Karashaev M.M., Petrushin N.V., Zaysev D.V., Svetlov I.L. Structure formation during hot plastic deformation of a nickel high-temperature alloy with zero γ/γ′-misfit // Proceedings of VIAM. 2026. No. 6 (160). С. 3–18. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-6-3-18.

Structure formation during hot plastic deformation of a nickel high-temperature alloy with zero γ/γ′-misfit

Karashaev M.M., Petrushin N.V., Zaysev D.V., Svetlov I.L.
Abstract

In this work, using the method of transmission electron microscopy, the mechanisms of grain structure formation during hot deformation and microstructure formation during subsequent full heat treatment in the two-phase (γ + γ′)-region of an experimental nickel-based superalloy with zero γ/γ'-misfit for gas turbine engine disks have been identified. The chemical composition of this alloy was developed based on a granular nickel-based superalloy VZh178P using the method of computer design. Creep mechanisms at temperatures of 750 and 850 °C for an experimental deformed alloy in a heat-treated state were analyzed.

Keywords
deformable nickel-based superalloys, hot deformation, grain structure, recrystallization, deformation defects, microsegregation of alloying elements, creep mechanisms
Reference list
  1. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 2. Aviation materials and technologies, 2023, no. 2 (71), pp. 3–22. Available at: http://www.journal.viam.ru (accessed: December 01, 2025). DOI: 10.18577/2713-0193-2023-0-2-3-22.
  4. D’Souza N., Li W., Argyrakis C. et al. On the Evolution of Primary Gamma Prime Precipitates During High Temperature and High Strain Rate Deformation and Subsequent Heat Treatment in the Ni-Based Superalloy, RR1000. Metallurgical and Materials Transactions A, 2019, vol. 50A, pp. 4205–4222.
  5. Aoki C., Ueno T., Ohno T. Influence of hot working conditions on grain growth behavior of Alloy 718. Superalloys 2016. Pennsylvania: Minerals, Metals & Materials Society, 2016, pp. 609–617.
  6. Parr I.M.D., Jackson T.J., Hardy M.C. et al. In homogeneous grain coarsening behavior in supersolvus heat treated nickel-based superalloy RR1000. Superalloys 2016. Pennsylvania: Minerals, Metals & Materials Society, 2016, pp. 447–456.
  7. Thomas J.-P., Bauchet E., Dumont C., Montheille F. Electrone Backscattered Diffraction Investigation and Modeling of the Microstructural Evolutions of Superalloy 718 During Hot Deformation. Superalloys 2004. Pennsylvania: Minerals, Metals & Materials Society, 2004, pp. 959–968.
  8. Tu Wen, Pollock Tresa M. Grain scale straining processes during high temperature compression of a PM disk alloy. Superalloys 2008. Pennsylvania: Minerals, Metals & Materials Society, 2008, pp. 395–403.
  9. Kienl C., Leon-Cazares F.D., Rae C.M.F. Deformation twinning during high temperature compression tests of the Ni-base superalloy ATI 718Plus. Acta Materialia, 2022, vol. 225, no. 4–5, pp. 1–21. DOI: 10.1016/j.actamat.2019.12.047.
  10. Lin L., Xu P., Wang P. et al. Dissolution of η phase and evolution of dynamically recrystallized grains in ATI 718Plus superalloy during hot compressive deformation. Journal of Materials Research and Technology, 2024, vol. 30, pp. 4612–4624.
  11. Azarbarmasa M., Aghaie-Khafria M., Cabrera J.M., Calvo J. Dynamic recrystallization mechanisms and twining evolution during hot deformation of Inconel 718. Materials Science & Engineering A, 2016, vol. 678, pp. 137–152. DOI: 10.1016/j.msea.2016.09.100.
