Zhitnyuk S.V., Medvedev P.N., Sorokin O.Ju., Kachaev A.A. Formation of crystallographic texture in polycryctalline ceramics as a way to enhance properties (review) // Proceedings of VIAM. 2022. No. 5 (111). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-5-74-86.
Formation of crystallographic texture in polycryctalline ceramics as a way to enhance properties (review)
Abstract
Considers the main achievements in the field of obtaining ceramic materials with a predominant crystallographic orientation of grains. It is shown that ceramics, which is characterized by the presence of a crystallographic texture, has increased properties in specific directions in comparison with non-textural materials. The development of fundamental research aimed at identifying the processes of texture formation contributes to the obtaining of ceramics with adjustable properties, which are in demand in many areas of industry
Keywords
crystallographic texture, ceramics, diffraction research methods, microstructure, property determination
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Buznik V.M., Kablov E.N. State and prospects of Arctic materials science. Vestnik RAN, 2017, vol. 87, no. 9, pp. 827–839.
- Kablov E.N. Dominant of the national technology initiative. Problems of accelerating the development of additive technologies in Russia. Metally of Evrazii, 2017, no. 3, pp. 2–6.
- Lavrov A.V., Yakovlev N.O., Erasov V.S. Destruction of ceramic materials under the influence of high-speed indenter. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 88–94. DOI: 10.18577/2071-9140-2018-0-2-88-94.
- Loshchinin Yu.V., Budinovskiy S.A., Razmakhov M.G. Heat conductivity of heat-protective coatings ZrO2–Y2O3 alloyed by REM oxides obtained by magnetronny application. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 42–49. DOI: 10.18577/2071-9140-2018-0-3-42-49.
- Voronov Vs.A., Lebedeva Yu.E., Sorokin O.Yu., Vaganova M.L. Investigation of the high-temperature coatings properties on the basis of an yttrium-alumosilicate system for the protection of SiC materials from the action of an oxidizing environment. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 63–73. DOI: 10.18577/2071-9140-2018-0-4-63-73.
- Babashov V.G., Maksimov V.G., Varrik N.M., Samorodova O.N. Studying of structure and pro-perties of samples of ceramic composite materials on the basis of mullite. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 54–63. DOI: 10.8577/2071-9140-2020-0-1-54-63.
- Messing G.L., Poterala S., Chang Y. et al. Texture-engineered ceramics – Property enhancements through crystallographic tailoring. Journal of Material Research, 2017, vol. 32, pp. 3219–3241.
- Seabaugh M.M., Kerscht I.H., Messing G.L. Texture development by templated grain growth in liquid-phase-sintered α-alumina. Journal of the American Ceramic Society, 1997, no. 80, pp. 1181–1188.
- Tani T. Texture engineering of electronic ceramics by the reactive-templated grain growth method. Journal of the Ceramic Society of Japan, 2006, no. 114, pp. 363–370.
- Yilmaz H., Messing G.L., Trolier-McKinstry S. (Reactive) templated grain growth of textured sodium bismuth titanate (Na1/2Bi1/2TiO3–BaTiO3) ceramics processing. Journal of Electroceramics, 2003, no. 11, pp. 207–215.
- Jin S., Sherwood R.C. et al. High TC superconductors-composite wire fabrication. Applied Physics Letters, 1987, no. 51, pp. 203–204.
- Goyal A., Feenstra R., List F.A. et al. Using RABiTS to fabricate high-temperature superconducting wire. The Journal of The Minerals, Metals & Materials Society, 1999, no. 51, pp. 19–23.
- Sakka Y., Suzuki T.S. Textured development of feeble magnetic ceramics by colloidal processing under high magnetic field. Journal of the Ceramic Society of Japan, 2005, vol. 113, pp. 26–36.
- Messing G.L., Trolier-McKinstry T., Sabolsky E.M. et al. Templated grain growth of textured piezoelectric ceramics. Critical Reviews in Solid State and Material Sciences, 2004, no. 29, pp. 45–96.
- Kabirova D.B. Evolution of the microstructure and texture upon annealing and deformation of superconducting YBa2Cu3O7–x ceramics: thesis, Cand. Sc. (Phys. & Math.). Ufa: Institute for Problems of Superplasticity of Metals of the Russian Academy of Sciences, 2020, 190 p.
- Lotgering F.K.J. Topotactical reactions with ferromagnetic oxides having hexagonal crystal structures. Journal of Inorganic and Nuclear Chemistry, 1959, no. 9, pp. 113–123.
- Kingery W.D. Introduction to ceramics: trans. from Engl. Moscow: Stroyizdat, 1967, 499 p.
- Stuijts A.L., Rathenau G.W., Weber G.H. Ferroxdure II and III, anisotropic permanent magnet materials. Philips Technical Review, 1954, vol. 16, no. 5–6, pp. 141–180.
