Dubrovin I.M., Manzhosova Е.N., Isaev A.Yu., Lukina N.F. Hot-melt pressure-sensitive adhesives based on styrene-butadiene copolymers: properties and applications // Proceedings of VIAM. 2026. No. 5 (159). С. 42–54. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-5-42-54.

Hot-melt pressure-sensitive adhesives based on styrene-butadiene copolymers: properties and applications

Dubrovin I.M., Manzhosova Е.N., Isaev A.Yu., Lukina N.F.
Abstract

The review examines hot-melt pressure-sensitive adhesives (HMPSA) based on styrene-butadiene-styrene (SBS) thermoplastic elastomers. The influence of microphase separation and block copolymer composition on the rheological parameters-elastic and viscous moduli as well as on the adhesive properties, including tack, shear, and peel strength, is analyzed. Modern HMPSA application methods and their use in aerospace, mechanical engineering, electronics, and related industrial fields are presented.

Keywords
pressure-sensitive adhesives, HMPSA adhesives, thermoplastics, SBS block copolymers, shear strength, peel strength
Reference list
  1. Zuev A.V., Zarichnyak Yu.P., Barinov D.Ya., Krasnov L.L. Measurement of thermophysical properties of flexible thermal insulation. Aviation materials and technology, 2021, no. 1 (62), pp. 119–126. Available at: http://www.journal.viam.ru (accessed: October 07, 2025). DOI: 10.18577/2713-0193-2021-0-1-119-126.
  2. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), pp. 70–80. Available at: http://www.journal.viam.ru (accessed: September 05, 2025). DOI: 10.18577/2713-0193-2021-0-4-70-80.
  3. Aviation Materials: a Handbook in 13 vols. Ed. E.N. Kablov. Moscow: VIAM, 2019, vol. 10: Adhesives, Sealants, Rubbers, Hydraulic Fluids, part 1: Adhesives, Adhesive Prepregs, 276 p.
  4. Lukina N.F., Starodubtseva O.A., Sharova I.A. Properties and Purpose of Self-Adhesive Materials for Aviation Purposes. Novosti materialovedeniya. Nauka i tekhnika, 2016, no. 4 (22), pp. 88‒100. URL: www.materialsnews.ru (accessed: September 05, 2025).
  5. Akhmadieva K.R., Petrova А.P., Shosheva A.L., Bokov V.V. Heat-resistant polyimide adhesive of constructive purposes. Trudy VIAM, 2023, no. 6 (124), pp. 15–24. Available at: http://www.viam-works.ru (accessed: October 07, 2025). DOI: 10.18577/2307-6046-2023-0-6-15-24.
  6. Chaykun A.M., Bobrova I.I., Gerasimov D.M., Sergeyev A.V. Elastomers for sealing harness materials: properties, methods of receiving and feature of manufacturing. Trudy VIAM, 2023, no. 7 (125), pp. 56–68. Available at: http://www.viam-works.ru (accessed: October 07, 2025). DOI: 10.18577/2307-6046-2023-0-7-56-68.
  7. Kozlov I.A., Isaev A.Yu., Lukina N.F., Alekhine A.K., Starodubtseva O.A. Adhesives with permanent tack, pressure-sensitive adhesives, self-adhesive materials. Current state of the art. Part 1. Klei. Germetiki. Tekhnologii, 2024, no. 10, pp. 19–28. DOI: 10.31044/1813-7008-2024-0-10-19-28.
  8. Kozlov I.A., Isaev A.Yu., Lukina N.F., Alekhine A.K., Starodubtseva O.A. Adhesives with permanent tack, pressure-sensitive adhesives, self-adhesive materials. Current state of the art. Part 2. Klei. Germetiki. Tekhnologii, 2024, no. 11, pp. 16–26. DOI: 10.31044/1813-7008-2024-0-11-16-26.
  9. Adhesive composition and self-adhesive material based on it: pat. 2346970 Rus. Federation; appl. 08.11.07; publ. 20.02.09.
  10. Selina A.Yu., Lyusova L.R. Natural rubber in adhesives with «permanent» tack. Klei. Germetiki. Tekhnologii, 2012, no. 3, pp. 13–16.