  12. Xie B., Yu H., Sheng T. et al. Discontinuous Dynamic Recrystallization and Continuous Dynamic Recrystallization of an as-cast nickel-based superalloy during hot compression at γ′ sub-/super-solvus temperatures. Journal of Alloys and Compounds, 2019, vol. 803, pp. 16–29. DOI: 10.1016/j.jallcom.2019.06.202.
  13. Lv S., Chen J., He X. et al. Investigation on Sub-Solvus Recrystallization Mechanisms in an Advanced γ-γ′ Nickel-Based Superalloy GH4151. MDPI Materials, 2020, vol. 13, p. 4553. DOI: 10.339/ma13204553.
  14. Cuia J., Liu Y., Zhong L. et al. Microstructure and γ′ phase evolution characteristics of novel nickel-based superalloy during compression. Journal of Materials Research and Technology, 2024, vol. 33, pp. 9968–9978.
  15. Charpagne M.-A., Billot T., Franchet J.-M., Bozzolo N. Heteroepitaxial Recrystallization, a new Recrystallization Mechanism in sub-solvus Forged γ-γ′ Nickel-Based Superalloys with low Lattice Mismatch. Proceedings of the 6th International Conference on Recrystallization and Grain Growth (ReX&GG 2016). TMS, 2016, pp. 259–264.
  16. Charpagne M.-A., Billot T., Franchet J.-M., Bozzolo N. Heteroepitaxial Recrystallization Observed in Rene65TM and Udimet720TM: A new Recrystallization Mechanism Possibly Occuring in All Low Lattice Mismatch γ-γ′ Superalloys? Superalloys 2016. Pennsylvania: Minerals, Metals & Materials Society, 2016, pp. 417–426.
  17. Petrushin N.V., Visik E.M., Elyutin E.S. Improvement of the chemical composition and structure of castable nickel-base superalloy with low density. Part 2. Trudy VIAM, 2021, no. 4 (98), pp. 3–15. Available at: http://www.viam-works.ru (accessed: December 01, 2025). DOI: 10.18577/2307-6046-2021-0-4-3-15.
  18. Petrushin N.V., Zaitsev D.V., Svetlov I.L., Karashaev M.M., Epishin A.I. Mechansims of creep in the temperature range 750–850 °С оf nickel-based superalloy with zero γ/γ′-lattice misfit. Trudy VIAM, 2023, no. 12 (130), pp. 3–18. Available at: http://www.viam-works.ru (accessed: December 01, 2025). DOI: 10.18577/2307-6046-2023-0-12-3-18.
  19. Martin J., Doherty R. Stability of the microstructure of metallic systems. Moscow: Atomizdat, 1978, 280 p.
  20. Reed R.C. The Superalloys. Fundamentals and Applications. Cambridge: University Press, 2006, 372 p.
  21. Gorelik S.S. Recrystallization of metals and alloys. 2nd ed. Moscow: Metallurgiya, 1978, 568 p.
  22. Hardy M.C., Detrois M., Mcdevitt E.T. et al. Solving Recent Challenges for Wrought Ni-Base Superalloys. Metallurgical and Materials Transactions: 50th anniversary collection. Springer, 2020, vol. 51A, pp. 2626–2650.
  23. Novikov I.I. Theory of heat treatment of metals: textbook. 3rd ed., corr. and add. Moscow: Metallurgiya, 1978, 392 p.
  24. Rogozhkin S.V., Ber L.B., Nikitin A.A. et al. Study of granulated nickel alloy by atomic probe tomography. Fizika metallov i metallovedenie, 2020, vol. 121, no. 1, pp. 1‒12.
  25. Barba D., Alabort E., Pedrazzini S. et al. On the microtwinning mechanism in a single crystal superalloy. Acta Materialia, 2017, vol. 135, pp. 314‒329. DOI: 10.1016/j.actamat.2017.05.072.
  26. Smith T.M., Esser B.D., Antolin N. et al. Segregation and η phase formation along stacking faults during creep at intermediate temperatures in Ni-base superalloys. Acta Materialia, 2015, vol. 100, pp. 19‒31. DOI: 10.1016/j.actamat.2015.08.053.
