Sidorina A.I., Safronov A.M. Development of carbon fabrics with high surface density manufacturing technologies // Proceedings of VIAM. 2020. No. 6-7 (89). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-67-72-80.

Development of carbon fabrics with high surface density manufacturing technologies

Sidorina A.I., Safronov A.M.
Abstract

The article describes features of development of carbon fabrics with high surface density manufacturing technologies for applying as reinforcing fillers at manufacturing of constructional polymeric composite materials and for manufacturing of composite equipment. The technical calculation of carbon fabrics and the construction of a filling pattern depending on the requirements for the developed carbon fabrics are shown. Results of determination of properties of the carbon fabrics received on established filling parameters and technological modes of manufacturing are presented.

Keywords
carbon fabrics, carbon fibers, reinforcing fillers, polymeric composite material, prepreg, carbon plastic, composite equipment, forming equipment.
Reference list
  1. Perepelkin E.E. Reinforcing fibers and fibrous polymer composites. St. Petersburg: Nauchnye osnovy i tekhnologii, 2009, 360 p.
  2. Sidorina A.I., Gunyaeva A.G. Market of carbon fibers and composites based on them. Review. Khimicheskiye volokna, 2016, no. 4, pp. 48–53.
  3. Kablov E.N. New generation materials – the basis for innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  4. Timoshkov P.N. Equipment and materials for the technology of automated calculations prepregs. Aviacionnye materialy i tehnologii, 2016, no. 2, pp. 35–39. DOI: 10.18577/2071-9140-2016-0-2-35-39.
  5. Muhametov R.R., Petrova A.P., Ponomarenko S.A., Ahmadieva K.R., Pavlyuk B.F. Influence of woven fibrous fillers of various types on properties of cured binder VS-2526K). Trudy VIAM, 2018, no. 3 (63), paper no. 04. Available at: http//www.viam-works.ru (accessed: February 26, 2020). DOI: 10.18577/2307-6046-2018-0-3-28-36.
  6. Kutsevich K.E., Tyumeneva T.Yu., Petrova A.P. Influence of fillers on properties of adhesive prepregs and PCM on their basis. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 51–55. DOI: 10.18577/2071-9140-2017-0-4-51-55.
  7. Sidorina A.I., Gunyaeva A.G. Woven reinforcing fillers for polymer composites. Review. Khimicheskiye volokna, 2017, no. 2, pp. 20–23.
  8. Zhidkova O.G., Kashtanov P.P., Tumanin A.N. Features of the design of composite shaping equipment for the manufacture of high-precision dimensionally stable mirror composite antennas of integral design. Konstruktsii iz kompozitsionnykh materialov, 2019, no. 1, pp. 36–44.
  9. Gunyayeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
  10. Kablov E.N. Main results and directions of development of materials for advanced aviation technology. 75 years. Aviation materials. Moscow: VIAM, 2007, pp. 20–26.
  11. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  12. Design of technological process of weaving production: method. instructions for the implementation of course and diploma projects. Ed. G.S. Shipilova. Volgograd: Volgograd. state tech. Un-t, 2004, 43 p.
  13. Polyakova L.P. Technical calculations in weaving: textbook. St. Petersburg: SPGUTD, 2004, 57 p.
  14. Fomchenkova L.N. Modern equipment for weaving production in the domestic market. Tekstilnaya promyshlennost, 2010, no. 2, pp. 48–55.
  15. Terentyev V.I. Trends in the improvement of modern weaving machines. Tekstilnaya promyshlennost, 2010, no. 2, pp. 6–10.
  16. Kablov E.N. Marketing of materials science, aircraft construction and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5–6, pp. 40–44.