Zakirova L.I., Sibileva S.V., Vdovin A.I., Koltsova M.А. Selection of electrodeposited coating on corrosion-resistant steels for corrosion protection in contact with aluminium alloys // Proceedings of VIAM. 2025. No. 9 (151). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2025-0-9-63-76.

Selection of electrodeposited coating on corrosion-resistant steels for corrosion protection in contact with aluminium alloys

Zakirova L.I., Sibileva S.V., Vdovin A.I., Koltsova M.А.
Abstract

The paper presents the results ofelectrochemical studies of samples of corrosion-resistant steels (08kH18N10, 12kH18N10T) and aluminum alloys (1163, В95, 1933) both with and without coatings. We have determined the values of the steady-state potentials, impedance modulus, the potential and current density of contact corrosion, and the tans passivation potential. Based on the results of 2160-hour corrosion tests in the salt spray chamber on samples packages made of corrosion-resistant steels with electroplating and aluminum alloys with nonchromated anodic coating, we have selected an electrodeposited coating that is as good as cadmium coating in its protective ability.

Keywords
electrodeposition, cadmium coating, alloy coating, electrodeposited coating, electrochemical impedance spectroscopy, anodic and cathodic polarization curves, contact corrosion potential, contact corrosion current density, acc
Reference list
  1. Nochovnaya N.A., Ivanov V.I., Alekseyev E.B., Islamov R.S. Intermetallic compound Ti2AlNb – promising material for aviation and space technology. Part 1. Crystal structure and phase transformations. Aviation materials and technologies, 2023, no. 3 (72), paper no. 04. Available at: http://www.journal.viam.ru (accessed: July 03, 2025). DOI: 10.18577/2713-0193-2023-0-3-42-61.
  2. Peskova A.V., Sukhov D.I., Mazalov P.B. Examination of the formation of the titanium alloy VT6 structure obtained by additive manufacturing. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 38–44. DOI: 10.18577/2071-9140-2020-0-1-38-44.
  3. Illarionov E.I., Kolobnev N.I., Gorbunov P.Z., Kablov E.N. Aluminum alloys in aerospace engineering. Gen. ed. E.N. Kablov. Moscow: Nauka, 2001, 192 p.
  4. Antipov V.V., Klochkova Yu.Yu., Romanenko V.A. Modern aluminum and aluminum-lithium alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 195–211. DOI: 10.18577/2071-9140-2017-0-S-195-211.
  5. Peng Y., Zhao J., Liu Y. et al. Galvanic corrosion between Al‒Zn‒Mg‒Cu alloy and stainless steel in the salt-spray atmosphere. Materials Chemistry and Physics, 2023, vol. 294, art. 127009. DOI: 10.1016/j.matchemphys.2022.127009.
  6. Vahromov R.O., Tkachenko E.A., Popova O.I., Milevskaya T.V. Summarizing of the experience of usage and optimization of manufacturing technology semi-fished product of high strength aluminum alloy 1933 for the primary structures of modern aircraft. Aviacionnye materialy i tehnologii, 2014, no. 2, pp. 34–39. DOI: 10.18577/2071-9140-2014-0-2-34-39.
  7. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  8. Ruiz A.G., Jimenez-Gonzalez E., Canoc E. et al. The corrosion products in a carbon steel/aluminum alloy galvanic couple under thin electrolyte films: An efficient model. Electrochemistry Communications, 2019, vol. 104, art. 106485. DOI: 10/1016/j.elecom.106485.
  9. Matzdorf C.A., Nickerson W.C., Rincon Tronconis B.C. et al. Galvanic Test Panels for Accelerated Corrosion Testing of Coated Al Alloys: Part 1 – Concept. Corrosion, 2013, vol. 69, is. 12, pp. 1240‒1246.
  10. State Standard 9.005–72. Unified system of protection against corrosion and aging. Metals, alloys, metallic and non-metallic inorganic coatings. Permissible and impermissible contacts with metals and non-metals. Moscow: Standartinform, 2008, 28 p.
  11. Rosenfeld I.L. Corrosion and protection of metals. Moscow: Metallurgiya, 1970, 448 p.
  12. ASTM STP 576. Galvanic and Pitting Corrosion ‒ Field and Laboratory Studies. American Society For Testing And Materials, 1974, pp. 5‒19.
  13. Kucera V., Mattson Е. Atmospheric Corrosion of bimetallic Structures. Atmospheric Corrosion. Wiley & Sons, 1982, pp. 561–574.
