Budinovskiy S.A., Benklyan A.S., Azarovskiy E.N., Tatarnikov S.V. The effect of substrate electrical potential on the composition and structure of deposited condensate in the ion-plasma process of NiCrAl coating // Proceedings of VIAM. 2026. No. 5 (159). С. 94–102. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-5-94-102.

The effect of substrate electrical potential on the composition and structure of deposited condensate in the ion-plasma process of NiCrAl coating

Budinovskiy S.A., Benklyan A.S., Azarovskiy E.N., Tatarnikov S.V.
Abstract

The results of a study examining the effect of substrate electrical potential in the range from 0 to 150 V on the structure and composition of NiCrAl coatings alloyed with refractory metals (Ta, Hf, and Re) are presented. It is shown that the deposition rate of all three selected coating alloys decreases linearly with increasing substrate electrical potential, reaching zero at approximately 200 V. This is due to the presence of high-energy, multiply charged metal ions in the vacuum arc discharge plasma. The elemental composition of the condensate also changes with increasing substrate electrical potential.

Keywords
heat-resistant nickel alloys, ion-plasma coatings, vacuum arc process
Reference list
  1. Kablov E.N. Science as a branch of the economy. Nauka i zhizn, 2009, no. 10, pp. 6–10.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Muboyadzhyan S.A., Kablov E.N. Ion etching and surface modification of critical machine parts in vacuum-arc plasma. Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie, 2011, no. SP2, pp. 149–163.
  4. Kablov E.N., Muboyadzhyan S.A. Heat-protective coatings with a ceramic layer of low thermal conductivity based on zirconium oxide for high-pressure turbine blades of advanced gas turbine engines. Proceedings of the sc. and tech. conf. «Modern achievements in the field of creating advanced non-metallic composite materials and coatings for aviation and space technology»: in 2 parts. Moscow: VIAM, 2015, part 2, art. 3.
  5. Alexandrov D.A., Gorlov D.S. The Research of erosion resistance and residual stresses in layered ion-plasma coatings. Trudy VIAM, 2022, no. 12 (118), pp. 87–95. Available at: http://www.viam-works.ru (accessed: October 15, 2025). DOI: 10.18577/2307-6046-2022-0-12-87-95.
  6. Doronin O.N., Artemenko N.I., Stekhov P.A., Voronov V.A. Deposition of ceramic layers of heat protection coatings based on the system Gd2O3–ZrO2–HfO2 and Sm2O3–Y2O3–HfO2. Aviation materials and technologies, 2022, no. 3 (68), pp. 108–119. Available at: http://www.journal.viam.ru (accessed: October 15, 2025). DOI: 10.18577/2713-0193-2022-0-3-108-119.
  7. Batraev I.S., Rybin D.K., Ivanyuk K.V., Ulianitsky V.Yu., Shtertser A.A. Wear resistant detonation coatings based on tungsten carbide for aviation products. Aviation materials and technologies, 2022, no. 1 (66), pp. 92–109. Available at: http://www.journal.viam.ru (ассеssed: October 15, 2025). DOI: 18577/2713-0193-2022-0-1-92-109.
  8. Aleksandrov D.A., Artemenko N.I. Wear-resistant coatings to protect friction parts of modern gas turbine engines. Trudy VIAM, 2016, no. 10, pp. 65–72. Available at: http://www.viam-works.ru (accessed: October 15, 2025). DOI: 10.18577//2307-6046-2016-0-10-6-6.
  9. Goncharov B.E., Sipatov A.M., Cherkashneva N.N., Pleskan A.Yu., Samokhvalov N.Yu., Vaganova M.L., Sorokin O.Yu., Solntsev St.S., Evdokimov S.A. Studies of thermal shock resistance of an anti-oxidation coating for a multi-layered ceramic composite. Aviation materials and technologies, 2021, no. 4 (65), pp. 51–58. Available at: http://www.journal.viam.ru (accessed: October 15, 2025). DOI: 10.18577/2713-0193-2021-0-4-51-58.
  10. Budinovskiy S.A., Benklyan A.S., Tatarnikov S.V. Working process features of an ion-plasma installation for applying protective coatings in a high-current vacuum arc discharge with a binary consumable cathode and a partitioned anode. Aviation materials and technologies, 2025, no. 3 (80), pp. 110–120. Available at: http://www.journal.viam.ru (accessed: October 15, 2025). DOI: 10.18577/2713-0193-2025-0-3-110-120.
  11. Method for protecting gas turbine blades: pat. 2404286 Rus. Federation; appl. 22.10.09; publ. 20.11.10.
  12. Method of applying protective coatings and device for its implementation: pat. 2625698 Rus. Federation; appl. 29.08.16; publ. 18.07.17.
  13. Muboyadzhyan S.A. Industrial ion-plasma equipment for applying protective coatings. Entsiklopediya inzhenera-khimika, 2012, no. 5, pp. 34–41.
  14. Muboyadzhyan S.A. Protective coatings for parts of the hot gas turbine tract. Vse materialy. Entsiklopedicheskiy spravochnik, 2011, no. 3, pp. 26–30.
  15. Muboyadzhyan S.A., Budinovsky S.A. MAP-1 industrial installation for applying protective coatings for various purposes. Aviatsionnaya promyshlennost, 1995, no. 7–8, pp. 44–48.