Mishagin K.A., Gotlieb E.M., Valeeva A.R., Yamaleeva E.S. Epoxy materials filled with synthetic wollastonite based on zeolite-containing siliceous rock // Proceedings of VIAM. 2026. No. 2 (156). С. 107‒116. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-2-107-116.

Epoxy materials filled with synthetic wollastonite based on zeolite-containing siliceous rock

Mishagin K.A., Gotlieb E.M., Valeeva A.R., Yamaleeva E.S.
Abstract

The use of synthesized wollastonite (the main component being β-wollastonite) based on zeolite siliceous rock enables the production of epoxy compositions with high tribotechnical properties, hardness, wear resistance and adhesive strength to steel. Calcium silicate from zeolite-containing siliceous rock increases the chemical and thermal resistance of epoxy materials as well as their resistance to UV radiation, making it a promising material for use in the aviation industry.

Keywords
epoxy compositions, zeolite-containing siliceous rock, synthetic wollastonite, wear resistance, hardness, antifriction properties, adhesion to steel
Reference list
  1. Semenukha O.V., Voronina S.Yu. Features of Using Epoxy Resins in the Manufacture of Composite Materials for Antenna Reflectors. Aktualnye problemy aviatsii i kosmonavtiki, 2020, vol. 1, pp. 352–353.
  2. Turanov R.A. Composite Materials Using Boron in Aircraft Manufacturing. Sovremennye naukoyemkiye tekhnologii, 2013, no. 8–2, pp. 230–231.
  3. Kovrizhkina N.A., Kuznetsova V.A., Silaeva A.A., Marchenko S.A. Ways to improve the properties of paint coatings by adding different fillers (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 41–48. DOI: 10.18577/2071-9140-2019-0-4-41-48.
  4. Gladun V.D., Akateva L.V., Andreeva N.N., Kholkin A.I. Production and application of synthetic wollastonite from natural and man-made raw materials. Khimicheskaya tekhnologiya, 2004, no. 9, pp. 4–11.
  5. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122–144. Available at: http://www.journal.viam.ru (accessed: March 05, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  6. Evdokimov S.A., Shchegoleva N.E., Kachaev A.A. Methods for joining ceramic composite materials based on SiC with ceramic and metallic materials (review). Aviation materials and technologies, 2022, no. 3 (68), pp. 75–83. Available at: http://www.journal.viam.ru (accessed: June 08, 2025). DOI: 10.18577/2713-0193-2022-0-3-75-83.
  7. Garshin A.P., Nilov A.S., Galinskaya O.O., Krasnov V.I. Prospects for development and ways to improve aircraft braking systems on the base ceramic matrix composite materials (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 104–121. Available at: http://www.journal.viam.ru (accessed: March 05, 2025). DOI: 10.18577/2713-0193-2023-0-2-104-121.
  8. Sharafiev D.R., Khatsrinov A.I. Analysis of consumer properties of natural zeolites in the CIS countries. Vestnik tekhnologicheskogo universiteta, 2016, vol. 19, no. 12, pp. 95–98.
  9. Morozov N.M., Khokhryakov O.V., Morozova N.N., Khozin V.G., Sagdatullin D.G. Efficiency of zeolite-containing marls in cement concretes. Izvestiya KGASU, 2011, no. 3 (17), pp. 134–138.
  10. Mishagin K.A., Tverdov I.D., Gotlib E.M. et al. Study of natural domestic raw materials for the production of silicate fillers. Yuzhno-Sibirskiy nauchnyy vestnik, 2022, no. 3, pp. 67–73.
  11. Mishagin K., Gotlib E., Yamaleeva E. et al. Comparison of the Properties of Calcium Silicates Derived from Different Raw Materials. E3S Web of Conferences, 2023, vol. 410, pp. 1–8. DOI: 10.1051/e3sconf/202341001001.
