Vlasov I.I., Sevalnev G.S., Valyuhova I.V., Dyachenko O.A. Analysis of the parameters of deformation hardening of a multicomponent high-entropy alloy of the NiCoCrWReNbAlTiC system according to the Johnson–Cook model // Proceedings of VIAM. 2026. No. 6 (160). С. 46–56. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-6-46-56.

Analysis of the parameters of deformation hardening of a multicomponent high-entropy alloy of the NiCoCrWReNbAlTiC system according to the Johnson–Cook model

Vlasov I.I., Sevalnev G.S., Valyuhova I.V., Dyachenko O.A.
Abstract

This paper presents a comprehensive analysis of the deformation hardening of a NiCoCrWReNbAlTiC system heat-resistant alloy, made by casting, hot plastic deformation and selective laser sintering. It is established that materials produced by selective laser sintering method with further heat treatment demonstrate the highest deformation hardening characteristics with a relative contribution of up to 70 %. The material after hot plastic deformation with subsequent heat treatment shows maximum values of the hardening modulus (460.4 MPa at ε  = 0.1).

Keywords
deformation hardening, Johnson–Cook model, selective laser sintering, hot plastic deformation, casting, mechanical properties, high-entropy alloys
Reference list
  1. Kablov E.N., Ospennikova O.G., Vershkov A.V. Rare metals and rare-earth elements are materials for modern and future high technologies. Aviacionnye materialy i tehnologii, 2013, no. S2, pp. 3–10.
  2. Kablov E.N. Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode. Aviacionnye materialy i tehnologii, 2013, no. S1, pp. 3–9.
  3. Sevalnev G.S. Beryllium-containing steels – perspective material with a high level of physical and mechanical properties. Aviation materials and technologies, 2023, no. 3 (72), pp. 15–29. Available at: http://www.journal.viam.ru (accessed: July 25, 2025). DOI: 10.18577/2713-0193-2023-0-3-15-29.
  4. Kaplanskii Yu.Yu., Mazalov P.B. World trends in the development of refractory high-entropy alloys for heat-loaded units of aerospace technics (review). Aviation materials and technologies, 2022, no. 2 (67), pp. 30–42. Available at: http://www.journal.viam.ru (accessed: October 17, 2025). DOI: 10.18577/2713-0193-2022-0-2-30-42.
  5. Sevalnev G.S., Korobova E.N., Dvoreckov R.M., Doroshenko A.V., Muzafarova S.-V.R., Samoilova I.I. Influence of the degree of martensitic structure dispersion and size of carbide phase on the frictional interaction under conditions of dry sliding friction of high-carbon complex alloy steel. Trudy VIAM, 2022, no. 6 (112), pp. 15–26. Available at: http://www.viam-works.ru (accessed: July 25, 2025). DOI: 10.18577/2307-6046-2022-0-6-15-26.
  6. Vlasov I.I., Sevalnev G.S., Lyahov A.A., Nefedkin D.Yu. Study of the structure and mechanical properties of Ni–Co–Cr entropy alloy in the cast state. Trudy VIAM, 2024, no. 12 (142), pp. 18–30. Available at: http://www.viam-works.ru (accessed: March 20, 2026). DOI: 10.18577/2307-6046-2024-0-12-18-30.
  7. Kablov E.N., Sidorov V.V., Min P.G., Vadeev V.E., Kramer V.V. Research and development of technological parameters for vacuum melting of corrosion-resistant heat-resistant nickel alloys. Metallurg, 2021, no. 2, pp. 62–67.
  8. Gibson I., Rosen D.W., Stucker B. Additive Manufacturing Technologies: Rapid Prototyping to Direct Digital Manufacturing. Springer, 2010, 459 p.
  9. Ludwik P. Elemente der technologischen Mechanik. Berlin: Springer, 1909, 32 p.
  10. Hollomon J.H. Tensile deformation. Transactions of the Metallurgical Society of AIME, 1945, vol. 162, рр. 268–290.
  11. Kelly A., Nicholson R.B. Strengthening Methods in Crystals. London: Applied Science Publishers, 1971, 534 p.
  12. Khan A.S., Huang S. Continuum theory of plasticity. John Wiley & Sons, 1995, 420 p.
  13. Johnson G.R., Cook W.H. A constitutive model and data for metals subjected to large strains, high strain rates and high temperatures. Proceedings of the 7th International Symposium on Ballistics. 1983, vol. 21, pp. 541–547.
  14. Yadroitsev I., Gusarov A., Yadroitsava I., Smurov I. Single track formation in selective laser melting of metal powders. Journal of Materials Processing Technology, 2010, vol. 210, pp. 1624–1631.
  15. Sames W.J., List F.A., Pannala S. et al. The metallurgy and processing science of metal additive manufacturing. International Materials Reviews, 2016, vol. 61 (5), pp. 315–360.
  16. Herzog D., Seyda V., Wycisk E., Emmelmann C. Additive manufacturing of metals. Acta Materialia, 2016, vol. 117, рр. 371–392.
  17. Valiev R.Z., Aleksandrov I.V. Nanostructured materials obtained by severe plastic deformation. Moscow: Logos, 2000, 272 p.
  18. McQueen H.J., Ryan N.D. Constitutive analysis in hot working. Materials Science and Engineering A, 2002, vol. 322, pp. 43–63.
  19. Hirsch P.B., Howie A., Nicholson R.B. Electron Microscopy of Thin Crystals. London: Butterworths, 1965, 549 p.
  20. Meerson G.A. High-Strength Austenitic Steels. Moscow: Metallurgiya, 1982, 295 p.
  21. Kolachev B.A., Livanov V.A., Elagin V.I. Metallurgy and Heat Treatment of Non-Ferrous Metals and Alloys. Moscow: MISiS, 2005, 432 p.
  22. Hall E.O. The deformation and ageing of mild steel: III Discussion of results. Proceedings of the Physical Society B, 1951, vol. 64 (9), pp. 747–753.
  23. Lin Y.C., Chen X.M. A critical review of experimental results and constitutive descriptions for metals and alloys in hot working. Materials & Design, 2011, vol. 32, pp. 1733–1759.