Ryzhkov P.V., Gorbovets M.A. Numerical model for predicting fatigue life under conditions of initial surface roughness of nickel alloy obtained by additive technological processes // Proceedings of VIAM. 2026. No. 3 (157). С. 183–202. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-3-183-202.

Numerical model for predicting fatigue life under conditions of initial surface roughness of nickel alloy obtained by additive technological processes

Ryzhkov P.V., Gorbovets M.A.
Abstract

A numerical fatigue damage model for the nickel-based alloy VZh159 SLS was developed, accounting stochastic surface roughness and implementing a two-stage approach. The predicted fatigue life at Δε = 0.5 % and an elliptical crack with a ratio a/b = 2 was 7,725 cycles (–19 % error) compared to the experiment; at Δε = 0.4 % and a/b = 1: 23,043 cycles (–8 % error). A method for generating surface topography based on the spectral attenuation of periodic functions is proposed.

Keywords
material fatigue, nickel alloy VZh159 SLS, additive manufacturing, surface roughness, numerical modeling, Smith–Watson–Topper (SWT) parameter, Paris’ law, finite element method, microcracks, damage model
Reference list
  1. Evgenov A.G., Ryzhkov P.V., Shurtakov S.V., Malinin R.Yu. Influence of the Surface Element Exposure Algorithm in Selective Laser Melting on the Mechanical Properties of the Synthesized Material. Part 1. Short-Term and Long-Term Strength. Deformatsiya i razrusheniye materialov, 2023, no. 10, pp. 10–18. DOI: 10.31044/1814-4632-2023-10-10-18.
  2. Evgenov A.G., Ryzhkov P.V., Shurtakov S.V., Malinin R.Yu. Influence of the Surface Element Exposure Algorithm in Selective Laser Melting on the Mechanical Properties of the Synthesized Material. Part 2. Fatigue. Deformatsiya i razrusheniye materialov, 2023, no. 11, pp. 2–12. DOI: 10.31044/1814-4632-2023-11-2-12.
  3. Kablov E.N., Evgenov A.G., Petrushin N.V. On the Mechanism of Fine Track Structure Formation in Selective Laser Melting. Metallovedeniye i termicheskaya obrabotka metallov, 2023, no. 2 (812), pp. 44–55. DOI: 10.30906/mitom.2023.2.44-55.
  4. Kablov E.N., Evgenov A.G., Petrushin N.V. New Generation Materials and Digital Additive Technologies for the Production of Resource Parts by FSUE VIAM. Part 3. Adaptation and Creation of Materials. Electrometallurgiya, 2022, no. 4, pp. 15–25. DOI: 10.31044/1684-5781-2022-0-4-15-25.
  5. Kablov E.N., Evgenov A.G., Bakradze M.M. New-generation materials and digital additive technologies for the production of resource parts at FSUE VIAM. Part 1. Materials and synthesis technologies. Electrometallurgiya, 2022, no. 1, pp. 2–12. DOI: 10.31044/1684-5781-2022-0-1-2-12.
  6. Kablov E.N., Evgenov A.G., Petrushin N.V. New-generation materials and digital additive technologies for the production of resource parts at FSUE VIAM. Part 4. Development of heat-resistant materials. Electrometallurgiya, 2022, no. 5, pp. 8–19. DOI: 10.31044/1684-5781-2022-0-5-8-19.
  7. Kartashev M.M. Fatigue Strength of Structures: Textbook. Moscow: Mashinostroenie, 2006, 384 p.
  8. Nezhadfar P., Shamsaei N., Daniewicz S.R., Moser R.D. Damage tolerant design of additively manufactured metallic components subjected to cyclic loading: State of the art and challenges. Materials, 2021, no. 14 (16), art. 4502. DOI: 10.3390/ma14164502.
  9. Noll C.J., Lipson C. Fatigue endurance of steels as influenced by surface condition and hardness. Society for Experimental Stress Analysis, 1946, vol. 3, no. 2, p. 29.
  10. Marin J. Mechanical Behavior of Engineering Materials. New York: McGraw-Hill, 1962, 671 p.
  11. Analytical Strength Assessment of Components in Mechanical Engineering: in 2 parts. Frankfurt am Main: VDMA-Verlag, 1994, FKM-Issue no. 183, part 2: Guideline, 234 p.
