Potapov M.V., Buzenkov A.V., Morgunov R.B., Piskorsky V.P. Effect of gadolinium doping on the magnetic properties of sintered Pr–Dy–Fe–Co–B magnets // Proceedings of VIAM. 2026. No. 1 (155). С. 150–161. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-1-150-161.

Effect of gadolinium doping on the magnetic properties of sintered Pr–Dy–Fe–Co–B magnets

Potapov M.V., Buzenkov A.V., Morgunov R.B., Piskorsky V.P.
Abstract

The dependence of the magnetic properties of sintered materials of the composition (Pr1–z–xDyxGdz)12,55–12,81(Fe0,80Co0,20)balB5,71–6,25 (x = 0,34–0,58; z = 0,11–0,33)on the gadolinium concentration and sintering temperature of 1120–1140 °C was studied. The temperature coefficient of induction was measured in the temperature range of 20–100 °C. Demagnetization curves (magnetization and induction) were measured using a vibrating sample magnetometer (VSM) at temperature of 20±5 °C. The temperature dependences of the magnetization in the temperature range of 300–600 K were revealed. about the article states the effect of gadolinium on the magnetic characteristics of sintered materials.

Keywords
dynamically adjustable gyroscope, rare earth metals, residual induction, coercive force by magnetization and induction, temperature dependence of magnetization, squareness of the demagnetization curve
Reference list
  1. Mezentsev G.M. Analysis of a Two-Mass Model of Linear Motion of a Dynamically Tuned Gyroscope. Miass: Publ. House of the South Ural State University, 2019, 94 p.
  2. Martynenko Yu.G. Trends in the Development of Modern Gyroscopy. Sorosovskiy obrazovatelnyy zhurnal, 1997, no. 11, pp. 120–127.
  3. Vasilevsky N.I. Development of a Dynamically Tuned Gyroscope Taking into Account its Vibration Characteristics. Miass: Publ. House of the South Ural State University, 2018, 77 p.
  4. Chirkin D.S., Roslovets P.V., Tatarinov F.V. et al. Reducing the Drift of a Dynamically Tuned Gyroscope from Launch to Launch. Inzhenernyy zhurnal: nauka i innovatsii, 2017, no. 1, pp. 1–14. DOI: 10.18698/2308-6033-2017-01-1579.
  5. Topilskaya S.V., Borodulin D.S., Kornyukhin A.V. Experimental assessment of permissible mechanical effects on a dynamically tuned gyroscope. Vestnik MGTU im. N.E. Baumana. Ser.: Priborostroyenie, 2018, no. 4, pp. 69–79.
  6. Kablov E.N., Ospennikova O.G., Vershkov A.V. Rare metals and rare-earth elements are materials for modern and future high technologies. Aviacionnye materialy i tehnologii, 2013, no. S2, pp. 3–10.
  7. Sun T., Zhu J., Wan D. The anisotropic expansion and fracture of radially oriented toroid specimens of the rare-earth-cobalt permanens magnets. Fourth International Workshop on Rare Earth-Cobalt Permanent Magnets and Their Applications. Hakone, 1979, paper nо. 12-5, pp. 419–435.
  8. Tian J., Qu H., Zhang S. еt al. Magnetic properties and microstructure of radially oriented Sm(Co, Fe, Cu, Zr)Z ring magnets. Materials Letters, 2007, vol. 61, pp. 5271–5274.
  9. Tian J., Qu H., Zhang S. еt al. Influence of heat treatment on fracture and magnetic properties of radially oriented Sm2Co17 permanent magnets. Transaction of Nonferrous Metals Society of China, 2007, vol. 17, pp. 491–495.
  10. Li A., Li W., Wang H. et al. The study on thermal expansion of sintered Sm2Co17 magnets. IEEE Transaction on Magnetics, 2009, vol. 45, no. 10, pp. 4402–4404.
  11. Tian J., Pan D., Zhou H. et al. Radial cracks and fracture mechanism of radially oriented ring 2:17 type SmCo magnets. Journal of Alloys and Compounds, 2009, vol. 467, pp. 98–101.
  12. Moiseeva N.S., Rezchikova I.I., Korolev D.V. et al. Limitation of the permissible coercive force caused by the stray field of a magnet. Zhurnal tekhnicheskoy fiziki, 2019, vol. 89, no. 7, рр. 1055–1058.
  13. Tenaud P., Lemaire H., Vial F. Recent improvements in NdFeB sintered magnets. Journal of Magnetism and Magnetic Materials, 1991, vol. 101, pp. 328–332.
  14. Herbst J.F. R2Fe14B materials: intrinsic properties and technological aspects. Reviews of Modern Physics, 1991, vol. 63, no. 4, pp. 819–898.
  15. Sergeev V.V., Bulygina T.N. Magnetically hard materials. Moscow: Energiya, 1980, 224 p.
