Balinova Yu.A., Stepanova E.V., Babashov V.G., Bondarenko E.S., Kulikova E.S., Prutskov G.V. Investigation of the properties of oxide monofilaments // Proceedings of VIAM. 2026. No. 2 (156). С. 84–93. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-2-84-93.

Investigation of the properties of oxide monofilaments

Balinova Yu.A., Stepanova E.V., Babashov V.G., Bondarenko E.S., Kulikova E.S., Prutskov G.V.
Abstract

Using X-ray microdiffraction and microfluorescence methods, as well as electronography methods, the processes of structure formation in oxide monofilaments under the influence of temperature were studied. It was shown that the main phase of the studied samples is mullite. Research shows that all samples demonstrate the uniform phase composition during the monofilament length. The investigation shows pronounced grain structure with elongated crystallites, that have the mullite habitus. The grains demonstrate homogeneous distribution.

Keywords
monofilaments, phase composition, X-ray diffraction, electron microscopy, trace element analysis, length, distribution
Reference list
  1. Kablov E.N. The Role of Fundamental Research in the Creation of Next-Generation Materials. Reports of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  2. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and Technological Development of Russia in the Context of Achieving National Goals: Problems and Solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  3. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122–144. Available at: http://www.journal.viam.ru (accessed: December 22, 2024). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  4. Ivakhnenko Yu.A., Kuzmin V.V., Bespalov A.S. Status and development prospects of heat and sound insulating fireproof materials. Problemy bezopasnosti poletov, 2014, no. 7, pp. 27–30.
  5. Wei W.Ch., Halloran J.W. Transformation Kinetics of Diphasic Alluminisilicate Gels. Journal of American Ceramic Society, 1988, vol. 71, pp. 581–587.
  6. High Performance Synthetic Fibers for Composites: Report. Washington, DC: National Academy Press, 1992, 148 p.
  7. Ceramic Matrix Composites: Fiber Reinforced Ceramics and their Applications. Ed. W. Krenkel. Wiley-VCH, 2008, 440 p.
  8. Buchilin N.V., Maksimov V.G., Babashov V.G. Ceramic filters for aluminum melt (review). Steklo i keramika, 2015, no. 7, pp. 20–28.
  9. Balinova Yu.A., Lugovoy A.A., Butakov V.V. Application trends of high temperature refractory oxides for solid oxides fuel cells. Trudy VIAM, 2024, no. 8 (138), pp. 48–63. Available at: http://www.viam-works.ru (accessed: December 11, 2024). DOI: 10.18577/2307-6046-2024-0-8-48-63.
  10. Maksimov V.G., Varrik N.M., Babashov V.G. Features of obtaining ceramic materials from sintering-active powders. Novye ogneupory, 2023, no. 10, pp. 14–21.
  11. Lebedeva Yu.E., Shchegoleva N.E., Voronov V.A., Solntcev S.S. Al2O3 and ZrO2 ceramic materials obtained by sol-gel method. Trudy VIAM, 2021, no. 4 (98), pp. 61–73. Available at: http://www.viam-works.ru (accessed: December 11, 2024). DOI: 10.18577/2307-6046-2021-0-4-61-73.
  12. Voronov V.A., Chainikova A.S., Lebedeva Yu.E., Tkalenko D.M. Influence of morphology, phase composition and content of aluminum oxide particles on rheological properties of aqueous suspensions based on them. Aviation materials and technologies, 2021, no. 4 (65), pp. 14–25. Available at: http://www.journal.viam.ru (accessed: December 16, 2024). DOI: 10.18577/2713-0193-2021-0-4-14-25.
  13. Non-frangible alumina-silica fibers: pat. US4047965A; appl. 04.05.76; publ. 13.09.77.
  14. Process for producing alumina fiber or alumina-silica fiber: pat. US4101615A; appl. 20.02.73; publ. 18.07.78.
  15. Process for producing alumina-based fiber: pat. US5002750A; appl. 19.09.89; publ. 26.03.91.
  16. Jia Y., Cao Xu, Jiao X., Chen D. Preparation of Alumina Ceramic Continuous Fibers with Inorganic Acid Aluminium Sol as Precursor. Journal of Inorganic Materials, 2023, vol. 38, pp. 1257–1264. DOI: 10.15541/jim20230153.
  17. Continuous process for producing long α-Alumina fibers: pat. US 4812271; appl. 04.09.87; publ. 14.03. 89.
  18. Technology of preparing aluminium oxide based continuous fibers by sol-gel process: pat. 101717257 CN; appl. 01.12.09; publ. 02.06.10.
  19. Technology of preparing aluminium oxide based continuous fibers by sol-gel process: pat. 101717258 CN; appl. 01.12.09; publ. 02.06.10.
  20. Process for preparing alumina-based continuous fiber with sol-gel method: pat. 101723682 CN; appl. 01.12.09; publ. 09.06.10.
  21. Alumina based long fiber containing mullite crystal phase, and preparation method thereof: pat. 102358697 CN; appl.18.07.11; publ. 22.02.12.
  22. Method for preparing alumina-based continuous fibers by using SiO2 nanopowder raw material: pat. 102351516 CN; appl. 06.07.11; publ. 15.02.12.
  23. Preparation method of alumina-based continuous long fiber containing mullite whisker second phase: pat. 102978745 CN; appl. 28.11.12; publ. 20.03.13.
  24. Tan H., Guo C. Preparation of long alumina fibers by sol-gel method using malic acid. Transactions of non-ferrous metals society of China, 2011, vol. 21, pp. 1563–1567.
  25. Zhang Y., Xiao C., An S. et al. Characterization of Defects of Mullite Fibers Prepared by Polyvinyl Butyral as Spinning Aid. Science of Sintering, 2010, vol. 42, pp. 203–210.
  26. Zhang Y., Ding Y., Gao J., Yang J. Mullite fibres prepared by sol-gel method using polyvinylbutyral. Journal of the European Ceramic Society, 2009, vol. 29, no. 6, pp. 1101–1107.
  27. Technology for preparing alumina-based continuous fibers by using inorganic aluminum salts: pat. 102180656 CN; appl. 22.02.11; publ. 14.09.11.
  28. Preparation method of aluminum oxide ceramic continuous fiber: pat. 102965764 CN; appl. 13.11.12; publ. 13.03.13.
  29. Svetogorov R., Dorovatovskii P., Lazarenko V. Belok/XSA Diffraction Beamline for Study Crystilline Samplеs at Kurchatov Synchrotron Radiation Source. Crystal Research and Technology, 2020, vol. 55 (5), art. 1900184. DOI: 10.1002/crat.201900184.