  12. Itoga H., Tokaji K., Nakajima M., Ko H.-N. Effect of surface roughness on step-wise S-N characteristics in high strength steel. International Journal of Fatigue, 2003, vol. 25, no. 5, pp. 379–385. DOI: 10.1016/S0142-1123(02)00166-4.
  13. Maiya P.S., Busch D.E. Effect of surface roughness on low-cycle fatigue behavior of type 304 stainless steel. Metallurgical Transactions A, 1975, vol. 6, pp. 1761–1766. DOI: 10.1007/BF02642305.
  14. Sonsino C.M. Course of SN-curves especially in the high-cycle fatigue regime with regard to component design and safety. International Journal of Fatigue, 2007, vol. 29, no. 12, pp. 2246–2258.
  15. McKelvey S.A., Fatemi A. Surface finish effect on fatigue behavior of forged steel. International Journal of Fatigue, 2012, vol. 36, no. 1, pp. 130–145. DOI: 10.1016/j.ijfatigue.2011.08.008.
  16. Shareef I., Hasselbusch M.D. Endurance limit modifying factors for hardened machined surfaces: SAE Technical Paper No. 961054. Warrendale, PA: SAE International, 1996, pp. 1–12.
  17. Moussaoui K., Mousseigne M., Senatore J., Chieragatti R. The effect of roughness and residual stresses on fatigue life time of an alloy of titanium. International Journal of Advanced Manufacturing Technology, 2015, vol. 78, pp. 557–563. DOI: 10.1007/s00170-014-6596-7.
  18. Zhang J., Fatemi A. Surface roughness effect on multiaxial fatigue behavior of additive manufactured metals and its modeling. Theoretical and Applied Fracture Mechanics, 2019, vol. 103, art. 102260. DOI: 10.1016/j.tafmec.2019.102260.
  19. Gunther J., Beretta S., Romano S. et al. A comparison of fatigue strength sensitivity to defects for materials manufactured by AM or traditional processes. International Journal of Fatigue, 2017, vol. 98, pp. 178–191. DOI: 10.1016/j.ijfatigue.2017.01.001.
  20. Greitemeier D., Palm F., Holzweissig J. et al. Fatigue strength of additively manufactured Ti‒6Al‒4V: surface roughness as dominant factor. International Journal of Fatigue, 2019, vol. 124, pp. 380–388. DOI: 10.1016/j.ijfatigue.2019.03.025.
  21. Neuber H. Theory of stress concentration for shear-strained prismatic bodies with arbitrary nonlinear stress-strain law. Journal of Applied Mechanics, Transactions of the ASME, 1961, vol. 28, pp. 544–550.
  22. Topper T.H., Wetzel R.M., Morrow J. Neuber’s Rule Applied to Fatigue of Notched Specimens: Report No. NAEC-ASL-1114. Philadelphia, PA: U.S. Naval Air Engineering Center, 1967, 44 p.
  23. Zhu X., Dong Z., Zhang Y., Cheng Z. Fatigue life prediction of machined specimens with the consideration of surface roughness. Materials, 2021, vol. 14, art. 5420. DOI: 10.3390/ma14185420.
  24. Murakami Y., Endo M. A geometrical parameter for the quantitative estimation of the effects of small defects on fatigue strength of metals. Transactions of the Japan Society of Mechanical Engineers, Series A, 1983, vol. 49, no. 438, pp. 127–136.
  25. Murakami Y., Tsutsumi K., Fujishima M. Quantitative evaluation of effect of surface roughness on fatigue strength (Effect of depth and pitch of roughness). Transactions of the Japan Society of Mechanical Engineers, Series A, 1996, vol. 62, no. 597, pp. 1124–1131. DOI: 10.1299/kikaia.62.1124.
  26. Liu Y., Li X., Maeda Y. Fatigue failure initiation modeling in AA7075-T651 using microstructure-sensitive continuum damage mechanics combined with crystal plasticity FE modelling. Journal of Failure Analysis and Prevention, 2015, vol. 15, pp. 701–710. DOI: 10.1007/s11668-015-0005-x.
  27. Rojas-Garnica J.C., Bedolla-Hernández J., Szwedowicz-Wasik D. Failure by deformation in the lateral contact between sinusoidal asperities. Tribology-Materials, Surfaces & Interfaces, 2016, vol. 10, no. 2, pp. 106–115. DOI: 10.1177/1687814016647252.
