Kondrashov S.V., Pykhtin A.A., Solovyanchik L.V., Bolshakov V.A., Pavlyuk B.Ph., Badamshina E.R., Dzhalmukhanova A.S., Karpov S.V. Research of dependence of adhesion of ice to polyurethane coatings from their physicomechanical properties // Proceedings of VIAM. 2019. No. 3 (75). Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-3-87-95.

Research of dependence of adhesion of ice to polyurethane coatings from their physicomechanical properties

Kondrashov S.V., Pykhtin A.A., Solovyanchik L.V., Bolshakov V.A., Pavlyuk B.Ph., Badamshina E.R., Dzhalmukhanova A.S., Karpov S.V.
Abstract

Development of the materials preventing frosting of various designs is one of relevant tasks of the modern polymeric industry. In this work, we studied the adhesion characteristics of ice to coatings based on polyurethanes of various grades: polypropylene glycol, polybutylene adipate, polycaprolactone diol, fluorine-containing oligodiol of the MAOK brand, including those modified with carbon Taunit-MD nanotubes. Researches of dependence of the dynamic module of elasticity of polymeric matrixes on temperature are conducted. It is shown that the elastic modulus of the investigated coatings lies in the range from 116 to 297 MPa. The amount of adhesion of ice to the investigated coatings ranges from 40 to 210 kPa. Introduction to structure of initial polyurethane compositions of carbon nanotubes leads to decrease in glass transition temperature the coatings. It is established that the size of adhesion of ice to the studied coatings is defined by the coatings thickness, density of a grid of cross chemical stitchings and also structure of a physical grid of gearing.