  12. Kolesnikov V.I., Bardushkin V.V., Lapitsky A.V. et al. Effective elastic characteristics of antifriction composites on an epoxy basis. Vestnik Yuzhnogo nauchnogo tsentra RAN, 2010, vol. 6, no. 1, pp. 5–10.
  13. Karimov N.K., Ganiev I.N., Olimov N.S. Study of the influence of the main factors on the physicochemical properties of composite epoxy materials used as antifriction and anticorrosion coatings. Doklady akademii nauk Respubliki Tadzhikistan. Ser.: Kompozitsionnyye materialy, 2008, vol. 51, no. 9, pp. 685–689.
  14. Okonkwo A.O., Jagadale P., GarcíaHerrera J.E. et al. High-toughness/low-friction epoxy coating forced with carbonnano structures. Polymer Testing, 2015, vol. 47, pp. 113–119.
  15. Bakhareva V.E., Nikolaev G.I., Anisimov A.V. Improving the functional properties of antifriction polymer composites for sliding friction units. Zhurnal Rossiyskogo khimicheskogo obshchestva im. D.I. Mendeleyeva, 2009, vol. LIII, no. 4. pp. 4–18.
  16. Gotlib E.M., Yamaleeva E.S., Valeeva A.R. et al. Antifriction epoxy materials filled with silicates based on fossil, plant, and technogenic raw materials. Polzunovskiy vestnik, 2024, no. 1, pp. 214–223.
  17. Kuskov V.N., Kolenchin N.F., Shadrina P.N., Safronov A.V. Structure and properties of the anodic oxide film on aluminum and D16 alloy. Fundamentalnye issledovaniya, 2012, no. 11-3, pp. 625–629.
  18. Keishi N., Michiyuki Y., Yoshihide A. Tensile properties of cristobalite-filled epoxy resin. Journal of Applied Polymer Science, 2020, vol. 138 (16), p. 50410.
  19. Arjmandi R., Hassan A., Majeed K., Zakaria Z. Rice Husk Filled Polymer Composites. International Journal of Polymer Science, 2015, vol. 2, pp. 798–829.
  20. Deev I.S., Kurshev E.V., Lonskiy S.L., Zhelezina G.F. The influence of long-term climatic aging on the surface microstructure of epoxy organoplastics and the nature of its destruction under bending conditions. Voprosy materialovedeniya, 2016, vol. 87, no. 3, pp. 104–114.
  21. Pavlov M.R., Nikolaev E.V., Andreeva N.P., Barbotko S.L. To question of technique of assessment of firmness of polymeric materials to influence of solar radiation (review). Trudy VIAM, 2016, no. 7, pp. 98–112. Available at: http://www.viam-works.ru (accessed: March 06, 2025). DOI: 10.18577/2307-6046-2016-0-7-11-11.
  22. Wang H., Liu Z., Luo S. et al. Preparation and properties of UV curable SiO2/Epoxy resin composite. 23rd International Conference on Electronic Packaging Technology (ICEPT). Dalian, China, 2022, pp. 1–4. DOI: 10.1109/ICEPT56209.2022.9872589.
  23. Kablov E.N. Materials and chemical technologies for Aircraft Engineering. Herald of the Russian Academy of Sciences, 2012, vol. 82, no. 3, pp. 158–167.
  24. Babinova A.A., Knyazev A.V., Belyachenkov I.O., Sorokin O.Yu. Testing the resistance of ceramics materials to high temperatur corrosion at a temperature of 900 °C. Aviation materials and technologies, 2025, no. 1 (78), pp. 99–110. Available at: http://www.journal.viam.ru (accessed: June 05, 2025). DOI: 10.18577/2713-0193-2025-0-1-99-110.
  25. Gribova I.A., Vinogradova O.V. Advances in the Production of Thermostable Antifrication Plastics. Russian Chemical Reviews, 2019, vol. 48, no. 1, pp. 95–102.
  26. Volkov D.P., Egorov A.G., Mironenko M.E. Thermophysical properties of polymer composite materials. Nauchno-tekhnicheskiy vestnik informatsionnykh tekhnologiy, mekhaniki i optiki, 2017, vol. 17, no. 2, pp. 287–293.