  16. Kablov E.N., Ospennikova O.G., Piskorskij V.P., Rezchikova I.I., Valeev R.A., Davydova E.A. Phase composition of the Pr–Dy–Fe–Co–B sintered materials. Aviacionnye materialy i tehnologii, 2015, no. S2 (39), pp. 5–10. DOI: 10.18577/2071-9140-2015-0-S2-5-10.
  17. Buzenkov A.V., Burkanov M.V., Valeev R.A., Piskorsky V.P. Properties of sintered magnets Pr–Dy–Fe–Co–B depending on the composition and technological parameters of manufacture. Trudy VIAM, 2024, no. 5 (135), pp. 91–100. Available at: http://www.viam-works.ru (accessed: February 20, 2025). DOI: 10.18577/2307-6046-2024-0-5-91-100.
  18. Valeev R.A., Korolev D.V., Morgunov R.B., Piskorsky V.P. The contribution of phases to the magnetization of sintered materials Nd–Dy–Fe-Co–B. Trudy VIAM, 2022, no. 11 (117), pp. 60–68. Available at: http://www.viam-works.ru (accessed: February 20, 2025). DOI: 10.18577/2307-6046-2022-0-11-60-68.
  19. Determination of the density of bodies by hydrostatic weighing: method. recommendations. Irkutsk: Irkutsk State Univ., 2003, pp. 1–9.
  20. Lapteva K.A., Tolmachev I.I. Calculation of the demagnetizing factor during longitudinal magnetization in magnetic particle testing. Izvestiya Tomskogo politekhnicheskogo universiteta, 2012, vol. 321, no. 2, pp. 140–144.
  21. Sato M., Ishii Y. Simple and approximate expressions of demagnetizing factors of uniformly magnetized rectangular rod and cylinder. Journal of Applied Physics, 1989, vol. 66, no. 2, pp. 983–985.
  22. Chen D.-X., Brug J.A., Goldfarb R.B. Demagnetizing factor for cylinder. IEEE Transactions on Magnetics, 1991, vol. 27, no. 4, pp. 3601–3619.
  23. Perigo E.A., Takiishi H., Motta C.C. et al. On the squareness factors behavior of RE–FeB (RE = Nd or Pr) magnets above room temperature. IEEE Transaction Magnetics, 2009, vol. 45, no. 10, pp. 4431–4434.
  24. Yuing Z., Tianyu M., Mi Y. et al. Squareness factors of demagnetization curves for multi-main-phase Nd–Ce–Fe–B magnets with different Ce contents. Journal of Magnetism and Magnetic Materials, 2019, vol. 487, p. 165355. DOI: 10.1016/ j.jmmm.2019.165355.
  25. Minna H., Sampo T., Timo S.-N. et al. Magnetic behavior of sintered NdFeB magnets on a long-term timescale. Advances in Materials Science and Engineering, 2014, vol. 7, p. 760584. DOI: 10.1155/2014/760584.
  26. Takiishi H., Lima L.F.C.P., Costa I. et al. The influence of process parameters and alloy structure on the magnetic properties of NdDyFeNb HD sintered magnets. Journal of Materials Processing Technology, 2004, vol. 152, pp. 1–8.
  27. de Vos K.J. The relationship between microstructure and magnetic properties of alnico alloys. Eindhoven: Technische Hogeschool Eindhoven, 1966, 119 p. DOI: 10.6100/IR287613.
  28. Akbar S., Ahmad Z., Awanb M.S. et al. Development of Fe–Cr–Co permanent magnets by single step thermo-magnetic treatment. Key Engineering Materials, 2012, vol. 510–511, pp. 507–512.
  29. Betancourt J.I. Nanocrystalline hard magnetic alloys. Revista Mexicana de Fisica, 2002, vol. 48 (4), pp. 283–289.
  30. Heritier L., Fruchart R. Crystallographic and magnetic study of solid solutions Gd2(Fe14-xCox)B, Gd2(Co14-xMnx)B, Dy2Fe14BHx, Y2Fe14BHx and Lu2Fe14BHx. Journal de Physique, 1985, vol. 46, pp. C6-319–C6-322.
  31. Korolev M.N. Study of technical characteristics of modern types of angular rate sensors. Proceedings of the 12th Int. sc. and tech. conf. «Instrument Engineering–2019». Minsk: BNTU, 2019, pp. 21–23.
  32. Blazhnov B.A., Nesenyuk L.P., Peshekhonov V.G., Staroseltsev L.P. Miniature integrated orientation and navigation systems. Elektronika: Nauka, Tekhnologiya, Biznes, 2001, vol. 5, pp. 56–59.
  33. Valeev R.A., Korolev D.V., Morgunov R.B., Piskorsky V.P. The effect of high concentrations of cobalt on the properties of magnets Pr–Dy–Fe–Co–B and Nd–Dy–Fe–Co–B. Trudy VIAM, 2022, no. 10 (116), pp. 66–75. Available at: http://www.viam-works.ru (accessed: February 20, 2025). DOI: 10.18577/2307-6046-2022-0-10-66-75.
  34. Valeev R.A., Piskorsky V.P., Korolev D.V., Morgunov R.B. Optimization of the cobalt content as a way of temperature stabilization of rare earth magnets. Trudy VIAM, 2023, no. 3 (121). pp. 58–66. Available at: http://www.viam-works.ru (accessed: February 20, 2025). DOI: 10.18577/2307-6046-2023-0-3-58-66.