Keywords
ice adhesion, icing, polyurethane coatings, anti-icing coatings, functional coatings.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Kondrashov S.V., Yurkov G.Y. Prospects of using carbonaceous nanoparticles in binders for polymer composites // Nanotechnologies in Russia. 2013. Vol. 8. No. 3–4. P. 163–185.
  3. Kablov E.N. Konstruktsionnyye i funktsionalnyye materialy – osnova ekonomicheskogo i nauchno-tekhnicheskogo razvitiya Rossii [Structural and functional materials - the basis of economic and scientific-technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
  4. Yurkov G.Yu., Kondrashov S.V., Kraev I.D. Nanokompozity na osnove polijetilena vysokogo davleniya i nanochastic kobalta: sintez, struktura i svojstva [Nanocomposites based on high-density polyethylene and cobalt nanoparticles: synthesis, structure and properties] // Aviacionnye materialy i tehnologii. 2014. №S2. S. 29–33. DOI: 10.18577/2071-9140-2014-0-S2-29-33.
  5. Chajnikova A.S., Orlova L.A., Popovich N.V., Lebedeva Yu.E., Colncev S.St. Funkcionalnye kompozity na osnove steklo/steklokristallicheskih matric i diskretnyh napolnitelej: svojstva i oblasti primeneniya (obzor) [Functional composites based on glass/glass-ceramics matrixes and discrete fillers: properties and possible applications] // Aviacionnye materialy i tehnologii. 2014. №S6. S. 52–58. DOI: 10.18577/2071-9140-2014-0-s6-52-58.
  6. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Polimernye kompozicionnye materialy konstrukcionnogo naznacheniya s funkcionalnymi svojstvami [Constructional polymer composites with functional properties] // Aviacionnye materialy i tehnologii. 2017. №S. S. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  7. Kablov E.N., Startsev V.O. Sistemnyj analiz vliyaniya klimata na mekhanicheskie svojstva polimernykh kompozitsionnykh materialov po dannym otechestvennykh i zarubezhnykh istochnikov (obzor) [Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review)] // Aviacionnye materialy i tehnologii. 2018. №2 (51). S. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  8. Kirillov V.N., Efimov V.A., Shvedkova A.K., Nikolaev E.V. Issledovanie vliyaniya klimaticheskih faktorov i mehanicheskogo nagruzheniya na strukturu i mehanicheskie svojstva PKM [Research of influence of climatic factors and mechanical loading on structure and the PCM mechanical properties] // Aviacionnye materialy i tehnologii. 2011. №4. S. 41–45.
  9. Laforte J.L., Allaire M.A., Laflamme J. State-of-the-art on power line de-icing // Atmospheric Research. 1998. Vol. 46. No. 1–2. P. 143–158.
  10. Laakso T., Holttinen H., Ronsten G. et al. Baring-Gould State-of-the-art of wind energy in cold climates // IEA annex XIX. 2003. Vol. 24. P. 28–36.
  11. Ryerson C.C. Ice protection of offshore platforms // Cold Regions Science and Technology. 2011. Vol. 65. No. 1. P. 97–110.
  12. Dehghani-Sanij A.R., Dehghani S.R., Naterer G.F., Muzychka Y.S. Marine icing phenomena on vessels and offshore structures: Prediction and analysis // Ocean Engineering. 2017. Vol. 143. P. 1–23.
  13. Cao Y., Tan W., Wu Z. Aircraft icing: an ongoing threat to aviation safety // Aerospace Science and Technology. 2018. Vol. 75. P. 353–383.
  14. Wang Y., Xu Y., Huang Q. Progress on ultrasonic guided waves de-icing techniques in improving aviation energy efficiency // Renewable and Sustainable Energy Reviews. 2017. Vol. 79. С. 638–645.
  15. Jiang W., Huang Y., Sha A. A review of eco-friendly functional road materials //Construction and Building Materials. 2018. Vol. 191. P. 1082–1092.
  16. Fakorede O., Feger Z., Ibrahim H. et al. Ice protection systems for wind turbines in cold climate: characteristics, comparisons and analysis // Renewable and Sustainable Energy Reviews. 2016. Vol. 65. P. 662–675.
  17. Kreder M.J., Alvarenga J., Kim P., Aizenberg J. Design of anti-icing surfaces: smooth, textured or slippery? // Nature Reviews Materials. 2016. Vol. 1. No. 1. P. 15003.
  18. Solovyanchik L.V., Kondrashov S.V., Nagornaya V.S., Melnikov A.A. Osobennosti polycheniya antiobledenitelnykh pokrytiy (obzor) [Feature of receipt anti-icing coating (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №6 (66). St. 09. Available at: http://www.viam-works.ru (accessed: December 17, 2018). DOI: 10.18577/2307-6046-2018-0-6-77-98.
  19. Liu Y., Ma L., Wang W. et al. An experimental study on soft PDMS materials for aircraft icing mitigation // Applied Surface Science. 2018. Vol. 447. P. 599–609.
  20. Yeong Y.H., Milionis A., Loth E., Sokhey J. Self-lubricating icephobic elastomer coating (SLIC) for ultralow ice adhesion with enhanced durability // Cold Regions Science and Technology. 2018. Vol. 148. P. 29–37.
  21. Liu J., Wang J., Mazzola L. et al. Development and evaluation of poly (dimethylsiloxane) based composite coatings for icephobic applications // Surface and Coatings Technology. 2018. Vol. 349. P. 980–985.
  22. Li H., Li X., Luo C. et al. Icephobicity of polydimethylsiloxane-b-poly (fluorinated acrylate) // Thin Solid Films. 2014. Vol. 573. P. 67–73.
  23. Wang H., He G., Tian Q. Effects of nano-fluorocarbon coating on icing // Applied surface science. 2012. Vol. 258. No.18. P. 7219–7224.
  24. Li X., Li Y., Ren L., Zhu K. et al. Self-crosslinking coatings of fluorinated polysiloxanes with enhanced icephobicity // Thin Solid Films. 2017. Vol. 639. P. 113–122.
  25. Wang Y., Mingzhen J.L., Qingjun L. et al. The icephobicity comparison of polysiloxane modified hydrophobic and superhydrophobic surfaces under condensing environments // Applied Surface Science. 2016. Vol. 385. P. 472–480.
  26. Valentini L. Bon S.B., Hernández M. et al. Nitrile butadiene rubber composites reinforced with reduced graphene oxide and carbon nanotubes show superior mechanical, electrical and icephobic properties // Composites Science and Technology. 2018. Vol. 166. Р. 109–114.
  27. Golovin K., Kobaku S.R.P., Lee D.H. et al. Designing durable icephobic surfaces // Science Advances. 2016. Vol. 2. No. 3. P. 1–12.
  28. Santamaria-Echart А., Fernandes I., Saralegi A. at al. Synthesis of waterborne polyurethane-urea dispersions with chain extension step in homogeneous and heterogeneous media // Journal of Colloid and Interface Science. 2016. Vol. 476. P. 184–192.
  29. Zou M., Beckford S., Wei R. et al. Effects of surface roughness and energy on ice adhesion strength // Applied Surface Science. 2011. Vol. 257. No. 8. P. 3786–3792.
  30. Meuler A.J., Smith J.D., Varanasi K.K. et al. Relationships between water wettability and ice adhesion //ACS applied materials & interfaces. 2010. Vol. 2. No. 11. P. 3100–3110.
  31. Bharathidasan T., Kumar S.V., Bobji M.S. et al. Effect of wettability and surface roughness on ice-adhesion strength of hydrophilic, hydrophobic and superhydrophobic surfaces // Applied Surface Science. 2014. Vol. 314. P. 241–250.
  32. Léger L., Creton C. Adhesion mechanisms at soft polymer interfaces // Philosophical Transactions of the Royal Society of London A: Mathematical, Physical and Engineering Sciences. 2008. Vol. 366. No. 1869. P. 1425–1442.
  33. Chaudhury M.K., Kim K.H. Shear-induced adhesive failure of a rigid slab in contact with a thin confined film // The European Physical Journal E. 2007. Vol. 23. No. 2. P. 175–183.