Movenko D.A., Zaysev D.V. Calculated estimation of the structural-phase and thermodynamic characteristics of the VZhM1, VZhM4 and VZhM8 alloys // Proceedings of VIAM. 2026. No. 2 (156). С. 13–26. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-2-13-26.

Calculated estimation of the structural-phase and thermodynamic characteristics of the VZhM1, VZhM4 and VZhM8 alloys

Movenko D.A., Zaysev D.V.
Abstract

The article presents the results of a comparative study of the lattice parameters of the γ- and γ'-phases, the γ/γ'-misfit, γ'-solvus temperature, interfacial energy at the γ/γ' boundary and the antiphase boundary energy of single-crystal superalloys of the third to fifth generation. The focus was made on the dependence of these characteristics on the temperature and composition of the alloys. The calculations were carried out using thermodynamic modeling. It was found that the VZhM8 alloy has the highest values of misfit and γ'-solvus temperature; the VZhM4 alloy has the lowest interfacial energy at the γ/γ' boundary; the VZhM1 alloy has the highest antiphase boundary energy.

Keywords
Ni-based superalloys, single crystals, lattice parameters, misfit, solvus temperature, interfacial energy, antiphase boundary energy
Reference list
  1. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G. The metallurgical fundamentals for high quality maintenance of single crystal heat-resistant nickel alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 55–71. DOI: 10.18577/2071-9140-2017-0-S-55-71.
  2. Movenko D.A., Zavodov A.V., Laptev A.B., Loshchinina A.O. Changes in the structure of the VZhM4-VI alloy during high-temperature salt corrosion at 750 °C. Metallovedenie i termicheskaya obrabotka metallov, 2024, no. 5 (827), pp. 22–29.
  3. Movenko D.A., Shurtakov S.V. Microcrack formation and controlling in nickel superalloys processed by selective laser melting (review). Aviation materials and technologies, 2022, no. 2 (67), paper no. 04. Available at: http://www.journal.viam.ru (accessed: May 13, 2025). DOI: 10.18577/2713-0193-2022-0-2-43-51.
  4. Epishin A.I., Lisovenko D.S. Determination of isothermal elasticity constants of a single-crystal nickel-based superalloy in a wide temperature range. Aviation materials and technologies, 2024, no. 2 (75), pp. 122–136. Available at: http://www.journal.viam.ru (accessed: May 13, 2025). DOI: 10.18577/2713-0193-2024-0-2-122-136.
  5. Movenko D.A., Laptev A.B., Zagorskikh O.A. Study of the composition and morphology of hot salt corrosion products of heat-resistant nickel alloys. Voprosy materialovedeniya, 2021, no. 1 (105), pp. 107–115.
  6. Treninkov I.A., Petrushin N.V., Epishin A.I., Svetlov I.L., Nolze G., Elyutin E.S. Experimental determination of the temperature dependence of the structural-phase parameters of a nickel heat-resistant alloy. Materialovedenie, 2021, no. 7, pp. 3–12.
  7. Epishin A.I., Petrushin N.V., Svetlov I.L., Nolze G. Model for predicting the temperature dependence of γ/γʹamisfite in heat-resistant nickel alloys. Materialovedenie, 2021, no. 3, pp. 9–18.
  8. Chuang H., Liu L., Huang T. et al. The effects of misfit and diffusivity on γʹ rafting in Re and Ru containing Nickel based single crystal super-alloys – details in thermodynamics and dynamics. Vacuum, 2021, vol. 183, pp. 1–9.
  9. Goodfellow A., Owen L.R., Christofidou K.A. et al. The effect of temperature and Mo content on the lattice misfit of model Ni-based superalloys. Metals, 2019, vol. 9, is. 6, pp. 1–9.
  10. Petrushin N.V., Epishin A.I., Svetlov I.L., Nolze G., Elyutin E.S., Soloviev A.E. Influence of the sign of γ/γʹ-misfit on the structure and long-term strength of single crystals of nickel-based heat-resistant alloys. Materialovedenie, 2022, no. 3, pp. 17–26.
  11. Ren Y., Hu T., Xu S. et al. Rapid estimation of γʹ solvus temperature for composition design of Ni-based superalloy via physics-informed generative artificial intelligence. Journal of alloys and metallurgical systems, 2024, vol. 6, ID: 100073.
  12. Horst O.M., Schmitz D., Schreuer J. et al. Thermoelastic properties and γʹ-solvus temperature of single-crystal Ni-base superalloys. Journal of Materials Science, 2021, vol. 56, pp. 7637–7658.
  13. Wang C., Chen X., Chen Y. et al. Accelerated design of high γʹ solvus temperature and yield strength cobalt-based superalloy based on machine learning and phase diagram. Frontiers in Materials, 2022, vol. 9, ID: 882955.
  14. Caron P. High γʹ solvus new generation nickel-based superalloys for single crystal turbine blade applications. Superalloys 2000. TMS, 2000, pp. 737–746.
  15. Liang S.X., Liu K.Y., Zhou Y.X. et al. Interfacial energy between γ/γʹ phases of Ni-Al alloys extracted by using a new method. Materials Chemistry and Physics, 2022, vol. 277, ID: 125538.
  16. Ardell A.J. Temperature dependence of the γ/γʹ interfacial energy in binary Ni-Al alloys. Metallurgical and Materials Transactions A, 2021, vol. 52, pp. 5182–5199.
  17. Zhuang X., Antonov S., Li L., Feng Q. Effect of alloying elements on the coarsening rate of γʹ precipitates in multi-component CoNi-based superalloys with high Cr content. Scripta Materialia, 2021, vol. 202, ID: 114004.
  18. Kar S., Bagui S., Mahato B. et al. Coarsening behavior of γʹ precipitates in high Fe containing Ni-Fe‒Cr-based medium entropy alloy. Metallurgical and Materials Transactions A, 2024, vol. 55, pp. 2609–2615.
  19. Zhang J., Huang T., Lu F. et al. The effect of rhenium on the microstructure stability and γ/γʹ interfacial characteristics of Ni-based single crystal superalloys during long-term aging. Journal of alloys and compounds, 2021, vol. 876, ID: 160114.
  20. Dodaran M., Hemmasian Ettefagh A., Guo S.M. et al. Effect of alloying elements on the γʹ antiphase boundary energy in Ni-base super-alloys. Intermetallics, 2020, no. 117, ID: 106670.
  21. Vamsi K.V., Karthikeyan S. Modeling APB energies in multicomponent Ni-base superalloys. Intermetallics, 2021, no. 132, ID: 107124.
  22. Chen E., Tamm A., Wang T. et al. Modeling antiphase boundary energies of Ni3Al-based alloys using automated density functional theory and machine learning. Computational Materials, 2022, vol. 8, is. 1, ID: 80.
  23. Chen Y., Han J., Yang C. et al. Coupling effect of Ni and Ta on the antiphase boundary energy in γʹ phase of CoNi-based superalloys. Materials Today Communications, 2025, vol. 46, ID: 112600.
  24. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), pp. 30–50. Available at: http://www.journal.viam.ru (accessed: May 13, 2025). DOI: 10.18577/2713-0193-2023-0-1-30-50.
  25. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaev M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 2. Aviation materials and technologies, 2023, no. 2 (71), pp. 3–22. Available at: http://www.journal.viam.ru (accessed: May 13, 2025). DOI: 10.18577/2713-0193-2023-0-2-3-22.