffusion saturation with boron, chromium and titanium. International Journal of Applied and Fundamental Research, 2018, no. 10, pp. 16–21. DOI: 10.17513/mjpfi.12409.