Vakhrusheva Ja.A., Tkachuk A.I., Afanaseva E.A., Kurshev E.V., Lonskii S.L. Perspective epoxy resin system VSE-81 for incoming quality inspection of carbon fiber // Proceedings of VIAM. 2026. No. 6 (160). С. 96–107. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-6-96-107.

Perspective epoxy resin system VSE-81 for incoming quality inspection of carbon fiber

Vakhrusheva Ja.A., Tkachuk A.I., Afanaseva E.A., Kurshev E.V., Lonskii S.L.
Abstract

In the study the technological and operational characteristics of the epoxy resin system VSE-81, developed at the NRC «Kurchatov Institute» – VIAM, are considered. The results of gelation and rheological tests are presented. Mechanical properties are obtained by stretching VSE-81 samples cured according to the selected mode, and the conversion rate is determined by the DSC method. We compared the mechanical characteristics of microplastics based on UMT49S-12K-EP carbon fiber with VSE-81 binder and its imported analogue. The results of microstructural research interpreted using a model of the microcomposite structure of thermosetting polymers are presented.

Keywords
epoxy resin system, polymeric composite materials, microplastics, testing of carbon fibers
Reference list
  1. Gunyaeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
  2. Putilina P.M., Kutsevich K.E., Isaev A.Yu. Carbon fiber-reinforced and glass fiber-reinforced polymer composites for the manufacture of components for unmanned aerial vehicles and their developing prospects. Trudy VIAM, 2023, no. 8 (126), pp. 85–99. Available at: http://www.viam-works.ru (accessed: August 15, 2025). DOI: 10.18577/2307-6046-2023-0-8-85-99.
  3. Park S.-J. Carbon Fibers. Singapore: Springer Verlag, 2019, 358 p.
  4. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122–144. Available at: http://www.journal.viam.ru (accessed: August 18, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  5. Gunyaeva A.G., Kurnosov A.O., Gulyaev I.N. High-temperature polymer composite materials developed FSUE «VIAM» for aerospace engineering: past, present and future (review). Trudy VIAM, 2021, no. 1 (95), pp. 43–53. Available at: http://www.viam-works.ru (accessed: August 15, 2025). DOI: 10.18577/2307-6046-2021-0-1-43-53.
  6. Valueva M.I., Evdokimov A.A., Klimenko O.N., Nacharkina A.V. Carbon fiber-reinforced plastics in spacecraft designs (review). Vse materialy. Entsiklopedicheskiy spravochnik, 2022, no. 1, pp. 12–21.
  7. Analysis of the Russian carbon fiber-based polymer composites market. Interregional industrial cluster «Composites without Borders». Available at: http://www.compositescluster.ru/documentation/ (accessed: August 15, 2025).
  8. Valueva M.I., Zelenina I.V., Mishurov K.S., Gulyaev I.N. Review of publications on the development of blades made of polymer composite materials for aircraft engine fans. Vestnik mashinostroyeniya, 2019, no. 2, pp. 34–41.
  9. Varshavsky V.Ya. Carbon fibers. Moscow: Nauka, 2005, 496 p.
  10. Molchanov B.I., Gudimov M.M. Properties of carbon fiber reinforced plastics and their scope of application. Aviatsionnaya promyshlennost, 1997, no. 3–4, pp. 58–60.
  11. Erasov V.S., Sibayev I.G., Sutubalov A.I., Popkova E.A., Gorbovets M.A. Methods of mechanical testing to determine the strength of carbon fibers. Aviation materials and technologies, 2024, no. 2 (75), pp. 137–148. Available at: http://www.journal.viam.ru (accessed: August 15, 2025). DOI: 10.18577/2713-0193-2024-0-2-137-148.
  12. Erasov V.S., Konoplenko V.P., Pirogov E.N. Effect of the Sample Base on the Strength of Carbon Fibers. Fizika i mekhanika deformatsii i razrusheniya, 1978, is. 5, pp. 48–53.
  13. Ginne S.V. On the Issue of Polymer Composite Materials Based on Carbon Fibers. Mekhaniki XXI veku, 2022, no. 21, pp. 235–241.
  14. Kolobkov A.S., Malakhovsky S.S. Development of Carbon Fiber Production Technologies (review). Khimicheskie volokna, 2020, no. 1, pp. 3–7.
  15. Malakhovsky S.S., Panafidnikova A.N., Kostromina N.V., Osipchik V.S. Carbon fiber reinforced plastics in the modern world: their properties and applications. Uspekhi v khimii i khimicheskoy tekhnologii, 2019, vol. 33, no. 6 (216), pp. 62–64.
