Forostovich T.L., Narskiy A.R., Bityutskaya O.N. Removal of model compositions from shell molds in the production of cast gas turbine engine blades // Proceedings of VIAM. 2026. No. 2 (156). С. 3–12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-2-3-12.

Removal of model compositions from shell molds in the production of cast gas turbine engine blades

Forostovich T.L., Narskiy A.R., Bityutskaya O.N.
Abstract

Gas turbine engine parts are made of nickel superalloys by die casting. One of the most important technological stages of this process, which largely determines the quality of the finished casting, is the removal of model masses from shell molds. The review examines the advantages and disadvantages of various methods of removing model compounds, as well as the main trends of domestic scientific research studies aimed at intensifying the process, reducing the possibility of cracks formation in molds and casting defects.

Keywords
gas turbine engine, blades, superalloys, precision casting, model compositions, wax
Reference list
  1. Demonis I.M. At full tilt. Nauka i zhizn, 2007, no. 6, pp. 40–44.
  2. Kovalenko T.S. «Burned» type defect on cast billets of heat-resistant nickel alloys (type ZhS32). Aviation materials and technologies, 2023, no. 4 (73), pp. 14–22. Available at: http://www.journal.viam.ru (accessed: April 16, 2025). DOI: 10.18577/2713-0193-2023-0-4-14-22.
  3. Echin A.B., Bondarenko Yu.A., Kolodyazhny M.Yu., Surova V.A. Review of perspective high-temperature superalloys based on refractory non-metallic materials for production of gas turbine engines. Aviation materials and technologies, 2023, no. 3 (72), pp. 30–41. Available at: http://www.journal.viam.ru (accessed: April 16, 2025). DOI: 10.18577/2713-0193-2023-0-3-30-41.
  4. Kablov E.N. S.T. Kishkin and his contribution to the development of science and materials science. Repors Intl. Sci.-tech. Conf. dedicated to the 100th anniversary of the birth of Academician S.T. Kishkina «Scientific ideas of S.T. Kishkin and modern materials science». Moscow: VIAM, 2006, pp. 5–11.
  5. Casting heat-resistant alloys. Effect of S.T. Kishkin: sci.-tech. collection. Ed. E.N. Kablov. Moscow: Nauka, 2006, 272 p.
  6. History of aviation materials science. VIAM – 80 years: years and people. Ed. E.N. Kablov. Moscow: VIAM, 2012, 520 p.
  7. Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crystallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), pp. 3–12. Available at: http://www.viam-works.ru (accessed: April 16, 2025). DOI: 10.18577/2307-6046-2020-0-3-3-12.
  8. Kishkin S.T. Development, Research, and Application of Heat-Resistant Alloys: Selected Works (on the 100th Anniversary of His Birth). Moscow: Nauka, 2006, 407 p.
  9. Kablov E.N. Production of Gas Turbine Engine Blades by Directional Solidification. Gazoturbinnye tekhnologii, 2000, no. 3, pp. 10–13.
  10. Kablov E.N. Cast Blades of Gas Turbine Engines. Alloys, Technologies, Coatings. 2nd ed. Moscow: Nauka, 2006, 632 p.
  11. Repyakh S.I. Technological Foundations of Investment Casting. Dnepropetrovsk: Lira, 2006, 1056 p.
  12. Gini E.Ch., Zarubin A.M., Rybkin V.A. Special casting technologies. Moscow: Publ. house of Bauman Moscow State Tech. Univ., 2010, 368 p.
  13. Investment casting. Ed. Ya.I. Shklennik, V.A. Ozerov. 3rd ed. Moscow: Mashinostroenie, 1984, 408 p.