  11. Adhesive for adhesive tapes: pat. 2185411 Rus. Federation; appl. 13.12.00; publ. 20.07.02.
  12. Maltanava H. Polymer coatings of polystyrene (PSt), polyisobutylene (PIB) and tri block copolymer SIBS on MXene films. Coatings, 2022, vol. 12, p. 1477.
  13. Mnyango J.I., Nyoni B., Mama N. et al. Polybutene, polyisobutylene, and beyond: a comprehensive review of synthesis to sustainability. Materials Advances, 2025, is. 16, pp. 5339–5390.
  14. Polymeric composition containing a hydrogenated block copolymer and tackifier resin: pat. US7442739B1; appl. 11.01.07; publ. 28.10.08.
  15. Hot melt pressure sensitive adhesive composition with intermediate softening point: pat. DE69937111T2; appl. 15.07.99; publ. 12.06.08.
  16. Hot melt pressure sensitive adhesive composition: pat. US6384138B1; appl. 02.09.99; publ. 07.05.02.
  17. High styrene SBS hot melt adhesive: pat. US8163824B2; appl. 22.04.10; publ. 24.04.12.
  18. Adhesive composition: pat. 2593604 Rus. Federation; appl. 03.02.15; publ. 10.08.16.
  19. Pressure-sensitive adhesives: pat. 2208030 Rus. Federation; appl. 18.06.96; publ. 10.07.03.
  20. Adhesive composition for the manufacture of self-adhesive tape: pat. 2466166 Rus. Federation; appl. 22.06.09; publ. 10.11.12.
  21. D-series copolymers for HMPSA by Kraton. Available at: https://kraton.com/products/kraton-d/ (accessed: July 07, 2025).
  22. SEBS tape adhesives by Kraton. Available at: https://www.specialchem.com/adhesives/product/kraton-kraton-d1118-et (accessed: July 04, 2025).
  23. Polymers guide 2024. Kraton A, G, FG series for adhesive applications. Available at: https://kraton.com/products (accessed: July 02, 2025).
  24. Kennedy J.E., Higginbotham C.L. Synthesis and Characterisation of Styrene Butadiene Styrene Based Grafted Copolymers for Use in Potential Biomedical Applications. Bio-medical Engineering: Trends in Materials Science. Rijeka: InTech, 2011, pp. 475–498. DOI: 10.5772/13051.
  25. Ilyin S.O., Melekhina V.Y., Kostyuk A.V., Smirnova N.M. Hot-melt and pressure-sensitive adhesives based on styreneisoprene-styrene triblock copolymer, asphal-tene/resin blend and naphthenic oil. Polymers, 2022, vol. 14, p. 4296. DOI: 10.3390/polym14204296.
  26. O’Connor A.E., Macosko C.W. Melt versus solvent coating: structure and properties of block-copolymer-based. Journal of Applied Polymer Science, 2002, vol. 86 (13), pp. 3355–3367.
  27. Mazzeo F.A. Characterization of Pressure Sensitive Adhesives by Rheology. TA Instruments Report RH082, 2002, no. 1, p. 12.
  28. Hot-melt pressure-sensitive adhesive composition: pat. EP 4368682 A1; appl. 10.11.22; publ. 15.05.24.
  29. Modified epoxy resin film for RFI molding process and preparation method thereof: pat. 101735573 CN; appl. 12.03.09; publ. 30.05.12.
  30. A kind of hot-fusible pressure-sensitive adhesive and preparation method thereof: pat. CN 103694934 A; appl. 09.12.13; publ. 02.04.14.
  31. Hot melt pressure sensitive adhesives for paper labels: pat. WO2008077509A1; appl. 12.04.07; publ. 03.07.08.
  32. Methods for producing silicon nitride films and silicon oxynitride films by thermal chemical vapor deposition: pat. US7192626B2; appl. 24.09.03; publ. 20.03.07.
  33. Process and apparatus for the conversion of sludges: pat. US5865956A; appl. 23.04.98; publ. 02.02.99.
  34. Sherriff M.W. Peel adhesion and viscoelasticity of rubber–resin blends. Journal of Applied Polymer Science, 1980, vol. 18, pp. 2597–2608.