E. A. Timoshina, V. A. Kuznetsova, S. A. Marchenko Influence of modification of polyester film-forming substance on wear resistance and decorative properties of lacquer coatings // Proceedings of VIAM. 2026. No. 9 (163). С. 141-148. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-9-141-148.
Influence of modification of polyester film-forming substance on wear resistance and decorative properties of lacquer coatings
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
Abstract
The effect of the chemical nature of the modifier and its concentration in a polyester film-forming agent on the wear resistance, gloss, and roughness of varnish coatings was studied. The adhesion, physical and mechanical properties (flexural resilience, impact strength), roughness, and gloss of the coating (in the initial state and after abrasion for 7000 cycles) were examined. The optimal modifiers and their ratio with the polyester were determined to obtain a coating with the required combination of properties.
Keywords
polymer film-forming agent, modifier, hardener, lacquer coating, wear resistance, adhesion, coating gloss, roughness
Reference list
- Kablov E.N. Aviation Materials Science in the 21st Century. Prospects and Tasks. Aviation Materials. Selected Works of VIAM 1932–2002. Moscow: MISiS–VIAM, 2002, pp. 23–47.
- Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products. Trudy VIAM, 2019, no. 5 (77), pp. 62–67. Available at: http://www.viam-works.ru. (accessed: April 16, 2026). DOI: 10.18577/2307-6046-2019-0-5-62-67.
- Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), pp. 70–80. Available at: http://www.journal.viam.ru (accessed: April 16, 2026). DOI: 10.18577/2713-0193-2021-0-4-70-80.
- Kablov E.N. New Generation Materials – the Basis for Innovation, Technological Leadership, and National Security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
- Kablov E.N. New Generation Materials. Zashchita i bezopasnost, 2014, no. 4, pp. 28–29.
- Kablov E.N. Main Results and Directions for the Development of Materials for Advanced Aviation Technology. 75th Anniversary. Aviation Materials. Moscow: VIAM, 2007, pp. 20–26.
- Kuznetsova V.A., Timoshina E.A., Shapovalov G.G., Zheleznyak V.G. Trends in the development of matte wear-resistant paint coatings. Trudy VIAM, 2023, no. 10 (128), pp. 132–144. Available at: http://www.viam-works.ru (accessed: April 16, 2026). DOI: 10.18577/2307-6046-2023-0-10-132-144.
- Romanova A.V., Sokolova E.A., Razuvaev A.V. Protective wear-resistant coatings of machine parts. Coll. sci. t. IX All-Rus. sc. and tech. conf. with int. participation «Modern innovations in science and technology». Kursk, 2019, pp. 313–316.
- Gohardani O. Impact of erosion testing aspects on current and future flight conditions. Progress in Aerospace Science, 2011, vol. 47, pp. 280–303.
- Merkulova Yu.I., Kuznetsova V.A., Kodachenko E.N., Zheleznyak V.G. Study of the influence of the primer layer's chemical nature on the properties of the coating system based on fluoropolymerthane enamel. Aviation materials and technologies, 2022, no. 1 (66), pp. 110–119. Available at: http://www.journal.viam.ru (accessed: April 16, 2026). DOI: 10.18577/2713-0193-2022-0-1-110-119.
- Sukhareva L.A. Polyester coverings: structure and properties. Moscow: Khimia, 1987, 192 p.
- Kozlova A.A., Kondrashov E.K. Influence of molecular weight and elemental composition of isocyanates on the properties of fluoropolymerthane enamels. Aviation materials and technologies, 2023, no. 4 (73), pp. 92–100. Available at: http://www.journal.viam.ru (accessed: April 16, 2026). DOI: 10.18577/2713-0193-2023-0-4-92-100.
- Kuznetsova V.A., Timoshina E.A., Shapovalov G.G., Kurshev E.V. Influence of amodified film-forming agent on the properties of anti-wear matte coating used to protect cabin and dashboard components in aircraft. Trudy VIAM, 2025, no. 9 (151), pp. 90–101. Available at: http://www.viam-works.ru (accessed: April 16, 2026). DOI: 10.18577/2307-6046-2025-0-9-90-101.
- Bobryshev A.N., Kozomazov V.N., Kozomazov R.V. et al. Strength and Durability of Polymer Composite Materials. Ed. V.I. Solomatov. Lipetsk: Orius, 1994, 153 p.
- Bobryshev A.N., Kozomazov V.N., Babin L.O., Solomatov V.I. Synergetics of Composite Materials. Lipetsk: Yulis, 2006, 170 p.
- Bobryshev A.N., Gumerov A.F., Zharin D.E. et al. Physicomechanics of Durability and Strength of Composite Materials. Moscow: Academia, 2007, 226 p.
- Gulyaev I.N., Klimenko O.N., Lonskii S.L., Slavin A.V., Cherfas L.V. Determination of the composition and structure of polymer composite materials. Aviation materials and technologies, 2025, no. 4 (81), pp. 32–47. Available at: http://www.journal.viam.ru (accessed: April 24, 2026). DOI: 10.18577/2713-0193-2025-0-4-32-47.
- Verkholantsev V.V., Babyants V.D., Mulin Yu.A. Wear-resistant coatings from two-phase polymer-oligomer composites. Lakokrasochnye materialy i ikh primenenie, 1981, no. 2, pp. 26–27.
- Strekachinskaya E.S., Verkholantsev V.V., Grozinskaya Z.P. Patterns of stratification of oligomer mixture solutions. Lakokrasochnye materialy i ikh primenenie, 1980, no. 4, pp. 13–15.
- Müller B., Pot U. Paints and varnishes and coatings. Formulation principles. Moscow: Paint-Media, 2007, 237 p.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
The article was submitted
2026-06-18
received in revised form
2026-07-10
approved and accepted for publication after reviewing
2026-07-14