  16. Gul V.E., Kuleznev V.N. Structure and mechanical properties of polymers. Moscow: Labirint, 1994, 367 p.
  17. State Standard R ISO 10618–2012 (ISO 10618:2004, ASTM D 3039). Carbon fiber. Method for determination of tensile mechanical properties of resin-impregnated yarns. Moscow: Standartinform, 2015, 23 p.
  18. GOST 11262–2017 (ISO 527-2:2012). Plastics. Tensile test method. Moscow: Standartinform, 2018, 26 p.
  19. Fracture Mechanics. Fracture of Materials. Trans. from Engl. Ed. R.V. Goldstein. Moscow: Mir, 1979, 240 p.
  20. Deev I.S., Kobets L.P. Fractography of Epoxy Polymers. Vysokomolekulyarnye soedineniya. Ser.: A, 1996, vol. 38, no. 4, pp. 27–34.
  21. Deev I.S., Kurshev E.V., Lonskii S.L., Nikishin E.F. Тhe structure and composition of samples made of carbon-fiber-reinforced plastic KMU-4l exposed for 12 years on the exterior surface of the international space station: 1. Macrostructure and surface composition. Inorganic Materials: Applied Research, 2016, vol. 7, no. 6, pp. 840–846.
  22. Kurshev E.V., Lonskiy S.L., Egorov Yu.A., Zelenina I.V. Study of changes in the microstructure and chemical composition of polyimide carbon fiber reinforced plastic after exposure to simulated operational factors. Voprosy Materialovedeniya, 2024, no. 4 (120), pp. 88–102.
  23. Kurshev E.V., Lonskiy S.L., Deev I.S. Application of scanning electron microscopy and X-ray spectral microanalysis to study non-metallic composite materials. Study of structural materials and functional coatings by optical, scanning and transmission electron microscopy, X-ray diffraction and X-ray spectral microanalysis: collection of materials of the VIII All-Rus. Conf. on testing and research of materials properties «TestMat». Moscow, 2016, part 2, pp. 1–13.
  24. Zelenina I.V., Valueva M.I., Nacharkina A.V., Kurshev E.V. Structure and properties of high-temperature carbon fiber reinforced plastic based on polyimide binder. Trudy VIAM, 2023, no. 3 (121), pp. 13–28. Available at: http://www.viam-works.ru (accessed: August 15, 2025). DOI: 10.18577/2307-6046-2023-0-3-13-28.
  25. State Standard 25271–93 (ISO 2555:1989). Plastics. Liquid resins, emulsions, or dispersions. Determination of apparent viscosity by the Brookfield method. Moscow: Publishing House of Standards, 1994, 15 p.
  26. State Standard R 55134–2012 (ISO 11357-1:2009). Plastics. Differential scanning calorimetry (DSC). Part 1. General principles. Moscow: Standartinform, 2014, 26 p.
  27. Veshkin E.A., Slavin A.V., Postnova M.V., Apalkova A.V. The role of temperature-time curing conditions in the formation of unidirectional and equally strong carbon fiber plastics properties. Aviation materials and technologies, 2025, no. 2 (79), pp. 59–71. Available at: http://www.journal.viam.ru (accessed: August 15, 2025). DOI: 10.18577/2713-0193-2025-0-2-59-71.
  28. Zelenina I.V., Gulyayev I.N., Kucherovskiy A.I., Mukhametov R.R. Heat-resistant CFRP for the impulse wheel of the centrifugal compressor. Trudy VIAM, 2016, no. 2 (38), pp. 64–71. Available at: http://www.viam-works.ru (accessed: August 18, 2025). DOI: 10.18577/2307-6046-2016-0-2-8-8.
  29. Deev I.S., Kablov E.N., Kobets L.P., Chursova L.V. Research of the scanning electron microscopy method deformation of microphase structure of polymeric matrix at mechanical loading. Trudy VIAM, 2014, no. 7, pp. 35–50. Available at: http://www.viam-works.ru (accessed: August 18, 2025). DOI: 10.18577/2307-6046-2014-0-7-6-6.
  30. Deev I.S., Kobets L.P. Study of the microstructure and fracture characteristics of epoxy polymers and composite materials based on them. Materialovedenie, 2010, no. 5, pp. 8–16.
  31. Deev I.S., Kobets L.P. Study of the microstructure and fracture characteristics of epoxy polymers and composite materials based on them (conclusion). Materialovedenie, 2010, no. 6, pp.13–18.
  32. Liu L., Du M., Liu F. Recent advances in interface microscopic characterization of carbon fiber-reinforced polymer composites. Frontiers in Materials, 2023, vol. 10, pp. 1–18.