Antipov V.V., Medvedev I.M., Kutyrev A.E., Volkov I.A. Rapid assessment of hot water sealed anodic oxide coatings protective properties during NaCl immersion testing // Proceedings of VIAM. 2019. No. 8 (80). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-8-67-78.

Rapid assessment of hot water sealed anodic oxide coatings protective properties during NaCl immersion testing

Antipov V.V., Medvedev I.M., Kutyrev A.E., Volkov I.A.
Abstract

Multilayer systems based on anodizing and painting are used in the aircraft industry for aluminum alloys corrosion protection. Porous anodic oxide coatings with insufficient corrosion protection properties are formed during anodizing in chromium-free electrolytes. These coatings are sealed for better corrosion protection. Hot water sealing is one of the most widely used methods to enhance aluminum anodic oxide coatings protective properties. Lengthy neutral salt spray tests (usually at least 336 h) are used for protective properties assessment. In the present study, EIS data was fitted using equivalent electrical circuits for investigation of changes in coating parameters during 3% NaCl solution immersion up to 1440–3600 h. Coatings were obtained by 1163, V-1461, V96C3p.ch. aluminum alloys anodizing in sulfuric acid water solution for 15, 30, 45 minutes, followed by hot water sealing in deionized water. Changes in impedance modulus at low frequencies (so-called «degradation function») cannot be used to assess the protective properties of sealed anodic oxide coatings. The electrochemical criterion for quick evaluation of sealed anodic oxide coatings protective properties (time to first corrosion spots) was introduced – change in capacitive parameter of sealing CPEseal-T during the first 24 h of testing in NaCl solution.

Keywords
anodic oxide coatings, electrochemistry, EIS, aluminum alloys.
Reference list
  1. Hu N., Dong X., He X. et al. Effect of sealing on the morphology of anodized aluminum oxide // Corrosion Science. 2015. Vol. 97. P. 17–24. DOI: 10.1016/j.corsci.2015.03.021.
  2. López V., Bartolomé M.J., Escudero E. et al. Comparison by SEM, TEM, and EIS of Hydrothermally Sealed and Cold Sealed Aluminum Anodic Oxides // Journal of the Electrochemical Society. 2006. Vol. 153. No. 3. P. B75–B82. DOI: 10.1149/1.2163811.
  3. Hoar T.P., Wood G.C. The sealing of porous anodic oxide films on aluminium // Electrochimica Acta. 1962. Vol. 7. No. 3. P. 333–353. DOI: 10.1016/0013-4686(62)87009-1.
  4. Kablov E.N., Startsev O.V. Fundamentalnye i prikladnye issledovaniya korrozii i stareniya materialov v klimaticheskih usloviyah (obzor) [The basic and applied research in the field of corrosion and ageing of materials in natural environments (review)] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  5. Semenychev V.V., Smirnova T.B. Ocenka korrozionnoj stojkosti zashhitnyh i funkcionalnyh pokrytij s pomoshhyu izmeritelya skorosti korrozii [The evaluation of corrosion resistance of protective and functional coatings using corrosion-ratemeter] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №6. St. 12. Available at: http://www.viam-works.ru (accessed: July 29, 2016). DOI: 10.18577/2307-6046-2016-0-6-12-12.
  6. Whelan M., Cassidy J., Duffy B. Sol-gel sealing characteristics for corrosion resistance of anodised aluminium // Surface and Coatings Technology. 2013. Vol. 235. P. 86–96. DOI: 10.1016/j.surfcoat.2013.07.018.
  7. Whelan M., Barton K., Cassidy J. et al. Corrosion inhibitors for anodised aluminium // Surface and Coatings Technology. 2013. Vol. 227. P. 75–83. DOI: 10.1016/j.surfcoat.2013.02.029.
  8. Mansfeld F., Kendig M.W. Technical Note: Impedance Spectroscopy as Quality Control and Corrosion Test for Anodized Al Alloys // Corrosion. 1985. Vol. 41. No. 8. P. 490–492. DOI: 10.5006/1.3583832.
  9. Mansfeld F. Evaluation of Anodized Aluminum Surfaces with Electrochemical Impedance Spectroscopy // Journal of The Electrochemical Society. 1988. Vol. 135. No. 4. P. 828. DOI: 10.1149/1.2095786.
  10. Domingues L., Fernandes J.C.S., Da Cunha Belo M. et al. Anodising of Al 2024-T3 in a modified sulphuric acid/boric acid bath for aeronautical applications // Corrosion Science. 2003. Vol. 45. No. 1. P. 149–160. DOI: 10.1016/S0010-938X(02)00082-3.
  11. Antipov V.V., Medvedev I.M., Kutyrev A.E., Zhitnyuk S.V. Issledovaniye elektrokhimiche-skikh svoystv nenapolnennykh anodno-oksidnykh pokrytiy na alyuminiyevykh splavakh marok 1163, V-1461 i V96TS3p.ch. pri uskorennykh ispytaniyakh [The investigation of electrochemical properties of non-sealed oxide coatings on 1163, v-1461, v96с3pch aluminum alloys during accelerated testing] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2019. №6 (78). St. 06. Available at: http://www.viam-works.ru (accessed: July 26, 2019). DOI: 10.18577/2307-6046-2019-0-6-51-64.
  12. Franco M., Anoop S., Uma Rani R., Sharma A.K. Porous Layer Characterization of Anodized and Black-Anodized Aluminium by Electrochemical Studies // ISRN Corrosion. 2012. Vol. 2012. P. 1–12. DOI: 10.5402/2012/323676.13.
  13. Siva Kumar C., Rao V.S., Raja V.S. et al. Corrosion behaviour of solar reflector coatings on AA 2024T3 – An electrochemical impedance spectroscopy study // Corrosion Science. 2002. Vol. 44. No. 3. P. 387–393. DOI: 10.1016/S0010-938X(01)00082-8.14.
  14. Costenaro H., Lanzutti A., Paint Y. et al. Corrosion resistance of 2524 Al alloy anodized in tartaric-sulphuric acid at different voltages and protected with a TEOS-GPTMS hybrid sol-gel coating // Surface and Coatings Technology. 2017. Vol. 324. P. 438–450. DOI: 10.1016/j.surfcoat.2017.05.090.15.
  15. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  16. Kablov E.N., Antipov V.V., Klochkova Yu.Yu. Alyuminiy-litiyevyye splavy novogo pokole-niya i sloistyye alyumostekloplastiki na ikh osnove [New-generation aluminum-lithium alloys and layered aluminum-glass plastic based on them] // Tsvetnyye metally. 2016. №8. S. 86–91. DOI:10.17580/tsm.2016.08.13.17.
  17. Fomina M.A., Karimova S.A. Issledovanie korrozionnyh svojstv listov splava V-1461-T1 primenitelno k vseklimaticheskim usloviyam ekspluatacii aviacionnoj tehniki [Study of corrosion properties of V-1461-T1 aluminum alloy sheets in all-climatic conditions of aerotechnics operation] // Aviacionnye materialy i tehnologii. 2014. №4. S. 18–22. DOI: 10.18577/2071-9140-2014-0-4-18-22.
  18. Mansfeld F., Kendig M.W. Electrochemical Impedance Spectroscopy of protective coatings // Materials and Corrosion. 1985. Vol. 36. No. 11. P. 473–483. DOI: 10.1002/maco.19850361102.