Knyazev A. E., Min P.G. Features of manufacturing and filling large-sized and ring-shaped capsules in granule metallurgy. Analysis of shape change after hot isostatic pressing // Proceedings of VIAM. 2026. No. 6 (160). С. 32–45. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-6-32-45.

Features of manufacturing and filling large-sized and ring-shaped capsules in granule metallurgy. Analysis of shape change after hot isostatic pressing

Knyazev A. E., Min P.G.
Abstract

The article discusses the production of large-diameter «ring» capsules with a diameter-to-height ratio of more than 8 and massive large-diameter capsules with a diameter of up to 1000 mm for subsequent production of disk blanks by hot isostatic pressing. The features of filling the capsules with granules in a horizontal position are considered. The shape change of compact blanks after hot isostatic pressing is analyzed and shrinkage coefficients are calculated. The factors that affect the shape change of compact disk blanks and the shrinkage coefficients are examined.

Keywords
capsule, degassing, sealing, granules, compacting, hot isostatic pressing, granule metallurgy, shaping, filling density, horizontal filling, size composition, powder, segregation, density
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Vostrikov A.V., Yashin M.S., Kapitanenko D.V. Peculiarities of the technology of production of aircraft engine parts from granules of heat-resistant nickel alloys by the method of plasma melting and centrifugal spraying of a cast rotating blank. Trudy VIAM, 2025, no. 8 (150), pp. 16–26. Available at: http://www.viam-works.ru (accessed: December 10, 2025). DOI: 10.18577/2307-6046-2025-0-10-16-26.
  3. Min P.G., Vadeev V.E. The development and introduction into serial production of the new superalloy VZhL125 for the advanced aviation engines vanes. Aviation materials and technologies, 2023, no. 1 (70), pp. 3–16. Available at: http://www.journal.viam.ru (accessed: December 10, 2025). DOI: 10.18577/2713-0193-2023-0-1-3-16.
  4. Echin A.B., Bondarenko Yu.A., Kolodyazhny M.Yu., Surova V.A. Review of perspective high-temperature superalloys based on refractory non-metallic materials for production of gas turbine engines. Aviation materials and technologies, 2023, no. 3 (72), pp. 30–41. Available at: http://www.journal.viam.ru (accessed: December 10, 2025). DOI: 10.18577/2713-0193-2023-0-3-30-41.
  5. Narsky A.R., Deynega G.I., Kuzmina I.G. Obtaining a fine-grained structure of castings from nickel superalloys using a cobalt aluminate modifier. Aviation materials and technologies, 2023, no. 3 (72), pp. 3–14. Available at: http://www.journal.viam.ru (accessed: December 10, 2025). DOI: 10.18577/2713-0193-2023-0-3-3-14.
  6. Samarov V.N., Nepomnyashchy V.Z. Problems of Granule Metallurgy Processes. Tekhnologiya legkikh splavov, 2008, no. 1, pp. 9–20.
  7. Koshelev V.Ya. Study of the Process, Development, and Implementation of Industrial Technology for Thermal Degassing of Granules of Heat-Resistant Nickel Alloys of the EP741P Type in the Production of GTE Disk Blanks: thesis abstract, Cand. Sc. (Tech.). Moscow, 1985, 36 p.
  8. Musienko V.T. Development of Theoretical Foundations and Technology for the Production of Metal Powders at High and Ultra-High Cooling Rates by Centrifugal Atomization for the Manufacture of Gas Turbine Engine Components: thesis abstract, Dr Sc. (Tech.). Moscow, 1991, 54 p.
  9. Khodkin V.I. Research of processes and creation of technology for pulse-mechanical and vacuum-thermal treatment of granules of heat-resistant nickel alloys in the production of blanks for engine building: thesis abstract, Dr Sc. (Tech.). Moscow: VILS, 1982, 52 p.
  10. Kablov E.N. Powders eliminate excess. Ekspert, 2014, no. 49 (926), pp. 46–51.
  11. Knyazev A.E., Nerush S.V., Alishin M.I., Kuko I.S. Researches of the technological properties of metal-powder compositions of Ti-4-6 and VT20 titanium alloys obtained by induction melting and gas atomization. Trudy VIAM, 2017, no. 11 (59), pp. 46–55. URL: http://www.viam-works.ru (дата обращения: January 09, 2026). DOI: 10.18577/2307-6046-2017-0-11-6-6.
  12. Girshov V.L., Kotov S.A., Tsemenko V.N. Modern technologies in powder metallurgy: textbook. St. Petersburg: Publ. house of the Polytech. Univ., 2010, pp. 200–214.
  13. Knyazev A.E., Vostrikov A.V. Sieving of powders additive and powder manufacturings (review). Trudy VIAM, 2020, no. 11 (93), рр. 11–20. Available at: http://www.viam-works.ru (accessed: August 29, 2025). DOI: 10.18577/2307-6046-2020-0-11-11-20.
  14. Samarov V.N. Hot isostatic pressing of complex-shaped parts. Results and problems. Tekhnologiya legkikh splavov, 2000, no. 6, pp. 69–72.
  15. Shoroshev Yu.G., Rekhviashvili E.E., Fatkullin O.Kh. Development of a method and installation for determining the volume of capsules before hot isostatic pressing of granules. Metallurgiya granul, 1986, is. 3, pp. 83–86.
  16. Koshelev V.Ya., Buvin E.P., Kononov I.A. et al. Some features of the technology of group filling of large-sized capsules with granules in UZGK-type installations. Metallurgiya granul, 1989, is. 5, pp. 193–197.
  17. Khodkin V.I., Tararyshkina T.L. Effect of Granule Filling Modes in Capsules on Granule Segregation by Size. Metallurgiya granul, 1983, is. 1, pp. 110–114.
  18. Andrianov E.I. Methods for Determining Structural and Mechanical Characteristics of Powdered Materials. Moscow: Khimmiya, 1982, 255 p.
  19. Koshelev V.Ya., Garibov G.S. Effect of Heat-Resistant Nickel Alloy Granule Filling Density on Capsule Forming during Hot Isostatic Pressing. Tekhnologiya legkikh splavov, 2013, is. 1, pp. 27–33.
  20. Dzhenike E.V. Storage and Release of Bulk Materials. Trans. from Engl. by G.I. Arbachakova, ed. M.I. Agoshkova. Moscow: Mir, 1968, 164 p.