  28. Pavliček P., Soubusta J., Hýbl O. White-light interferometry on rough surfaces: measurement uncertainty caused by surface roughness. Applied Optics, 2003, vol. 42, no. 10, pp. 1809–1813. DOI: 10.1364/AO.42.001809.
  29. Singh K., Sadeghi F., Correns M., Blass T. A microstructure based approach to model effects of surface roughness on tensile fatigue. International Journal of Fatigue, 2019, vol. 129, art. 105229. DOI: 10.1016/j.ijfatigue.2019.105229.
  30. Li C., Dai W., Du F. Fatigue life estimation of medium-carbon steel with different surface roughness. Applied Sciences, 2017, vol. 7, no. 4, art. 338. DOI: 10.3390/app7040338.
  31. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  32. Kyarimov R.R., Smelov V.G., Alekseev V.P. Study of the structure and mechanical properties of samples obtained by selective laser melting from metal powder of heat-resistant alloy VZh159 (KhN58MBYu). Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2023, vol. 25, no. 4, pp. 36–46. DOI: 10.37313/1990-5378-2023-25-4-36-46.
  33. Evgenov A.G., Bazyleva O.A., Golovlev N.A., Zaitsev D.V. Features of structure and property of alloys on the basis of Ni3Al intermetallic compound, half-scientists method SLM. Trudy VIAM, 2018, no. 12 (72), pp. 25–36. Available at: http://www.viam-works.ru (accessed: December 10, 2024). DOI: 10.18577/2307-6046-2018-0-12-25-36.
  34. Ospennikova O.G., Naprienko S.A., Medvedev P.N., Zaitsev D.V., Rogalev A.M. Features of the formation of the structural-phase state of the EP648 alloy during selective lase manufacture. Trudy VIAM, 2021, no. 8 (102), pp. 3–11. Available at: http://www.viam-works.ru (accessed: December 10, 2024). DOI: 10.18577/2307-6046-2021-0-8-3-11.
  35. Erasov V.S., Oreshko E.I. Fatigue tests of metal materials (review). Part 1. Main definitions, loading parameters, representation of results of tests. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 59‒70. DOI: 10.18577/2071-9140-2020-0-4-59-70.
  36. Erasov V.S., Oreshko E.I. Tests for fatigue of metal materials (review). Part 2. Analysis of the Basquin–Manson–Coffin equation. Methods of testing and processing of results. Aviation materials and technology, 2021, no. 1 (62), pp. 80–94. Available at: http://www.journal.viam.ru (accessed: December 10, 2024). DOI: 10.18577/2713-0193-2021-0-1-80-94.
  37. Электронная справка по моделированию структурной механики Comsol Multiphysics. Available at: https://www.comsol.com (accessed: December 12, 2024).
  38. Feng X., Wang J., Gao R. Fatigue life prediction of machined specimens with the consideration of surface roughness. Materials, 2021, vol. 14, no. 18, art. 5420. DOI: 10.3390/ma14185420.
  39. Ryzhkov P.V., Gorbovets M.A., Hodinev I.A. Energy criteria for fatigue fracture of a heat-resistant nickel alloy. Trudy VIAM, 2023, no. 11 (129), pp. 111–122. Available at: http://www.viam-works.ru (accessed: June 01, 2025). DOI: 10/18577/2713-0193-2025-0-1-72-87.
  40. Ryzhkov P.V., Gorbovets M.A., Hodinev I.A. Determination of the parameters of the plasticity model under cyclic loading of a heat-resistant nickel alloy at elevated temperatures. Aviation materials and technologies, 2025, no. 1 (78), pр. 72–87. Available at: http://www.journal.viam.ru. (accessed: June 06, 2025). DOI: 10.18577/2713-0193-2025-0-1-72-87.
  41. Ryzhkov P.V., Gorbovets M.A., Evgenov A.G. Development of damage from the exposed surface of a nickel alloy obtained by additive technological processes. XVII All-Rus. Conf. on Testing and Research of Material Properties «TestMat» on the topic «Physical and Mechanical Testing, Strength and Reliability of Modern Structural and Functional Materials»: Coll. Conf. Moscow: NRC «Kurchatov Institute» – VIAM, 2025, pp. 214–278.