Butakov V.V., Lugovoy A.A., Varrik N.M., Babashov V.G. Simulation of the propagation of a heat front through a sample of a multilayer thermal insulation material under conditions of non-stationary heat flow // Proceedings of VIAM. 2022. No. 10 (116). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-10-128-139.

Simulation of the propagation of a heat front through a sample of a multilayer thermal insulation material under conditions of non-stationary heat flow

Butakov V.V., Lugovoy A.A., Varrik N.M., Babashov V.G.
Abstract

An urgent task for developers of heat-protective materials is to create methods for a comprehensive assessment of the complex of their key properties that reliably ensure their operation under operating conditions. The purpose of this study is to evaluate the properties of a layered heat-shielding material sufficient to simulate the propagation of a heat front through a sample under conditions of non-stationary heat flow. Work has been carried out to evaluate a set of thermophysical properties of the material sufficient to construct a model of the propagation of a thermal front through a sample under unilateral heating. A model of the passage of the heat front through the material has been created. The work on the numerical evaluation of the thermal conductivity coefficient and the heat transfer coefficient on the front sides of the multilayer sample was carried out.

Keywords
thermal insulation material, thermal conductivity coefficient, heat flux, multilayer multicomponent heat protection systems
Reference list
  1. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  2. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  3. Krainov A.Yu. Fundamentals of heat transfer. Heat transfer through a layer of matter: textbook. Tomsk: STT, 2016, 48 p.
  4. Baikov V.I., Pavlyukevich N.V. Thermophysics: in 2 vols. Minsk: Institute of Heat and Mass Transfer named after A.V. Lykov NAS of Belarus, 2013. Vol. 1: Thermodynamics, statistical physics, physical kinetics, 400 p.
  5. Korotkikh A.G. Thermal conductivity of materials: textbook. Tomsk: Tomsk Polytech. University, 2011, 97 p.
  6. Tomak V.I., Burkov A.S., Rytsarev A.M., Tovstonog V.A. Experimental assessment of the thermophysical characteristics of high-temperature heat-insulating materials. Vestnik MGTU im. N.E. Baumana. Ser.: Natural sciences, 2020, no. 2, pp. 99–116. DOI: 10.18698/1812-3368-2020-2-99-116.
  7. Barinov D.Ya., Marakhovskij P.S., Zuev A.V. Mathematical modeling of destruction of fiberglass-based thermal-protection material. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 71–78. DOI: 10.18577/2071-9140-2020-0-4-71-78.
  8. Barbotko S.L., Volny O.S., Kirienko O.A., Shurkova E.N. Evaluation of fire safety of polymeric materials for aviation purposes. Ed. E.N. Kablov. M.: VIAM, 2018, 408 p.
  9. Barbotko S.L., Volnyy O.S., Kiriyenko O.A., Shurkova E.N. Creation of the mathematical model and calculation of sample temperatures at tests on fire resistance. Trudy VIAM, 2017, no. 7 (55), paper no. 12. Available at: http://www.viam-works.ru (accessed: June 7, 2022). DOI: 10.18577/2307-6046-2017-0-7-12-12.
  10. Vorobev N.N., Barinov D.Ya., Zuev A.V., Pakhomkin S.I. Computational and experimental study of the effective thermal conductivity of fibrous materials. Trudy VIAM, 2021, no. 7 (101), paper no. 10. Available at: http://www.viam-works.ru (accessed: June 07, 2022). DOI: 10.18577/2307-6046-2021-0-7-95-102.
  11. Barinov D.Ya., Prosuntsov P.V. Modeling of heat transfer in the layer of decomposing material of the heat-shielding coating of the descent vehicle. Vestnik MGTU im. N.E. Baumana. Ser.: Mechanical engineering, 2016, no. 6, pp. 22–32. DOI: 10.18698/0236-3941-2016-6-22-32.
  12. Belskikh G.N., Maiorov A.V. Development of highly efficient composite heat-shielding materials. Innovatsii, 2014, no. 9 (191), pp. 118–120.
  13. Aristova Е.Yu., Denisova V.А., Drozhzhin V.S. et al. Composite materials using hollow microspheres. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 52–57. DOI: 10.18577/2071-9140-2018-0-1-52-57.
  14. Flexible heat and sound insulating fibrous material of low density: pat. 2641495 Rus. Federation, no. 2016142842; filed 01.11.16; publ. 17.01.18.
  15. Fire-resistant layered sound and heat insulating material: pat. 2465145 Rus. Federation, no. 2011118705/05; filed11.05.11; publ. 27.10.12.
  16. Heat Insulation System: pat. 5246759 USA, no. 702269; filed 17.05.91; publ. 21.09.93.
  17. Lugovoy A.A., Babashov V.G., Karpov Yu.V. The thermal diffusivity of the gradientthermal insulation material. Trudy VIAM, 2014, no. 2, paper no. 02. Available at: http://viam-works.ru (accessed: March 2, 2022). DOI: 10.18577/2307-6046-2014-0-2-2-2.
  18. Stand for the qualitative assessment of heat-insulating materials: pat. 156904 Rus. Federation, no. 2014138916; заявл. 25.09.14; опубл. 20.11.15.
  19. Butakov V.V., Lugovoy A.A., Varrik N.M., Babashov V.G. Assessment of thermal conductivity of a layered highly porous thermal insulation material. Aviation materials and technologies, 2022, no. 1 (66), paper no. 11. Available at: http://www.journal.viam.ru (accessed: July 1, 2022). DOI: 10.18577/2713-0193-2022-0-1-129-142.
  20. Butakov V.V., Shavnev A.A., Lugovoy A.A., Varrik N.M., Babashov V.G. An approach to the construction of a mathematical model of the passage of a heat front through a sample of a heat-shielding material under conditions of an unsteady heat flow. Trudy VIAM, 2022, no. 6 (112), paper no. 11. Available at: http://www.viam-works.ru (accessed: July 1, 2022). DOI: 10.18577/2307-6046-2002-0-6-127-137.