UDC
543.51:669.1
DOI
10.18577/2307-6046-2026-0-3-215-224
Article PDF (Russian)
(769.58 KB)
How to cite
Alekseev A.V., Yakimovitch P.V. Analysis of tungsten by glow discharge high-resolution mass spectrometry // Proceedings of VIAM. 2026. No. 3 (157). С. 215–224. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-3-215-224.
Analysis of tungsten by glow discharge high-resolution mass spectrometry
Abstract
The impurities of 34 elements in tungsten by high-resolution glow discharge mass spectrometry was determined. The sample preparation for analysis is described. In order to achieve maximum analytical signals from all the elements corresponding equipment settings were selected. Spectral interferences were eliminated by using high resolution. Relative sensitivity coefficients for all determined elements were calculated using X-ray fluorescence spectroscopy.
Keywords
high resolution glow discharge mass spectrometry, tungsten, nickel alloys, determination of harmful impurities
Reference list
- Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
- Min P.G., Vadeev V.E., Kramer V.V. The development of the new VZhM200 superalloy and the technology of its production for casting of the advanced engines’ blades by the directional crystallization. Aviation materials and technologies, 2021, no. 3 (64), pp. 11–18. Available at: http://www.journal.viam.ru (accessed: June 11, 2025). DOI: 10.18577/2713-0193-2021-0-3-11-18.
- Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crystallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), pp. 3–12. Available at: http://www.viam-works.ru (accessed: June 11, 2025). DOI: 10.18577/2307-6046-2020-0-3-3-12.
- Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), pp. 30–50. Available at: http://www.journal.viam.ru (accessed: June 11, 2025). DOI: 10.18577/2713-0193-2023-0-1-30-50.
- Gromov V.I., Yakusheva N.A., Vostrikov A.V., Cherkashneva N.N. High strength structural steels for gas-turbine engine shafts (review). Aviation materials and technology, 2021, no. 1 (62), pp. 3‒12. Available at: http://www.journal.viam.ru (accessed: June 11, 2025). DOI: 10.18577/2713-0193-2021-0-1-3-12.
- Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level CRMs and MI. Kompetentnost, 2017, no. 2, pp. 40–46.
- State Standard 14339.3–91. Tungsten. Methods for determination of phosphorus content. Moscow: Publ. house of standards, 1991, pp. 3–6.
- State Standard 14339.2–82. Tungsten. Methods for determination of sulfur content. Moscow: Publ. house of standards, 1982, pp. 1–3.
- State Standard 14339.5–91. Tungsten. Methods of spectral analysis. Moscow: Publ. house of standards, 1991, pp. 2–4.
- ASTM B890–20. Standard test method for determination of metallic constituents of tungsten alloys and tungsten hardmetals by X-Ray fluorescence spectrometry. ASTM International, 2012, рр. 1–5.
- Brenner I., Erlich S., Vial G. et al. Direct trace element analysis of tungsten powders, alloys and related materials by inductively coupled plasma atomic emission spectrometry (ICP-AES). Journal of Analytical Atomic Spectrometry, 1987, vol. 2, pp. 637–644.
- Hu J., Wang H. Determination of Trace Elements in Super Alloy by ICP-MS. Mikrochimica Acta, 2001, vol. 137, pp. 149–155.
- Pupyshev A.A., Epova E.N. Spectral interference of polyatomic ions in the method of mass spectrometry with inductively coupled plasma. Analitika i kontrol, 2001, vol. 5, no. 4, pp. 335–369.
- Medvedev N., Volzhenin A., Saprykin A. Determination of trace elements in high-purity tungsten by electrothermal vaporization inductively coupled plasma mass spectrometry. Microchemical Journal, 2020, vol. 157, pp. 1–8.
- Jakubowski N., Prohaska T., Rottmann L., Vanhaecke F. Inductively coupled plasma- and glow discharge plasma-sector field mass spectrometry. Part I. Tutorial: Fundamentals and instrumentation. Journal of Analytical Atomic Spectrometry, 2011, vol. 26, pp. 693–726.
- Ganeev A.A., Gubal A.R., Uskov K.N., Potapov S.V. Analytical mass spectrometry with glow discharge. Izvestiya Akademii nauk. Seriya khimicheskaya, 2012, no. 4, pp. 1–15.