- Chen Y., Daigle A., Fitchorov T. et al. Electronic tuning of magnetic permeability in Co2Z hexaferrite toward high frequency electromagnetic device miniaturization. Applied Physics Letters, 2011, no. 98, art. 202502.
- Jian G., Meng F., Zhou D. et al. Fabrication of textured CoFe2O4 ceramics by novel RTGG method using rod-like α-FeOOH particles as templates. Materials Chemistry and Physics, 2015, vol. 162, pp. 380–385.
- Chang P., He L., Wei D. et al. Textured Z-type hexaferrite Ba3Co2Fe24O41 ceramics with high permeability by reactive template grain growth method. Journal of European Ceramic Society, 2016, vol. 36, pp. 2519–2524.
- Desgardin G., Monot I., Raveau B. Texturing of high–TC superconductors. Superconductors science and technology, 1999, vol. 12, no. 7, pp. 115–133.
- Susner M.A., Daniels T.W., Sumption M.D. et al. Drawing induced texture and the evolution of superconductive properties with heat treatment in powder-in-tube in situ MgB2 strands. Superconductors science and technology, 2012, vol. 25, art. 065002.
- Shi Y., Durrell J.H., Dennis A.R. et al. Multiple seeding for the growth of bulk GdBCO–Ag superconductors with single grain behavior. Superconductors science and technology, 2017, vol. 30, art. 015003.
- Miwa Y., Kawada S., Kimura M. et al. Processing and enhanced piezoelectric properties of highly oriented compositionally modified Pb(Zr, Ti)O3 ceramics fabricated by magnetic alignment. Applied Physics Express, 2015, no. 8, art. 041501.
- Yan Y., Wang Y.U., Priya S. Electromechanical behavior of [001]-textured Pb(Mg1/3Nb2/3)O3–PbTiO3 ceramics. Applied Physics Letters, 2012, vol. 100, art. 192905.
- Chang Y., Wu J., Sun Y. et al. Enhanced electromechanical properties and phase transition temperatures in [001]-textured Pb(In1/2Nb1/2)O3–Pb(Mg1/3Nb2/3)O3–PbTiO3 ternary ceramics. Applied Physics Letters, 2015, vol. 107, art. 082902.
- Yan Y., Zhou J.E., Maurya D. et al. Giant piezoelectric voltage coefficient in grain-oriented modified PbTiO3 material. Nature Communications, 2016, no. 7, art. 13089.
- Yan Y., Cho K., Maurya D. et al. Giant energy density in [001]-textured Pb(Mg1/3Nb2/3)O3–PbZrO3–PbTiO3 piezoelectric ceramics. Applied Physics Letters, 2013, vol. 102, art. 042903.
- Wei D., Yuan Q., Zhang G. et al. Templated grain growth and piezoelectric properties of 001>-textured PIN–PMN–PT ceramics. Journal of Material Research, 2015, vol. 30, no. 14, pp. 2144–2150.
- Yan Y., Priya S. Strong piezoelectric anisotropy d15/d33 in 111> textured Pb(Mg1/3Nb2/3)O3–Pb(Zr,Ti)O3 ceramics. Applied Physics Letters, 2015, vol. 107, art. 082909.
- Haugen A.B., Henning G., Madaro F. et al. Piezoelectric K0,5Na0,5NbO3 ceramics textured using needlelike K0,5Na0,5NbO3 templates. Journal of the American Ceramic Society, 2014, vol. 97, pp. 3818–3825.
- Hussain A., Kim J.S., Song T.K. et al. Fabrication of textured KNNT ceramics by reactive template grain growth using NN templates. Current Applied Physics, 2013, vol. 13, pp. 1055–1059.
- Li Y., Hui C., Wu M. et al. Textured (K0,5Na0,5)NbO3 ceramics prepared by screen-printing multilayer grain growth technique. Ceramics International, 2012, vol. 38, pp. 283–286.
- Zhang H., Xu P., Patterson E. et al. Preparation and enhanced electrical properties of grain–oriented (Bi1/2Na1/2)TiO3–based lead–free incipient piezoceramics. Journal of the European Ceramic Society, 2015, vol. 35, pp. 2501–2512.
- Maurya D., Zhou Y., Yan Y. et al. Synthesis mechanism of grain-oriented lead-free piezoelectric Na0,5Bi0,5TiO3–BaTiO3 ceramics with giant piezoelectric response. Journal of Materials Chemistry C, 2013, no. 1, pp. 2102–2111.
- Bai W., Hao J., Fu F. et al. Structure and strain behavior of 001> textured BNT-based ceramics by template grain growth. Materials Letters, 2013, vol. 97, pp. 137–140.
- Ma S., Zhang Y., Liu Z. et al. Preparation and enhanced electric-field-induced strain of textured 91BNT–6BT–3KNN lead-free piezoceramics by TGG method. Journal of Materials Science: Materials in Electronics, 2016, vol. 27, pp. 3076–3081.
