M. D. Panteleev, A. Yu. Fink, A. V. Sviridov, Z. S. Dementev Laser cladding of aluminum alloy AD33 // Proceedings of VIAM. 2026. No. 9 (163). С. 33-46. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-9-33-46.
Laser cladding of aluminum alloy AD33
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
Abstract
The paper compares laser and argon-arc cladding for aluminum alloy AD33. Weldability was studied, then a suitable filler material was selected for cladding. Following non-destructive tomographic testing were tested welding modes, providing defect-free cladding. A comparative analysis of the welding thermal cycle on the microstructure and microhardness distribution in the cross-section of cladded samples from AD33 aluminum revealed the superior performance of laser cladding over argon-arc cladding.
Keywords
aluminum alloys, weldability, hot cracks, filler wire, restoration cladding, laser cladding, argon-arc cladding
Reference list
- Fridlyander I.N. Modern aluminum, magnesium alloys and composite materials based on them. Metallovedeniye i termicheskaya obrabotka metallov, 2002, no. 7, pp. 24–29.
- Alieva S.G., Altman M.B., Ambartsumyan S.M. Industrial aluminum alloys: reference publication. 2nd ed., rev. and add. Moscow: Metallurgiya, 1984, 528 p.
- Beletsky V.M., Krivov G.A. Aluminum alloys (Composition, properties, technology, application). Kiev: Komitetkh, 2005, 365 p.
- Kablov E.N., Belov E.V., Trapeznikov A.V., Leonov A.A., Zaitsev D.V. Strengthening features and aging kinetics of high-strength cast aluminum alloy AL4MS based on Al–Si–Cu–Mg system. Aviation materials and technologies, 2021, no. 2 (63), pp. 24–34. Available at: http://www.journal.viam.ru (accessed: December 01, 2025). DOI: 10.18577/2713-0193-2021-0-2-24-34.
- Ivanov A.L., Shlyapnikova T.A., Somov A.V., Selivanov A.A., Benarieb I., Mitasov M.M., Oleinik I.I., Polovyanenko D.N. Low-deformation quenching of sheets of aluminum alloy V95pch in a low-concentration water-polymer medium based on domestic components. Aviation materials and technologies, 2025, no. 3 (80), pp. 47–62. Available at: http://www.journal.viam.ru (accessed: December 02, 2025). DOI: 10.18577/2713-0193-2025-0-3-47-62.
- Kablov E.N., Duyunova V.A., Benarieb I., Puchkov Yu.A., Sbitneva S.V. Features of the decomposition of a supercooled solid solution during hardening of sheets of B-1341 alloy. Tekhnologiya legkikh splavov, 2020, no. 3, pp. 20–33. DOI: 10.18577/2071-9140-2020-0-3-20-33.
- Kablov E.N., Lukina E.A., Sbitneva S.V., Khokhlatova L.B., Zaitsev D.V. Formation of metastable phases during the decomposition of a solid solution during artificial aging of Al alloys. Tekhnologiya legkikh splavov, 2016, no. 3, pp. 7–17. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kolobnev N.I., Ber L.B., Khokhlatova L.B., Ryabov D.K. Structure, Properties, and Application of Al–Mg–Si–(Cu) System Alloys. Metallovedenie i termicheskaya obrabotka metallov, 2011, no. 9, pp. 40–45.
- Selivanov A.A., Antipov K.V., Oglodkova Yu.S., Rudchenko A.S. Structure and Properties of Sheets from the New Alloy B-1381. Perspektivnye materialy, 2021, no. 5, pp. 18–27. DOI: 10.30791/1028-978X-2021-5-18-27.
- Benarieb I., Puchkov Yu.A., Shumeiko R.M. Influence of heat treatment modes on the structure and resistance to general and local corrosion of sheets made of aluminum alloy B-1341 of the Al–Mg–Si system. Tekhnologiya legkikh splavov, 2025, no. 3, pp. 18–32. DOI: 10.18698/0236-3941-2016-2-125-133.
- Benarieb I., Sbitneva S.V., Zaytsev D.V., Shorstov S.Yu. Features of quench-induced precipitation in sheets of V-1341 aluminum alloy of Al–Mg–Si system. Trudy VIAM, 2025, no. 8 (150), pp. 53–66. Available at: http://www.viam-works.ru (accessed: December 02, 2025). DOI: 10.18577/2307-6046-2025-0-2-53-66.
- Benarieb I., Romanenko V.A., Klochkova Yu.Yu., Ovchinnikov V.V., Sbitneva S.V. Application of hightech aluminum alloy V-1341 of Al–Mg–Si system for pipelines of aircraft products. Trudy VIAM, 2020, no. 11 (93), pp. 21–30. Available at: http://www.viam-works.ru (accessed: December 02, 2025). DOI: 10.18577/2307-6046-2020-0-11-21-30.
- Nikolaev G.A., Fridlyander I.N., Arbuzov Yu.P. Weldable aluminum alloys. Moscow: Metallurgiya, 1990, 296 p.
- Nikiforov T.D. Metallurgy of fusion welding of aluminum alloys. Moscow: Mashinostroenie, 1972, 264 p.
- Yakushin B.F., Makarov E.L. Theory of weldability of steels and alloys. Moscow: Publ. house of MSTU im.N.E. Bauman, 2018, 487 p.
- Likhanskii V.V., Ulybyshev K.E., Elkin N.N. Numerical simulations of the processes induced by laser shock peening in AMg6 aluminum alloy. Aviation materials and technologies, 2025, no. 2 (79), pp. 33–47. Available at: http://www.journal.viam.ru (accessed: December 11, 2025). DOI: 10.18577/2713-0193-2025-0-2-33-47.
- Rykalin N.N., Uglov A.A., Zuev I.V., Kokora A.N. Laser and Electron-Beam Processing of Materials: Handbook. Moscow: Mashinostroenie, 1985, 496 p.
- Volchenko V.N., Yampolsky V.M., Vinokurov V.A. et al. Theory of Welding Processes. Ed. V.V. Frolov. Moscow: Vysshaya shkola, 1988, 559 p.
- Lukin V.I., Kovalchuk V.G., Ioda E.N. Fusion welding is a core of welding manufacturing. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 130–143. DOI: 10.18577/2071-9140-2017-0-S-130-143.
- Panteleev M.D., Sviridov A.V., Skupov A.A. Welding features of heat-resistant aluminum alloys, alloy V-1213 and 1151. Trudy VIAM, 2022, no. 9 (115), pp. 28–39. Available at: http://www.viam-works.ru (accessed: December 11, 2025). DOI: 10.18577/2307-6046-2022-0-9-28-38.
- Panteleev M.D., Sviridov A.V., Skupov A.A., Odintsov N.S. Aluminum-Lithium alloy V-1469 welded fuselage constructions survivability. Aviation materials and technologies, 2022, no. 4 (69), pp. 25–35. Available at: http://www.journal.viam.ru (accessed: December 12, 2025). DOI: 10.18577/2713-0193-2022-0-4-25-35.
The article was submitted
2026-01-30
approved and accepted for publication after reviewing
2026-05-27