  14. Matys V.G., Poplavsky V.V. Resistance of aluminum and its alloy to contact corrosion in galvanic couples with steels with metallic coatings. Trudy BGTU: Khimiya i tekhnologiya neorganicheskikh veshchestv, 2015, no. 3, pp. 85‒92.
  15. Vinogradov S.S., Nikiforov A.A., Zakirova L.I., Vdovin A.I. Comparative assessment of the protective ability of a galvanothermic coating of the zinc-tin system and a cadmium coating in a chloride environment. Korroziya: materialy, zashchita, 2020, no. 5, pp. 21‒29. DOI: 10.31044/1813-7016-2020-0-5-21-29.
  16. Zakirova L.I., Laptev A.B. Properties of protective electroplating coatings for replacement of cadmium on steel fixing parts (review). Part 1. Morphology and corrosion resistance. Aviaсionnye materialy i tehnologii, 2020, no. 3 (60), pp. 37–46. DOI: 10.18577/2071-9140-2020-0-3-37-46.
  17. Laptev A.B., Zakirova L.I., Degovets M.L. Properties of protective galvanic coatings for replacement of cadmium on steel fixing parts (review). Part 2. Hydrogen embrittlement and frictional characteristics. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 35–40. DOI: 10.18577/2071-9140-2020-0-4-35-40.
  18. Navinsek B., Panjan P., Milosev I. PVD coatings as an environmentally clean alternative to electroplating and electroless processes. Surface and Coatings Technology, 1999, vol. 116–119, pp. 476–487.
  19. Enders B., Knau B.S., Wolf G.K. Corrosion properties of aluminum based alloys deposited by ion beam assisted deposition. Surface and Coatings Technology, 1994, vol. 65, pp. 203–207.
  20. Jianming X., Weijianga Z., Wolf G.K. The corrosion properties of Al/Al2O3 multilayered coatings on CK45 steel deposited by IBAD. Surface and Coatings Technology, 2004, vol. 187, pp. 194–198.
  21. Zakirova L.I., Sibileva S.V., Demin S.A., Duyunova V.A. Investigation of electroplating of corrosion-resistant steels to prevent contact corrosion. Trudy VIAM, 2024, no. 9 (139), paper no. 05. Available at: http://www.viam-works.ru (accessed: July 03, 2025). DOI: 10.18577/2307-6046-2024-0-9-42-53.
  22. State Standard 9.305–84. Unified system of corrosion and aging protection. Metallic and non-metallic inorganic coatings. Operations of technological processes for obtaining coatings. Moscow: Publ. House of Standards, 2003, 105 p.
  23. State Standard 9.402–2004. Unified system of corrosion and aging protection. Paint and varnish coatings. Preparation of metal surfaces for painting. Moscow: Standartinform, 2006, 43 p.
  24. State Standard 9.302–88. Unified system of corrosion and aging protection. Metallic and non-metallic inorganic coatings. Control methods. Moscow: Publ. House of Standards, 2001, 40 p.
  25. State Standard 9.909–2023. Unified system of corrosion and aging protection. Metallic and non-metallic inorganic coatings, metals and alloys. Test methods at climatic test stations. Moscow: RST, 2023, 12 p.
  26. State Standard 9.308–85. Unified system of corrosion and aging protection. Metallic and non-metallic inorganic coatings. Accelerated corrosion testing methods. Moscow: Publ. House of Standards, 1990, 21 p.
  27. State Standard R 9.907–2007. Unified system of corrosion and aging protection. Metals, alloys, metallic coatings. Methods of removing corrosion products after corrosion testing. Moscow: Standartinform, 2007, 19 p.
  28. Zhuk N.P. Course in the theory of corrosion and protection of metals. Moscow: Metallurgiya, 1976, 472 p.
  29. Tomashov N.D. Theory of corrosion and protection of metals. Moscow: Publ. House of the USSR Academy of Sciences, 1959, 592 p.
  30. Laptev A.B., Zakirova L.I., Zagorskikh O.A., Pavlov M.R., Gorbovets M.A. Methods of in-vestigation of the processes of corrosion-mechanical destruction and hydrogenation of metals (review). Part 2. Formation of passive films and hydrogen sulfide cracking of steels. Trudy VIAM, 2022, no. 5 (111), paper no. 12. Available at: http://www.viam-works.ru (accessed: July 03, 2025). DOI: 10.18577/2307-6046-2022-0-5-138-146.
  31. Kablov E.N., Kutyrev A.E., Vdovin A.I., Kozlov I.A., Afanasyev-Khodykin A.N. The research of possibility of galvanic corrosion in brazed connections used in aviation engine construction. Aviation materials and technologies, 2021, no. 4 (65), paper no. 01. Available at: http://www.journal.viam.ru (accessed: July 03, 2025). DOI: 10.18577/2713-0193-2021-0-4-3-13.