Buzenkov A.V., Valeev R.A., Piskorsky V.P., Morgunov R.B. The effect of the content of yttrium on the properties of the sintered magnets Nd–Dy–Y–Fe–Co–B // Proceedings of VIAM. 2022. No. 4 (110). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-4-108-117.

The effect of the content of yttrium on the properties of the sintered magnets Nd–Dy–Y–Fe–Co–B

Buzenkov A.V., Valeev R.A., Piskorsky V.P., Morgunov R.B.
Abstract

Was investigated by the effect of using yttrium on the properties of the sintered Magnets Nd–Dy–Y–Fe–Co–B. It is shown that the coercive force on the magnetization and induction is decreased with an increase in the content of yttrium. The magnitude of the rectangulation of the clarification curve slightly increases. The value of residual induction and the magnetization of saturation changes not significantly, but tend to increase with the content of yttria. Thus yttrium is not desirable impurity in thermostable magnets for navigation instruments.

Keywords
permanent magnets, rare earth magnets, magnetization migration curve, induction curve by induction, rectangle of demagnetization curve, yttrium
Reference list
  1. Chirkin D.S., Roslovets P.V., Tatarinov F.V., Novikov L.Z. Reducing the drift of a dynamically tuned gyroscope from run to run. Engineering Journal: Science and Innovations, 2017, no. 1 (61), art. 08. DOI: 10.18698/2308-6033-2017-01-1579.
  2. Xinyuan T., Podchezertsev V.P. Algorithms for certification of a dynamically tuned gyroscope in conditions of real orientation relative to the geographic coordinate system. Engineering Journal: Science and Innovations, 2017, no. 10 (70), art. 14. DOI: 10.18698/2308-6033-2017-10-1691.
  3. Dynamically adjustable gyroscope: pat. RU 2687169 C1; filed 17.04.18; publ. 07.05.19.
  4. Kablov E.N., Piskorskiy V.P., Burkhanov G.S., Valeyev R.A., Moiseyeva N.S., Stepanova S.V., Petrakov A.F., Tereshina I.S., Repina M.V. Thermostable ring magnets with radial texture based on Nd(Pr)–Dy–Fe–Co–B. Fizika i khimiya obrabotki materialov, 2012, no. 3, pp. 43–47
  5. Piskorsky V.P., Valeev R.A., Korolev D.V., Morgunov R.B., Rezchikova I.I. Terbium and gadolinium dopin g influence on thermal stability and magnetic properties of sintered magnets Pr–Tb–Gd–Fe–Co–B. Trudy VIAM, 2019, no. 7 (79), paper no. 07. Available at: http://www.viam-works.ru (accessed: October 15, 2021). DOI: 10.18577/2307-6046-2019-0-7-59-66.
  6. Morgunov R.B., Piskorskiy V.P., Valeev R.A., Korolev D.V. The thermal stability of rare-earth magnets supported by means of the magnetocaloric effect. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 88–94. DOI: 10.18577/2071-9140-2019-0-1-88-94.
  7. Min P.G., Vadeev V.E., Piskorskiy V.P., Kramer V.V. Development of melting technology of high pure REM–Fe–Co–B alloys for temperature-stable magnets. Trudy VIAM, 2016, no. 1 (37), paper no. 1 Available at: http://www.viam-works.ru (accessed: October 15, 2021). DOI: 10.18557/2307-6046-2016-0-1-1-1.
  8. Korolev D.V., Stolyankov Yu.V., Piskorsky V.P., Valeev R.A., Bahmetiev M.V., Dvorezkaya E.V., Koplak O.V., Morgunov R.B. Magnetic properties and magnetic strip domains in micro stripes PrDyFeCoB. Aviation materials and technologies, 2021, no. 3 (64), paper no. 08. Available at: http://www.journal.viam.ru (accessed: October 15, 2021). DOI: 10.18577/2713-0193-2021-0-3-86-93.
  9. Herbst J.F. R2Fe14B materials: intrinsic properties and technological properties and technological aspects. Reviews of Modern Physics, 1991, vol. 63, no. 4, pp. 819–898.
  10. Martynenko Yu.G. Trends in the development of modern gyroscopy. Soros Educational Journal, 1997, no. 11, pp. 120–127.
  11. Blazhnov B., Nesenyuk L., Peshekhonov V., Staroseltsev L. Miniature integrated systems. Electronics: Science, Technology, Business, 2001, no. 5, pp. 56–59.
  12. Korolev M.N. Study of the technical characteristics of modern types of angular velocity sensors. Abstracts of the 12th Intern. sci.-tech. conf. "Instrument making-2019". Moscow, 2019, pp. 21–23.
  13. Golovanov V.A. Gyroscopic orientation. St. Petersburg: St. Petersburg State Mining Institute, 2004. 92 p.
  14. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  15. Determination of the density of bodies by hydrostatic weighing: recommendations. Irkutsk: Irkutsk. state un-t, 2003, pp. 1–9.
  16. Lapteva K.A., Tolmachev I.I. Calculation of the demagnetizing factor during longitudinal magnetization in magnetic particle flaw detection. Izvestiya Tomskogo politekhnicheskogo universiteta, 2012, vol. 321, no. 2, pp. 140–144.
  17. Sato M., Ishii Y. Simple and approximate expressions of demagnetizing factors of uniformly magnetized rectangular rod and cylinder. Journal of Applied Physics, 1989, vol. 66, no. 2, pp. 983–985.
  18. Chen Du-Xing, Brug J.A., Goldfarb R.B. Demagnetizing factor for cylinder. IEEE Transactions on Magnetics, 1991, vol. 27, no. 4, pp. 3601–3619.
  19. Faria R.N., Takiishi H., Lima L.F.C.P., Costa I. Praseodymium-based HD-sintered magnets produced using a mixture of cast alloys. Journal of Magnetism and Magnetic Materials, 2001, vol. 237, pp. 261–266.
  20. Périgo E.A., Takiishi H., Motta C.C., Faria R.N. On the squareness factor behavior of RE–FeB (RE = Nd or Pr) magnets above room temperature. IEEE Transactions on Magnetics, 2009, vol. 45, no. 10, pp. 4431–4434.
  21. Angelo J.D., Motta C.C., Barbosa L.P. et al. The effect of niobium and boron content on magnetic properties and corrosion resistance of Pr–Fe–Co–B–Nb HD magnets. Material Science Forum, 2008, vol. 591–593, pp. 96–101.
  22. Corfield M.R., Williams A.J., Harris I.R. The effects of long term annealing at 10008C for 24 h on the microstructure and magnetic properties of Pr–Fe–B/Nd–Fe–B magnets based on Nd16Fe76 B8 and Pr16Fe76B8. Journal of Alloys and Compounds, 2000, vol. 296, pp. 138–147
  23. Zhang Y., Ma T., Jin J. et al. Effect of REFe2 on microstructure and magnetic properties of Nd–Ce–Fe–B sintered magnets. Acta Materialia, 2017, vol. 128, pp. 22–30.
  24. Sinnema S., Franse J.J.M., Radwanski R.J. et al. Magnetic measurements on R2Fe14B and R2Co14B compounds in high fields. Journal de Physique, 1985, vol. 46, pp. C6-301–C6-304.
  25. Kakol Z., Kapusta C., Figiel H. The Nd contribution to the magnetocrystalline anisotropy of (Y1–xNdx)2Co14B compounds. Journal of Magnetism and Magnetic Materials, 1988, vol. 75, pp. 141–148.