- Deng M., Li X., Zhao Z. et al. Crystallographic textured evolution in 0,85Na0,5Bi0,5TiO3–0,04BaTiO3–0,11K0,5Bi0,5TiO3 ceramics prepared by reactive-templated grain growth method. Journal of Materials Science: Materials in Electronics, 2014, vol. 25, pp. 1873–1879.
- Zou H., Sui Y., Zhu X. et al. Texture development and enhanced electromechanical properties in 001>-textured BNT-based materials. Materials Letters, 2016, vol. 184, pp. 139–142.
- Maurya D., Zhou Y., Wang Y. et al. Giant strain with ultralow hysteresis and high temperature stability in grain oriented lead-free K0,5Bi0,5TiO3–BaTiO3–Na0,5Bi0,5TiO3 piezoelectric materials. Scientific Reports, 2015, no. 5, art. 8595.
- Hu D., Mori K., Kong X. et al. Fabrication of [100]-oriented bismuth sodium titanate ceramics with small grain size and high density for piezoelectric materials. Journal of the European Ceramic Society, 2014, vol. 34, pp. 1169–1180.
- Vriami D., Damjanovic D., Vleugels J. et al. Textured BaTiO3 by templated grain growth and electrophoretic deposition. Journal of Materials Science, 2015, vol. 50, pp. 7896–7907.
- Fu F., Shen B., Xu Z. et al. Electric properties of BaTiO3 lead-free textured piezoelectric thick film by screen printing method. Journal of Electroceramics, 2014, vol. 33, pp. 208–213.
- Chemical technology of ceramics. Ed. I.Ya. Guzman. Moscow: Stroymaterialy, 2003, 496 p.
- Suzuki T.S., Sakka Y. Preparation of oriented bulk 5 wt. % Y2O3–AlN ceramics by slip casting in a high magnetic field and sintering. Scripta Materialia, 2005, vol. 52, pp. 583–586.
- Zhu X.W., Sakka Y., Zhou Y. et al. A strategy for fabricating textured silicon nitride with enhanced thermal conductivity. Journal of the European Ceramic Society, 2014, vol. 34, pp. 2585–2589.
- Nikova M.S. Synthesis and study of oxide compositions with a garnet structure in the Y2O3–Yb2O3–Sc2O3–Al2O3 system for optical ceramics: thesis, Cand. Sc. (Cand.). Stavropol: North Caucasian Federal University, 2020, 175 p.
- Liu P., Yi H., Zhou G. et al. HIP and pressureless sintering of transparent alumina shaped by magnetic field assisted slip casting. Optical Materials Express, 2015, vol. 5, pp. 441–446.
- Pringuet A., Takahashi T., Baba S. et al. Fabrication of transparent grain-oriented polycrystalline alumina by colloidal processing. Journal of the American Ceramic Society, 2016, vol. 99, pp. 3217–3219.
- Tanaka S., Takahashi T., Uematsu K. Fabrication of transparent crystal-oriented polycrystalline strontium barium niobate ceramics for electro-optical application. Journal of the European Ceramic Society, 2014, vol. 34, pp. 3723–3728.
- Sato Y., Arzakantsyan M., Akiyama J. et al. Anisotropic Yb:FAP laser ceramics by micro-domain control. Optical Materials Express, 2014, vol. 4, pp. 2006–2015.
- Akiyama J., Sato Y., Taira T. Laser demonstration of diod-pumped Nd3+-doped fluorapatite anisotropic ceramics. Applied Physics Express, 2011, vol. 4, art. 022703.
- Lee S., Lee Y., Kim Y. et al. Mechanical properties of hot-forged silicon carbide ceramics. Scripta Materialia, 2005, vol. 52, pp. 153–156.
- Nakamura M., Hirao K., Yamauchi Y. et al. Tribological properties of unidirectionally aligned silicon nitride. Journal of the American Ceramic Society, 2001, vol. 84, pp. 2579–2584.
- Zhang H.B., Hu C.F., Sato K. et al. Tailoring Ti3AlC2 ceramic with high anisotropic physical and mechanical properties. Journal of the European Ceramic Society, 2015, vol. 35, pp. 393–397.
- Medvedev P.N., Muboyadzhyan S.A. X-ray diffraction studies of electron beam ceramic thermal barrier coating layer based on ZrO2·Y2O3. Trudy VIAM, 2017, no. 1 (49), paper no. 03. Available at: http://www.viam-works.ru (accessed: December 16, 2021). DOI: 10.18577/2307-6046-2017-0-1-3-3.
- Lee S., Dursun S., Duran C. et al. Thermoelectric power factor enhancement of textured ferroelectric SrxBa1–xNb2O6–δ ceramics. Journal of Materials Research, 2011, vol. 26, pp. 26–30.
- Fukuda K., Okabe M., Asaka T. Microtexture of c-axis-oriented polycrystalline lanthanum silicate oxyapatite formed by reactive diffusion. Journal of the American Ceramic Society, 2016, vol. 99, pp. 2816–2822.