  14. Echin A.B., Deynega G.I., Narsky A.R. New developments of NRC «Kurchatov Institute» – VIAM in the field of materials for casting processes of superalloys. Trudy VIAM, 2023, no. 8 (126), pp. 13–24. Available at: http://www.viam-works.ru (accessed: April 16, 2025). DOI: 10.18577/2307-6046-2023-0-8-13-24.
  15. Forostovich T.L., Narsky A.R., Bityutskaya O.N., Mokeev N.A. Production of model compositions for investment casting in the National Research Center «Kurchatov Institute» – VIAM. Trudy VIAM, 2025, no. 4 (146), pp. 3–13. Available at: http://www.viam-works.ru (accessed: April 16, 2025). DOI: 10.18577/2307-6046-2025-0-4-3-13.
  16. Forostovich T.L., Narsky A.R., Bityutskaya O.N., Mokeev N.A. Granulation of model compositions produced by National Research Center «Kurchatov Institute» – VIAM for castings on smelted models. Trudy VIAM, 2024, no. 7 (137), pp. 3–11. Available at: http://www.viam-works.ru (accessed: April 16, 2025). DOI: 10.18577/2307-6046-2024-0-7-3-11.
  17. Narskiy A.R. Shell Mold Manufacturing Using Microwave Energy. Metallurgiya mashinostroeniya, 2005, no. 5, pp. 40–44.
  18. Leushina L.I., Leushin I.O., Koshelev O.S. Improving the Efficiency of Hot Water Melting of Paraffin-Stearin Precision Casting Patterns. Chernye metally, 2019, no. 10, pp. 38–42.
  19. Garanin V.F., Ozerov V.A., Murkina A.S., Kurenkova O.A. Melting Patterns from Shell Molds. Liteynoe proizvodstvo, 1997, no. 2, pp. 16–19.
  20. Shub I.E., Sorokin P.V. Precision Investment Casting. 2nd ed., rev. and add. Leningrad: Mashinostroenie, 1968, 237 p.
  21. Selivanov Yu.A. Microwave Energy in Investment Casting Processes. Improving the Quality and Efficiency of Investment Casting: Seminar Proceedings. Moscow: MDNTP, 1989, pp. 91–97.
  22. Arkhangelsky Yu.S. Dielectric Heating Units. Microwave Units. Saratov: Publ. House of Saratov State Tech. Univ., 2003, 344 p.
  23. Semenov A.S., Bayburin V.B. Microwave Energy and Its Application. Features, Equipment, and Technological Processes. Saratov: Publ. House of Saratov State Tech. Univ., 1999, 116 p.
  24. Uglev N.P., Poilov V.Z., Merzlyakov K.S. et al. On the Removal of Pattern Masses from Ceramic Shells in Investment Casting. Liteynoe proizvodstvo, 2015, no. 3, pp. 17–20.
  25. Leushin I.O., Leushina L.I., Rakitin S.R. Activation of Melting of Paraffin-Stearin Precision Casting Patterns in Hot Water. Progressive Foundry Technologies: Proceedings of the XI Int. Res. and Pract. Conf. Moscow, 2022, pp. 103–108.
  26. Method for Manufacturing Ceramic Shell Molds for Investment Casting: pat. 2707642 Rus. Federation; appl. 10.09.19; publ. 28.11.19.
  27. Sapchenko I.G., Evstigneev A.I., Kostina T.V. Features of Removing Patterns from Shell Molds in Investment Casting Machines. Liteynoe proizvodstvo, 1999, no. 2, pp. 35–36.
  28. Sapchenko I.G., Evstigneev A.I., Kostina T.V. Effect of Thermal Conductivity of Shell Molds on the Removal of Investment Patterns. Liteynoe proizvodstvo, 2000, no. 3, pp. 40–41.
  29. Evstigneev A.I., Dmitrevsky I.P., Sapchenko I.G., Timofeev G.I. Study of the regularities of the process of melting models from shell molds. Liteynoe proizvodstvo, 1994, no. 3, pp. 17–18.
  30. Gutko Yu.I., Voitenko V.V., Medvedchuk S.A. Experimental studies of melting wax models from plaster casting molds using microwave radiation. Science of the Young – the Future of Russia: Reports VII All-Rus. Sci. and Pract. Conf. Penza: Science and Education, 2024, pp. 67–70.