  27. Barba D., Smith T.M., Miao J. et al. Segregation-assisted plasticity in Ni-based superalloys. Metallurgical Materials Transactions, 2018, vol. 49A, pp. 4173−4185. DOI: 10.1007/s11661-018-4567-6.
  28. Smith T.M., Gabb T.P., Wertz K.N. et al. Enhancing the creep strength of next-generation disk superalloys via local phase transformation strengthening. Superalloys 2020. Pennsylvania: Minerals, Metals, Materials Series, 2020, pp. 726–736.
  29. Lilensten L., Antonov S., Gault B. et al. Enhanced creep performance in a polycrystalline superalloy driven by atomic-scale phase transformation along planar faults. Acta Materialia, 2021, vol. 202, pp. 232‒242.
  30. Viswanathan G.B., Sarosi P.M., Henry M.F. et al. Investigation of creep deformation mechanisms at intermediate temperatures in René 88 DT. Acta Materialia, 2005, vol. 53, no. 10, pp. 3041–3057.
  31. Saada G., Veyssiere P. Kear-Wilsdorf locks and mechanical properties of L12 alloys. MRS Online Proceedings Library, 1992, vol. 288, pp. 411−416. DOI: 10.1557/PROC-288-411.
  32. Rae C., Vorontsov V., Kovarik L., Mills M. Dislocations in a Ni-based superalloy during low temperature creep. MATEC Web of Conferences 14. EDP Sciences, 2014, art. 01006. DOI: 10.1051/matecconf/20141401006.
  33. Smith T.M., Unocic R.R., Deutchman H., Mills M.J. Creep deformation mechanism mapping in nickel base disk superalloys. Materials at High Temperatures, 2016, vol. 33, no. 4-5, pp. 372−383. DOI: 10.1080/09603409.2016.1180858.
  34. Wang G., Chen M., Lin Y. et al. Recrystallization nucleation under close-set δ phase in a nickel-based superalloy during annealing. Journal of Materials Science & Technology, 2022, vol. 115, pp. 166–176.
  35. Jena A.K., Chaturvedj M.C. The role of alloying elements in the design of nickel-base superalloys. Journal of Materials Science, 1984, vol. 19, pp. 3121–3139.
  36. Murakumo T., Kobayashi T., Koizumi Y., Harada H. Creep behavior of Ni-base single-crystal superalloys with various γ′ volume fraction. Acta Materialia, 2004, vol. 52, no. 12, pp. 3737–3744.
  37. Unocic R.R., Vismanathan G.B., Sarosi P.M. et al. Mechanisms of creep deformation in polycrystalline Ni-base disk superalloy. Materials Science and Engineering A, 2008, vol. 483–484, pp. 25‒32.
  38. Svetlov I.L., Zaitsev D.V., Karashaev M.M., Epishin A.I., Petrushin N.V. Microsegregation of Alloying Elements on Deformation-Induced Structural Defects in a Granulated Nickel Alloy. Fizika metallov i metallovedenie, 2023, vol. 124, no. 6, pp. 517–523.
  39. Ber L.B., Rogozhkin S.V., Khomich A.A., Zaluzhny A.G. Distribution of alloying element atoms between particles of the γ- and γ′-phases in a heat-resistant nickel alloy. Fizika metallov i metallovedenie, 2022, vol. 123, no. 2, pp. 177‒191.
  40. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), pp. 30–50. Available at: http://www.journal.viam.ru (accessed: December 01, 2025). DOI: 10.18577/2713-0193-2023-0-1-30-50.
  41. Link T., Epishin A., Brückner U., Portella P.D. Increase of misfit during creep of superalloys and its correlation with deformation. Acta Materialia, 2000, vol. 48, no. 8, pp. 1981‒1994. DOI: 10.1016/S1359-6454(99)00456-5.